本論文探討的重點為注入硼的單晶矽和多晶矽樣品的近表面處微結構、濃度分析、整個樣品的活化率、以及在樣品中的特定區域(像是團簇以及晶界處)與在一般晶粒的活化率差異。在實驗中,使用TEM來觀察樣品的近表面處微結構,會發現在離子佈植時形成的非晶矽會在經過熱處理後進行再結晶修復,轉變成單晶矽或是多晶矽。使用SIMS對樣品進行摻雜劑濃度的測量,可以得知原子擴散速率最快的是經過熱處理的多晶矽樣品,因為有溫度及晶界兩個條件來幫助原子向深處擴散。使用DHEM量測已退火樣品中的活性載子濃度、電阻率與載子遷移率,將載子濃度與SIMS和APT的濃度數據作比較,可計算出樣品中的載子活化率。使用APT來進行樣品的三維重構以及縱深濃度分析和小範圍的橫向濃度分析,從三維重構圖中可看到摻雜劑原子在樣品內部的分佈,觀察到B原子會聚集偏析在特定區域處(團簇以及晶界),並使用橫向取圖的方式取出偏析區域與一般原子正常分布區域的濃度曲線,再計算出局部的活化率。觀察活化率數據後可發現,在單晶矽樣品中,晶粒(原子正常分布的區域)的局部活化率為17.5 %,團簇區域的局部活化率為3.5 %;而在多晶矽樣品中,晶粒的局部活化率為30.9 %,晶界的局部活化率為14.7 %。較低的活化率代表在該區域中,活性載子所占比例較低,摻雜劑的去活性化比率較高。上面的數據顯示,活化率在原子聚集處會較低,驗證了B原子在矽材料中的偏析效應將會導致摻雜劑去活性化現象的發生。
This thesis focuses on the surface microstructures, concentration analysis, and activation ratios of bulk samples as well as in specific regions. Two types of silicon (Si) substrates, single crystal Si and polycrystalline Si (poly-Si), used in this work. In the experiments, TEM is used to observe the microstructures near the surface of the samples. It is found that the amorphous silicon (a-Si) formed during ion implantation and would recrystallize after heat treatment, transforming into single crystal Si or poly-Si. SIMS is used to measure the dopant concentration in the samples, revealing that the dopant diffusion rate of heat-treated poly-Si sample is faster than others due to the assistance of temperature and grain boundaries. DHEM is used to measure the active carrier concentration, resistivity, and carrier mobility in annealed samples. By comparing the carrier concentration with the B concentration data from SIMS and APT, the activation ratios in the samples can be calculated. APT is utilized for three-dimensional (3D) reconstruction, depth concentration analysis, and small-scale lateral concentration analysis of the samples. The 3D images show the distribution of dopant atoms, with B atoms observed to aggregate in specific areas (such as clusters and grain boundaries). By taking lateral concentration profiles of the segregation areas and normal areas, local activation ratios can be calculated. In single crystal Si samples, the local activation ratio in grains (areas with normal atomic distribution) is 17.5 %, while in cluster regions it is 3.5 %. In poly-Si samples, the local activation ratios in grains and grain boundaries are 30.9 % and 14.7 %, respectively. The data show that B atoms tend to segregate in clusters rather than in grain boundaries, significantly decreasing the carrier activation.
顯示完整詮釋資料 統計資料

引用此條目

李依遙 (2024). 硼摻雜矽基板之摻雜劑分佈與電性縱深分析. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/3685

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享

永久網址:https://thesis.lib.nycu.edu.tw/handle/20.500.14371/3685