氮化鋁鎵薄膜表面六角丘狀結構之螢光光譜和拉曼光譜之研究
Photoluminescence and Raman scattering Studies of Hillocks on Al[x]GaN[1-x] Film
摘要
本論文主要針對金屬有機化學氣相磊晶系統(MOCVD system)所成長的氮化鋁鎵薄膜(AlxGa1-xN)做一系列的微螢光光譜(□-PL)和微拉曼光譜(□-Raman)之研究。在顯微鏡下,我們可以在樣品表面觀察到幾種不同形狀的六角丘狀結構(Hillock),它們的大小分佈是約2~16 □m。
藉由顯微鏡載台的刻度,可以標定Hillock的位置,由此方式我們可以針對同一顆Hillock進行□-PL和□-Raman的量測。因為應力對螢光光譜的影響很小,而且Hillock內外的鋁組成濃度,從EDX (Energy Dispersion X-ray Spectrometer) 所量測出來的結果與微螢光光譜所推算出來的一致,所以將使用微螢光光譜去決定Hillock的鋁組成濃度。
從微螢光光譜的量測中,發現Hillock結構內部會出現額外的發光譜峰(能量位置約∼3.51eV),有別於該結構外部近帶躍遷的譜峰位置(能量位置約∼3.62eV)。根據微螢光光譜可以推導出Hillock內外的鋁組成濃度分別是約4%和約11%,進而再去計算出此濃度下所對應之沒有受到應力影響的E2模態位置,Hillock內部約在568.5cm-1而其外部約在570.2cm-1。接著使用微拉曼光譜去針對Hillock結構進行實際量測,實驗結果顯示,Hillock結構內部E2模態位置約在570 cm-1,其外部位置約在573 cm-1。比較微螢光光譜和微拉曼光譜之計算和量測結果,發現E2模態位置在Hillock結構內外分別有約1.5 cm-1 和約3 cm-1 的偏差,而此實驗結果顯示,Hillock結構受到了壓縮的應力影響。
我們亦使用微拉曼光譜去分析Hillock結構之形成機制。其結果顯示,Hillock結構內部之E2模態位置約在570 cm-1 而不會隨著聚焦深度變深而改變;聚焦深度越深,隨之出現的是sapphire Eg位於577 cm-1 的訊號。由微拉曼光譜的縱深分析結果,其證明了Hillock結構形成是從AlN緩衝層開始長成。
藉由顯微鏡載台的刻度,可以標定Hillock的位置,由此方式我們可以針對同一顆Hillock進行□-PL和□-Raman的量測。因為應力對螢光光譜的影響很小,而且Hillock內外的鋁組成濃度,從EDX (Energy Dispersion X-ray Spectrometer) 所量測出來的結果與微螢光光譜所推算出來的一致,所以將使用微螢光光譜去決定Hillock的鋁組成濃度。
從微螢光光譜的量測中,發現Hillock結構內部會出現額外的發光譜峰(能量位置約∼3.51eV),有別於該結構外部近帶躍遷的譜峰位置(能量位置約∼3.62eV)。根據微螢光光譜可以推導出Hillock內外的鋁組成濃度分別是約4%和約11%,進而再去計算出此濃度下所對應之沒有受到應力影響的E2模態位置,Hillock內部約在568.5cm-1而其外部約在570.2cm-1。接著使用微拉曼光譜去針對Hillock結構進行實際量測,實驗結果顯示,Hillock結構內部E2模態位置約在570 cm-1,其外部位置約在573 cm-1。比較微螢光光譜和微拉曼光譜之計算和量測結果,發現E2模態位置在Hillock結構內外分別有約1.5 cm-1 和約3 cm-1 的偏差,而此實驗結果顯示,Hillock結構受到了壓縮的應力影響。
我們亦使用微拉曼光譜去分析Hillock結構之形成機制。其結果顯示,Hillock結構內部之E2模態位置約在570 cm-1 而不會隨著聚焦深度變深而改變;聚焦深度越深,隨之出現的是sapphire Eg位於577 cm-1 的訊號。由微拉曼光譜的縱深分析結果,其證明了Hillock結構形成是從AlN緩衝層開始長成。
In this article, we analyzed AlxGa1-xN epilayer which was grown by MOCVD system, with the aid of the micro-photoluminescence (□-PL) and micro-Raman (□-Raman) systems. Under the microscope, we observed several types of hexagonal hillocks on the epilayer with sizes from 2 to 16 □m.
By using the microscope to demarcate the hillock position, we can combine the □-PL□and□□-Raman system to study the same hillock on this sample. Because the PL results are relatively insensitive to the strain and the Al fraction from Energy Dispersion X-ray Spectrometer ( EDX ) measurements agrees with that deduced from □-PL whether inside or outside the hillock, so we used □-PL spectra to determine the Al fraction of hillock.
From the □-PL spectra, we found that an additional emission peak at (~3.51eV) inside the hillock structure, that differs from the near-band-edge emission (~3.62eV) outside the hillock. According to the PL peak position, the calculated Al fraction is about 4% and 11% inside and outside the hillock. From the Al fraction, we also obtained the strain free E2 mode frequency to be 568.5cm-1 and 570.2 cm-1 inside and outside the hillock, respectively. However, the experimental results of □-Raman spectra show that E2 mode frequency is ~570 cm-1 and ~573 cm-1 inside and outside the hillock, respectively. These are blue shifted by ~1.5 cm-1 and ~3 cm-1 so that hillocks bear compressive stress.
We also used □-Raman scattering to investigate how deep hillocks are formed. The results showed that the E2 mode frequency remains at ~570 cm-1 inside hillock, it dose not shift while the focus depth increases. However, the sapphire Eg mode frequency at 577 cm-1 grows obviously with the increasing focus depth. According to the depth analysis, it is evident that the formation of hillock is from the AlN buffer layer.
By using the microscope to demarcate the hillock position, we can combine the □-PL□and□□-Raman system to study the same hillock on this sample. Because the PL results are relatively insensitive to the strain and the Al fraction from Energy Dispersion X-ray Spectrometer ( EDX ) measurements agrees with that deduced from □-PL whether inside or outside the hillock, so we used □-PL spectra to determine the Al fraction of hillock.
From the □-PL spectra, we found that an additional emission peak at (~3.51eV) inside the hillock structure, that differs from the near-band-edge emission (~3.62eV) outside the hillock. According to the PL peak position, the calculated Al fraction is about 4% and 11% inside and outside the hillock. From the Al fraction, we also obtained the strain free E2 mode frequency to be 568.5cm-1 and 570.2 cm-1 inside and outside the hillock, respectively. However, the experimental results of □-Raman spectra show that E2 mode frequency is ~570 cm-1 and ~573 cm-1 inside and outside the hillock, respectively. These are blue shifted by ~1.5 cm-1 and ~3 cm-1 so that hillocks bear compressive stress.
We also used □-Raman scattering to investigate how deep hillocks are formed. The results showed that the E2 mode frequency remains at ~570 cm-1 inside hillock, it dose not shift while the focus depth increases. However, the sapphire Eg mode frequency at 577 cm-1 grows obviously with the increasing focus depth. According to the depth analysis, it is evident that the formation of hillock is from the AlN buffer layer.