摘要

聚合物為日常生活中不可或缺的一部分,而聚氨酯(PU)是最有前途的高分子材料之一。然而,其使用壽命會因使用過程中的損壞而縮短,產生難以回收的廢棄物並造成許多環境問題。從以往文獻發現,二硒鍵接在主鏈上可在可見光下裂解形成硒自由基,而透過硒自由基的交換反應可再次形成新的二硒化物鍵,以此進行自癒合。本研究想嘗試若不將二硒鍵接在主鏈上是否可以達到同樣的自癒合效果,因為這樣可以大幅縮減時間與材料成本。因此,本研究利用二苯基二硒化物在水合性聚氨酯中實現自癒合,並用含有二(1-羥基乙烯)二硒化物的PU當作對照組,比較了兩者的自癒合效率和機械性能。實驗結果顯示,無需在主鏈中摻入二硒鍵即可實現高達 93% 的自修復效率,並且使用鎢絲檯燈照明可以獲得最佳的自癒效果。拉伸測試顯示出二苯基二硒化物除了能降低吸水率,還增強了斷裂強度和斷裂伸長率,並且合成所需的時間和材料成本顯著減少。未來的改進可以進一步提高含二苯基二硒化物的水性聚氨酯的自修復效率,使其適用於醫療器材或工業塗料。
Polymers have become an indispensable part of modern life, and polyurethane (PU) is one of the most promising polymer materials. However, its lifespan is often shortened due to damage incurred during use, resulting in difficult-to-recycle waste and various environmental problems. Previous literature has found that diselenide bonds in the main chain can cleave under visible light, forming selenium radicals, which can undergo exchange reactions to form new diselenide bonds, thus enabling self-healing.
This study aimed to investigate whether diselenide bonds could achieve similar self-healing effects without being incorporated into the main chain, thereby significantly reducing time and material costs. Therefore, this study added diphenyl diselenide in water-borne polyurethane to achieve self-healing, using water-borne polyurethane containing di(1-hydroxyethylene) diselenide as a control group to compare their self-healing efficiencies and mechanical properties. Experimental results showed that high self-healing efficiency of up to 93% was achieved without incorporating diselenide bonds into the main chain, and the best self-healing effect was obtained under desk lamp illumination. Tensile tests revealed that diphenyl diselenide not only reduced water absorption but also enhanced fracture strength and elongation at break. Additionally, the time and material costs required for synthesis were significantly reduced. Future improvements could further enhance the self-healing efficiency of water-borne polyurethane containing diphenyl diselenide, making it suitable for applications in medical devices or industrial coatings.
顯示完整詮釋資料 統計資料

引用此條目

Chen, R.-Y. (2024). Comparing the self-healing ability of diphenyl diselenide-added on water-borne PU with di(1-hydroxyethylene) diselenide-constituted water-borne PU. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/3301

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享

永久網址:https://thesis.lib.nycu.edu.tw/handle/20.500.14371/3301