過氧化鈉與氧氣氛對碳化矽氫氧化鉀蝕刻坑形貌與動力學的影響

Effects of sodium peroxide and oxygen atmosphere on the morphology and kinetic of silicon carbide potassium hydroxide etch pits

檔案

日期

2024

類型

語言

中文

摘要

碳化矽(SiC)和氮化鎵(GaN)作為第三代半導體的主要材料,因其優異的導熱
性和寬能隙特性,能夠承受高溫和大電流,成為目前最受關注的元件,特別適合應用
於高溫元件中。然而,SiC 晶體的生長過程具有相當的挑戰性,其缺陷會對元件性能造
成顯著影響。現階段,碳化矽主要以小尺寸晶圓為主,但隨著應用的日益廣泛,未來
勢必需要更大尺寸的晶圓。然而,在更大尺寸晶圓的生長過程中,缺陷的數量也將增
加。如果碳化矽在磊晶過程中無法及時識別這些缺陷,後續應用將受到這些缺陷的影
響,導致崩潰電壓下降,無法正常使用,而在通常情況下會利用 KOH 的蝕刻來進行缺
陷的判斷,但當 SiC 基板為 n-type 時便無法利用 KOH 就有效判斷出缺陷,於是便加入
了 Na2O2進行蝕刻。
此次實驗主要目的是判斷 Na2O2在加熱的過程中是否會產生變化進而導致失去其
功效,我們通過不同的加熱方式來確認其實驗結果,最後確認了在加熱的過程並不影
響 Na2O2的發揮,並推翻了參考資料所提到的 Na2O2會因為加熱而導致失去作用。而
這次實驗還有另一個目的則是判斷在不同的氣氛條件中是否會對 SiC 的蝕刻產生影
響,根據結果可以觀察出在相同溫度下氧氣氣氛可以使碳化矽得到較大的 TED 和
TSD,並且 TED 與 TSD 的大小差異也更大,更容易幫助我們區分不同的缺陷類型。
ilicon carbide (SiC) and gallium nitride (GaN), as the primary materials of thirdgeneration semiconductors, are gaining significant attention due to their excellent thermal
conductivity and wide bandgap characteristics, which enable them to withstand high
temperatures and large currents. These properties make them particularly suitable for hightemperature applications. However, the crystal growth process of SiC presents considerable
challenges, as defects can significantly impact device performance. Currently, SiC is mainly
produced in small-sized wafers, but with the increasing demand for applications, larger-sized
wafers will inevitably be needed in the future. However, as wafer size increases, the number
of defects also tends to rise. If these defects are not identified in a timely manner during the
epitaxy process, they will affect subsequent applications, leading to a decrease in breakdown
voltage and rendering the devices unusable.
Typically, KOH etching is used to identify defects, but it is ineffective for n-type SiC
substrates. To address this, Na₂O₂ is added for etching. The primary goal of this experiment
was to determine whether Na₂O₂ would undergo changes during heating that could
compromise its effectiveness. We tested different heating methods to verify this, ultimately
confirming that heating does not impair the function of Na₂O₂, thus disproving the claims in
the reference materials that suggested heating would cause Na₂O₂ to lose its effectiveness.
Another objective of this experiment was to assess whether different atmospheric conditions
would affect the etching of SiC. The results showed that, under the same temperature, an
oxygen atmosphere allows for larger TED (Threading Edge Dislocations) and TSD
(Threading Screw Dislocations) in silicon carbide, with a greater difference in size between
TED and TSD. This helps in more easily distinguishing between different types of defects
顯示完整詮釋資料 統計資料

引用此條目

王偉丞 (2024). 過氧化鈉與氧氣氛對碳化矽氫氧化鉀蝕刻坑形貌與動力學的影響. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/4285

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享

永久網址:https://thesis.lib.nycu.edu.tw/handle/20.500.14371/4285