電極優化與電漿處理實現氧化鉿鋯之厚度微縮
Thickness Reduction of Hf1-xZrxO2 Achieved through Electrode Optimization and In-situ Plasma Treatment
摘要
鐵電材料被譽為下一代記憶體的有力候選者,特別是在非揮發性記憶體的應用中。由於其材料特性,可以實現低功耗、快速讀寫和更長久的數據保存能力。其中,氧化鉿鋯(Hf1-xZrxO2, HZO)尤為突出,不僅兼容目前主流的半導體製程,還能在厚度十奈米以下展現出強大的鐵電特性,因此備受工業界的關注。然而,儘管HZO具有微縮的潛力,但隨著厚度減少,極化量降低和更高製程熱預算等問題逐漸浮現。因此,本研究旨在降低鐵電薄膜厚度的同時,保持其鐵電性質,並降低製程的熱預算。
本研究通過metal-ferroelectric-metal (MFM)電容結構對HZO的厚度微縮進行了系統性的調查,通過選用不同的電極材料、優化製程參數以及原位電漿處理,實現了更薄的HZO鐵電薄膜。選用鎢作為電極材料,使HZO在厚度降至4奈米時仍能維持良好的鐵電性能。對HZO進行氬氣電漿處理,不僅提升了HZO薄膜的結晶性,還減少了薄膜內部的氧空缺含量,並使HZO在4奈米時展現約30 μC/cm²的剩餘極化量且幾乎無喚醒效應,還能在更低的退火溫度下表現出鐵電性。本研究使用同步輻射X光進行材料分析,探討隨著製程演變,HZO的微觀和宏觀特性之間的變化與關聯性。
本研究通過metal-ferroelectric-metal (MFM)電容結構對HZO的厚度微縮進行了系統性的調查,通過選用不同的電極材料、優化製程參數以及原位電漿處理,實現了更薄的HZO鐵電薄膜。選用鎢作為電極材料,使HZO在厚度降至4奈米時仍能維持良好的鐵電性能。對HZO進行氬氣電漿處理,不僅提升了HZO薄膜的結晶性,還減少了薄膜內部的氧空缺含量,並使HZO在4奈米時展現約30 μC/cm²的剩餘極化量且幾乎無喚醒效應,還能在更低的退火溫度下表現出鐵電性。本研究使用同步輻射X光進行材料分析,探討隨著製程演變,HZO的微觀和宏觀特性之間的變化與關聯性。
Ferroelectric materials are considered strong candidates for next-generation memory, especially in non-volatile memory. They enable low power consumption, fast read/write speeds, and prolonged data retention. Among them, Hafnium Zirconium oxide (HZO) stands out for its compatibility with semiconductor processes and for exhibiting strong ferroelectric properties at thicknesses below 10nm. Therefore, it has obtained great attention from the industry. Despite HZO’s potential for scaling, issues such as polarization degradation and higher thermal budgets in the fabrication process have appeared as its thickness decreases. Therefore, the objective of this study is to reduce the thickness of HZO while maintaining their ferroelectricity and reducing the thermal budget of the process.
In this study, we systematically investigate the thickness reduction of HZO film. Thinner HZO was achieved by using different electrode materials, optimizing process parameters, and applying in-situ plasma treatments. W electrode allows HZO to maintain great ferroelectricity at a thickness decrease of 4nm. Argon plasma treatment during HZO deposit not only enhances the crystallinity of HZO but also improves the oxygen vacancy within the films, has a 2Pr ≈ 30 μC/cm² with wake-up free at 4nm HZO, and exhibits ferroelectricity at lower annealing temperatures. Material analysis was performed using synchrotron X-ray radiation to observe the changes and relationship between the microscopic and macroscopic characteristics of HZO as the process evolves.
In this study, we systematically investigate the thickness reduction of HZO film. Thinner HZO was achieved by using different electrode materials, optimizing process parameters, and applying in-situ plasma treatments. W electrode allows HZO to maintain great ferroelectricity at a thickness decrease of 4nm. Argon plasma treatment during HZO deposit not only enhances the crystallinity of HZO but also improves the oxygen vacancy within the films, has a 2Pr ≈ 30 μC/cm² with wake-up free at 4nm HZO, and exhibits ferroelectricity at lower annealing temperatures. Material analysis was performed using synchrotron X-ray radiation to observe the changes and relationship between the microscopic and macroscopic characteristics of HZO as the process evolves.