摘要
一般手術置換之人工關節使用年限為10年左右,其中UHMWPE元件之氧化,造成磨屑增加為置換手術失敗的主因。目前是利用gamma ray照射後進行交聯處理來改進磨耗問題,但市售之交聯產品力學性質較差,且長期抗氧化安定性不明等問題。本研究探討材料交聯與老化後材料物化性質與力學性質之關連。實驗改變不同交聯與老化條件分析其物理、化學及力學性質之變化:化性利用FTIR測量材料的C=O官能基變化來探討氧化度的變化。物性利用浮力法進行密度測試、DSC測量結晶度及熔點。力學性質則利用small punch test偵測initial peak load、ultimate load,ultimate displacement,work to failure及modulus等性質。結果顯示:改變照射劑量與交聯天數對各性質的影響不大,交聯溫度影響則較為顯著。交聯化處理有利於UHMWPE之ultimate load、ultimate displacement、work to failure等性質提升,並且當交聯溫度超過熔點對物化、力學及尺寸安定性分析均顯現有較佳之抗老化效果。動態氧化測試結果顯示,照射後直接氧化及照射交聯後再老化之材料,其氧化度、密度與力學性質在初期呈現一平緩區,當達一特定之延遲時間後,各項物、化及力學性質均呈現明顯加速變化之現象。此延遲時間明顯隨老化溫度增加而減少。藉由適當之物性及力學性質之檢測,亦可靈敏反應出材料老化程度之變化。加速老化模擬實驗結果與理論符合,增加老化時間氧化度上升,增加氧壓使次表層深度增加。
The service time of artificial joints in arthroplasties is usually limited to 10 years. The aseptic loosing and the osteolysis that are induced by wear debris which is caused by the oxidation of UHMWPE material became one of the main cause of long-term failure of joint arthroplasties. Crosslinking process of gamma ray irradiation has been known for several years to improve wear resistance of UHMWPE . But mechanical properties of the crosslinking material in market are worse and its stability of long term oxidation resistence is not clear. This research discuss the physical, chemical and mechanical properties of the material after crosslinking and oxidation processes. For chemical property, we observe the variation of functional groups C=O of the material by FTIR to study the change of OI. For physical properties, we measure density by buoyancy tests and analyze crystalline degree and Tm by DSC. For mechanical properties, we obtain modulus, initial peak load, ultimate load, ultimate displacement and work to failure by small punch test. The result of experiment shows changing irradiation doses and annealing time make no significant differences in each properties. Ultimate load、ultimate displacement and work to failure are improved by crosslinking. The OI、density、crystalline degree、ultimate load 、 ultimate displacement and the stability of dimension can be kept after aging when annealing temperature is over Tm. The changing aging time test shows that there are lag times of oxidation for OI, density and mechanical properties and each property changes a lot after the oxidation lag time. The lag time is inversely proportional to aging temperature. It shows that the degree of oxidation can be reflected sensitively by testing proper physical and mechanical properties. The result of acceleration aging experiment fits the oxidation model. OI is proportional to aging time, and the depth of subsurface is influenced by oxygen pressure.