摘要

釩鈦氧化物觸媒被廣泛應用於固定汙染源的氮氧化物去除;然而其僅於反應溫度300-400oC之間具有高脫硝效能。為因應減少能源消耗以及避免觸媒遭到毒化,開發具良好脫硝效率且同時具有抗二氧化硫毒化能力的中低溫觸媒為現今的主要研究方向。二氧化鈦為常見的觸媒擔體,其表面特性對於整體觸媒的特性與脫硝效能具有關鍵性的影響;為此,本研究旨在探討二氧化鈦擔體的表面特性對於釩鈦觸媒的特性、脫硝效能與抗毒化能力的影響。
本研究以氧化釩為活性金屬氧化物,並利用TiO2奈米片(TiO2 nanosheet,TNS)作為擔體合成V/TNS觸媒。研究結果顯示在重量流速為40,000 mL∙h-1∙g-1之條件下,V/TNS觸媒可在140-480°C溫度區間有高脫硝效率(> 90%)且同時保有高氮氣選擇性(>90%)。而脫硝穩定性測試結果顯示,以水熱溫度195oC製備之TNS-195擔載觸媒(V/TNS-195)為抗硫穩定性最佳之觸媒;其在反應溫度為160°C的條件下連續運行20小時仍然可以維持高脫硝效率(> 90%),顯示高催化穩定性。熱重分析結果指出觸媒表面的硫酸銨鹽為造成其失活的原因;觸媒表面上的硫酸銨鹽含量越高,觸媒失活的現象越嚴重。由物化分析、脫硝測試及脫硝穩定性測試等結果指出TNS擔體的水熱溫度會影響其表面氧缺陷及氫氧官能基的數量;TNS的表面氧缺陷及氫氧官能基的數量越高,V/TNS觸媒的表面氧缺陷及低價數V物種含量則越高,有助於增強其表面酸性與氧化能力,進而提升觸媒對於SO2的抵抗性。
V2O5/TiO2 catalyst has been widely applied for controlling NOx emissions from stationary sources. Nevertheless, they are active only over the reaction temperature of 300-400oC. To reduce energy consumption and avoid catalyst poisoning, developing medium and low-temperature catalysts with excellent deNOx efficiency and catalytic durability against SO2 has received considerable attention. TiO2 is commonly used in commercial and advanced SCR catalysts, and its surface properties critically influence the properties of the catalyst and its catalytic activity. This study aims to investigate the influence of the surface properties of TiO2 support on the physicochemical properties, deNOx efficiency, and catalytic durability against SO2 of VOx/TiO2 catalysts.
In this study, vanadium oxide was used as the active metal oxide, and TiO2 nanosheet (denoted TNS) was used as the support. Experimental results demonstrated that V/TNS catalysts achieved high NO conversion (>90%) and N2 selectivity (>90%) over a temperature range of 140-380°C at a WHSV of 40,000 mL∙h-1∙g-1.Moreover, the stability test revealed that the V/TNS-195 catalyst displayed excellent stability in the presence of SO2 and SO2H2O, exceeding over 90% NO conversion at 160°C during the 20-h reaction. The TGA results indicated that the formation of ammonium sulfate was responsible for the catalytic deactivation of the catalysts. The combined results of physicochemical and deNOx tests indicated that the high hydrothermal temperature promoted the formation of oxygen defects on the TNS supports. These oxygen defects facilitated the formation of low-coordinated V species and mobile oxygen species on the V/TNS catalysts, enhancing the surface acidity and redox property and, thus, the catalytic resistance against SO2.

所屬典藏

環境工程研究所
顯示完整詮釋資料 統計資料

引用此條目

許如溱 (2023). 釩鈦氧化物之低溫脫硝與SO2毒化影響研究:擔體的作用. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/421