聚乙烯蠟微球對陶瓷3D列印模型裂縫減少之影響
The effects of polyethylene wax microsphere on the crack reduction of the ceramic 3D printing model
摘要
3D列印擁有客製化設計和快速製造的優勢,已廣泛被應用於模型製作、醫療、汽車工業等多項領域。因陶瓷材料的優越的物理和化學特性,在積層製造的應用上越來越廣受關注。然而,陶瓷3D列印在熱處理汽化過程,易因樹脂汽化進而導致內部結構產生裂痕的缺陷。在本研究旨在添加聚乙烯微球於陶瓷漿料,經由低溫階段製造出汽化通道,減緩樣品內樹脂汽化的壓力,降低結構產生裂痕的風險。在本研究中,共設計三組配方進行試驗,並找出解決裂痕的最佳配例和實驗組進行比較。首先,在低固含量陶瓷漿料中添加不同配比的聚乙烯蠟微球進行列印和燒結,觀察微球比例對成品裂痕改善的效果。接著,基於將最佳比例的添加量應用於不同高固含量的組別進行實驗。最後,將最佳組與實驗組進行比較。在分析試驗,透過黏度測試、熱重分析,了解漿料性質以及適當的升溫參數,並測量樣品在燒結前、燒結後的收縮率及抗彎強度和觀察斷裂形貌。結果顯示,添加微球的組別在燒結前、燒結後的抗彎強度皆有提升的趨勢,且能透過斷裂形貌中觀察出均一的內部結構。
3D printing has the advantages of customized design and rapid manufacturing, and has been widely used in model making, automotive industry, medical and other fields. Because ceramic materials have superior physical and chemical properties, its application of additive manufacturing is attracting more and more attention. However, ceramic 3D printing is prone to crack defects due to the vaporization process during the heat treatment stage. The purpose of this study is to add polyethylene microspheres to the ceramic slurry and create a vaporization channel through a low-temperature stage to release the pressure of resin vaporization in the sample and reduce the risk of structural cracks. In this study, three groups of formulas were designed to find the best ratio for solving cracks in the formula and then compared with the experimental group. First, different ratios of polyethylene wax microspheres were added to the low-solid content ceramic slurry for printing and sintering, and then the effects of the ratio of microspheres on improving cracks in the final product. Next, experiments were conducted based on the optimal ratio of microspheres added to different high-solid content groups. The characterizations included viscosity test, thermogravimetric analysis, shrinkage test, and 3-point test. The results showed the flexural strength of the microsphere groups increases and the complete structure can be observed through the fracture morphology.