摘要

銅做為非常重要的金屬材料廣泛地使用於在半導體業與電池能源業中,這歸功於銅擁有優秀的機械強度、延展性、導電性、延展性、導熱性。並隨著近年電動車與5G基地台等產業的崛起,銅箔的需求量也隨之上升,並且在多種工業應用中,銅箔的機械性質更是備受重視,另外,在3D IC銅-銅異質接合製程中,銅會被加熱到200°C至300°C進行接合,因此,銅在高溫下的機械性質也顯得很重要。
本研究使用了不同的電鍍配方,製備出六種不同微結構的銅箔,分別為粗晶、細晶、超細晶、(110)雙晶、(111)奈米雙晶、奈米雙晶與超細晶,並在25°C至200°C溫度環境下進行拉伸試驗,並比較不同溫度段下各結構的機械強度與延展性上的差異,分析不同結構的適用溫度區間,以對應於不同類型產品的操作溫度。
25°C至75°C區間內奈米雙晶與超細晶結構有著最高的拉伸強度;75°C至125°C 區間內細晶結構有著最高的拉伸強度;125°C至200°C區間內(111)奈米雙晶結構有著最高的拉伸強度。這些結果歸因於不同結構的破裂行為與高溫弱化機制有所不同,粗晶主要為動態再回復,導致在200°C時UTS下降27.2 %;細晶、(110)雙晶為動態再結晶與晶粒成長,導致在200°C時UTS分別下降70 %與66.6 %;(111)奈米雙晶為動態再結晶、晶粒成長與去雙晶,導致在200°C時UTS下降43.9 %;超細晶、奈米雙晶與超細晶為晶界滑移,導致在200°C時UTS分別下降70.8 %與75.2 %
Copper, as a critically important metallic material, is extensively utilized in the semiconductor and battery energy industries due to its excellent mechanical strength, ductility, electrical conductivity, and thermal conductivity. With the recent rise of industries such as electric vehicles and 5G base stations, the demand for copper foil has also increased. Among various industrial applications, the mechanical properties of copper foil are a key focus. In Addition, in 3D IC Cu-Cu hybrid bounding Cu pads are heated to 200°C-300°C during the bounding process, therefore, the high temperature mechanical properties are of interests.
In this study, we prepared six types of copper foils with different microstructures using various electroplating formulations. The microstructures include coarse-grained, fine-grained, ultrafine-grained, (110) twinned, (111) nanotwinned, and nanotwinned plus ultrafine-grained. Tensile tests were conducted at temperatures ranging from 25°C to 200°C. The mechanical strength and ductility of each structure at different temperature ranges were compared, and the applicable temperature range for each structure was analyzed to correspond to the operating temperatures of different types of products.
Within the 25°C to 75°C range, the nanotwinned plus ultrafine-grained structure exhibited the highest tensile strength. In the 75°C to 125°C range, the fine-grained structure showed the highest tensile strength. In the 125°C to 200°C range, the (111) nanotwinned structure had the highest tensile strength. These differences are attributed to the distinct fracture behaviors and high-temperature weakening mechanisms of each structure. Coarse-grained copper primarily undergoes dynamic recovery, resulting in a 27.2 % decrease in UTS at 200°C. Fine-grained and (110) twinned structures undergo dynamic recrystallization and grain growth, leading to UTS reductions of 70 % and 66.6 %, respectively, at 200°C. (111) nanotwinned structure undergoes dynamic recrystallization, grain growth, and detwinning, causing a 43.9 % decrease in UTS at 200°C. Ultrafine-grained and nanotwinned plus ultrafine-grained structures experience grain boundary sliding, resulting in UTS reductions of 70.8 % and 75.2 %, respectively, at 200°C.
顯示完整詮釋資料 統計資料

引用此條目

陳柏言 (2024). 不同微結構銅箔的中高溫機械性質與破裂行為之研究. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/3274