二氧化鈰擔載釕金屬進行二氧化碳還原之研究: 擔體缺陷效應
Cerium Oxide Supported Ruthenium for Catalytic Reduction of CO2: Influence of Support Defect
摘要
傳統二氧化碳處理方法為二氧化碳捕獲及封存或二氧化碳捕獲及再利用技術,但其在實廠運用中仍需克服高成本之問題。整合二氧化碳捕獲及再利用 (Integrated CO2 capture and utilization)為近年來受廣泛研究的技術之一;其整合在在同一單元裡,同時同地捕獲並轉化二氧化碳。近幾年研究發現釕(Ru)金屬搭配氧化鈰(CeO2)對於轉化二氧化碳生成甲烷具有高活性;然大多相關研究著重於觸媒活性相之探討,鮮少有系統性的研究著重於CeO2擔體對整體觸媒之特性及二氧化碳甲烷化的活性的影響。為此,本研究旨在探討CeO2擔體的缺陷與Ru金屬相互作用及其對CO2催化還原效率及甲烷產量之影響,以突破現有已開發觸媒所需高操作溫度、低甲烷產率與低甲烷選擇性的瓶頸。
本研究以具有表面Ce缺陷的CevO2作為擔體,而Ru為活性金屬製備Ru/CevO2觸媒。CO2催化還原測試及物化分析結果指出,Ru為CO2甲烷化的活性位點,而CevO2擔體表面的Ce缺陷為決定Ru/CevO2觸媒表面RuOx特性的關鍵因子。XPS及TPR結果指出,CevO2擔體表面的高含量Ce缺陷可提升RuOx於CevO2擔體的分散性並且增加Ru/CevO2-280觸媒表面的Ru4+/Run+及Oβ比例;其為CO2吸附與活化的關鍵位點。CO2催化還原測試結果顯示,擔載2wt% Ru的Ru/CevO2-280觸媒為所有觸媒中具有最佳的甲烷產率(1.60 mmol/g)者。此外,Ru金屬含量對於Ru/CevO2-280觸媒的甲烷產量亦有顯著影響;最佳之4wt% Ru/CevO2-280觸媒具有2.94 mmol/g之甲烷產率。原位紅外光吸收光譜分析結果指出,吸附在Ru/CevO2-280表面的CO2會首先被轉化生成關鍵性的中間產物(Ru-CO與HCO3),再接著逐步被氫化形成甲烷。
本研究以具有表面Ce缺陷的CevO2作為擔體,而Ru為活性金屬製備Ru/CevO2觸媒。CO2催化還原測試及物化分析結果指出,Ru為CO2甲烷化的活性位點,而CevO2擔體表面的Ce缺陷為決定Ru/CevO2觸媒表面RuOx特性的關鍵因子。XPS及TPR結果指出,CevO2擔體表面的高含量Ce缺陷可提升RuOx於CevO2擔體的分散性並且增加Ru/CevO2-280觸媒表面的Ru4+/Run+及Oβ比例;其為CO2吸附與活化的關鍵位點。CO2催化還原測試結果顯示,擔載2wt% Ru的Ru/CevO2-280觸媒為所有觸媒中具有最佳的甲烷產率(1.60 mmol/g)者。此外,Ru金屬含量對於Ru/CevO2-280觸媒的甲烷產量亦有顯著影響;最佳之4wt% Ru/CevO2-280觸媒具有2.94 mmol/g之甲烷產率。原位紅外光吸收光譜分析結果指出,吸附在Ru/CevO2-280表面的CO2會首先被轉化生成關鍵性的中間產物(Ru-CO與HCO3),再接著逐步被氫化形成甲烷。
Conventional CO2 removal methods are CO2 capture and storage or CO2 capture and utilization, however, there is still a high-cost problem with the application. Integrated CO2 capture and conversion has recently been considered a promising technology in which CO2 adsorption and utilization are carried out simultaneously over dual-functional adsorbent/catalyst materials in a single reaction system. In this concern, developing dual-functional materials (DFMs) that combine excellent adsorption ability and catalytic property is required. Herein, we demonstrate a DFM combining MgO and Ru/Ce-defective CeO2 (denoted CevO2) for simultaneous CO2 capture and conversion for the first time.
The combined results of CO2 reduction tests and physicochemical analyses revealed that Ru served as the active site for CO2 methanation, and the surface Ce defects on the CevO2 support played a crucial role in determining the properties of RuOx species on the Ru/CevO2. XPS and TPR results indicated that a high concentration of Ce defect enhanced the dispersion of RuOx and increased the ratio of Ru4+/Run+ and Oβ on the catalyst surface, which are pivotal for CO2 adsorption and activation. The CO2 reduction results demonstrated that Ru/CevO2-280 catalyst loaded with 2wt% Ru exhibited the highest methane yield (1.60 mmol/g) among all the catalysts studied. The Ru loading significantly influenced the CH4 production yield of the Ru/ Ru/CevO2-280 catalyst, whereas the optimal 4wt% Ru/CevO2-280 catalyst showed a CH4 yield of 2.94 mmol/g. In situ DRIFT results indicated that the adsorbed CO2 on the Ru/CevO2-280 was activated into key intermediates (Ru-Co and HCO3), which were subsequently hydrogenated into CH4.
The combined results of CO2 reduction tests and physicochemical analyses revealed that Ru served as the active site for CO2 methanation, and the surface Ce defects on the CevO2 support played a crucial role in determining the properties of RuOx species on the Ru/CevO2. XPS and TPR results indicated that a high concentration of Ce defect enhanced the dispersion of RuOx and increased the ratio of Ru4+/Run+ and Oβ on the catalyst surface, which are pivotal for CO2 adsorption and activation. The CO2 reduction results demonstrated that Ru/CevO2-280 catalyst loaded with 2wt% Ru exhibited the highest methane yield (1.60 mmol/g) among all the catalysts studied. The Ru loading significantly influenced the CH4 production yield of the Ru/ Ru/CevO2-280 catalyst, whereas the optimal 4wt% Ru/CevO2-280 catalyst showed a CH4 yield of 2.94 mmol/g. In situ DRIFT results indicated that the adsorbed CO2 on the Ru/CevO2-280 was activated into key intermediates (Ru-Co and HCO3), which were subsequently hydrogenated into CH4.