低壓化學氣相沉積法成長於N型矽基板之全無機鈣鈦礦溴化銫鉛薄膜之研究
All-inorganic Perovskite CsPbBr3 Thin Film Grown on N-Type Silicon via Low-Pressure Chemical Vapor Deposition
摘要
本研究是以低壓化學氣相沉積法(LPCVD)於N型矽基板上製備全無機鈣鈦礦CsPbBr3薄膜。藉由控制三區管狀高溫爐腔體內環境壓力、溫度、調控載體氣流之流量,以及改變沉積溫度以改變CsPbBr3薄膜之表面形貌並觀察其放光特性。參考先前研究成果,並於實驗設計改變與參數調整後,歸納分析在環境壓力700 mTorr、前驅物PbBr2以320 °C、前驅物CsBr則以470 °C分別作為第一、第二加熱區之實驗溫度、升溫時間為30分鐘、持溫時間為120分鐘、載體氣流量為240 sccm、沉積溫度約為181 °C的生長條件下;可觀察到形成之鈣鈦礦薄膜平均粗糙度為30.6 nm、平均晶粒尺寸達0.56-0.81 µm、厚度達2.043 µm,於激發強度206.1 µJ/cm2可得到最低之半峰全寬(Full Width at Half Maximum,FWHM)為23.2 nm,其雷射激發強度自8.82 µJ/cm2至1095.4 µJ/cm2之間,皆不會使薄膜放光強度有所衰減,足見薄膜對雷射激發強度及熱耐受性較高,且為結晶度良好之單晶CsPbBr3薄膜。
This study used the low-pressure chemical vapor deposition (LPCVD) method to fabricate all-inorganic perovskite CsPbBr3 thin films on N-type silicon substrates. The surface morphology of the CsPbBr3 films was changed by regulating the environmental pressure, temperature, and carrier gas flow rate, and modifying the substrate deposition temperature in the three-zone tube furnace to observe the emission properties of CsPbBr3 films. Referring to the previous research results, and after making changes and adjustments to the experimental design and parameters, the following growth conditions were identified and analyzed: an environmental pressure of 700 mTorr, a temperature of 320 °C for the precursor PbBr2 in the first heating zone, and a temperature of 470 °C for the precursor CsBr in the second heating zone, heating time was 30 minutes, and soak time was 120 minutes. The carrier gas flow rate was set at 240 sccm, and the substrate deposition temperature was approximately 181 °C. Under these growth conditions, the CsPbBr3 thin film exhibited an average roughness of 30.6 nm, an average grain size from 0.56 to 0.81 µm, and a thickness of 2.043 µm. At an excitation intensity of 206.1 µJ/cm2, the film displayed the narrowest full width at half maximum (FWHM) of 23.2 nm. Importantly, the film maintained its luminescent intensity without significant degradation across a range of laser excitation intensities from 8.82 to 1095.4 µJ/cm2. This indicates that the film exhibits high tolerance laser excitation intensity and heat and is a well-crystallized single-crystal CsPbBr3 thin film.