摘要

本研究藉由在低壓化學氣相沉積法(Low-Pressure Chemical Vapor Deposition, LPCVD)中控制成長時間與成長氣流及基板溫度,成功地在室溫下觀察到無機鈣鈦礦溴化銫鉛CsPbBr3薄膜的放大式自發輻射效應(Amplified Spontaneous Emission, ASE)。在薄膜成長時間為120分鐘,氣流變化範圍為 80至240標準毫升每分(standard cubic centimeter per minute, sccm),搭配不同的基板溫度範圍,在基板溫度為攝氏78-27度下,均可觀察到ASE現象。在實驗的觀察中,隨著氣流流量的提升,改變了鈣鈦礦的表面形貌以及沉積的形貌尺寸,表面粗糙度由11奈米降至5.4奈米,晶粒的形貌尺寸自200 奈米升至近1微米。在放大式自發輻射效應的量測中,最低的ASE閾值為11.5 µJ/cm2;為確切的分析放大式自發輻射效應的機制,我們在藍寶石基板、玻璃、ITO基板、矽基板、以及鍍有高反射層的藍寶石基板上生長CsPbBr3鈣鈦礦薄膜,以此分析,證實ASE的產生是通過基板與CsPbBr3之間的折射率差所引起的全反射,以光波導模式在薄膜之間傳播,而產生光放大效應。這種低溫沉積方法不僅適用於各種基板,也對CsPbBr3鈣鈦礦薄膜在不同元件中的應用具有重要意義。
This study successfully observed the amplified spontaneous emission (ASE) of all inorganic perovskite CsPbBr3 thin films at room temperature by controlling the growth time, gas flow rate, and substrate temperature in the Low-Pressure Chemical Vapor Deposition (LPCVD) process. ASE phenomena were observed when the film growth time was 120 minutes, and the gas flow varied from 80 to 240 standard cubic centimeters per minute (sccm), with different substrate temperatures ranging from 78 to 27 degrees. During the experiments, it was observed that the surface morphology of perovskite films changed with increasing gas flow rate. The surface roughness decreased from 11 to 5.4 nanometers, and the grain size increased from 200 nanometers to nearly 1 micrometer. In the measurements of ASE, the lowest ASE threshold was recorded at 11.5 µJ/cm². To precisely analyze the mechanism of ASE, we attempted to grow CsPbBr3 perovskite films on various substrates, including sapphire, glass, indium tin oxide, silicon substrates, and sapphire substrates with high reflectivity coatings. Through this analysis, it was confirmed that ASE generation occurs through total internal reflection caused by the refractive index difference between the substrate and CsPbBr3, propagating light through waveguide modes between the thin films, resulting in optical amplification. This low-temperature deposition method is not only applicable to various substrates but also holds significant importance for the diverse applications of CsPbBr3 perovskite thin films in different devices.
顯示完整詮釋資料 統計資料

引用此條目

唐向豪 (2024). 化學氣相沉積溴化銫鉛薄膜與放大的自發輻射之研究. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/1124

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享

永久網址:https://thesis.lib.nycu.edu.tw/handle/20.500.14371/1124