藉由硼離子佈植形成高選擇比背面蝕刻停止層於晶圓減薄先進封裝
High Selectivity Backside Boron-Ion-Implantation Etch Stop Layer of Wafer Thinning for Advanced Packaging
摘要
在半導體製程技術不斷演進的環境中,因為人工智慧晶片高運算力的關係,電晶體微縮製程因物理極限而逐漸已無法滿足市場需求。三維積體電路(3D-IC)的先進封裝技術開始成為解決辦法,因此本研究將選擇專注於3D-IC中的晶圓薄化製程。晶圓薄化的優勢在於可以將多層堆疊的3D-IC中的每一片都縮小到極限的尺寸,使得整體的封裝尺寸能更進一步減少,讓晶圓薄化成為一個未來的發展方向。這項研究提出一個創新的硼離子佈值製程來形成薄化過程中的蝕刻停止層,此製程相較其他方法能減少成本,提高產量。我們先以穿透式電子顯微鏡(TEM)和二次離子質譜分析儀(SIMS)分析高硼離子參雜的停止層結構,下一階段比較了不同濕蝕刻液包含氫氧化鉀(KOH)和KOH + 異丙醇(IPA)的混合溶液對於硼離子蝕刻停止層的蝕刻選擇比影響,使用表面輪廓儀測量蝕刻深度以換算成選擇比,其中最高的蝕刻選擇比在KOH + IPA, 60度的情況下高達512。也使用原子力顯微鏡(AFM)分析不同濕蝕刻參數對於表面粗糙度的影響。最後一階段則實際進行兩片晶圓的接合,再對含有停止層的晶圓做粗磨、細磨、化學機械研磨和濕蝕刻一系列的晶圓薄化製程來驗證此方法,用聚焦離子束(FIB)製備的掃描電子顯微鏡(SEM)橫切面圖來驗證薄化製程完成後的極薄晶片結構,而最後的極薄晶片結構為大約400奈米。
In the ever-evolving landscape of semiconductor processing technology, the high computational power of AI (Artificial intelligence) chips has pushed the limits of transistor miniaturization, making it increasingly unable to meet market demands due to physical constraints. Advanced packaging technologies, such as three-dimensional integrated circuit (3D-IC), have emerged as a solution. Therefore, this study focuses on the wafer thinning process in 3D-IC. The advantage of wafer thinning is that it can reduce each layer in a multi-layered 3D-IC to its minimal size, further decreasing the overall packaging size, and making wafer thinning a future development direction. This study proposes an innovative boron ion implantation process to form an etch stop layer (ESL) during thinning. Compared to other methods, this process reduces costs and increases yield. Initially, we analyzed the high boron ion-doped stop layer structure using Transmission Electron Microscopy (TEM) and Secondary Ion Mass Spectrometry (SIMS). In the next stage, we compared the etch selectivity of different wet etching solutions, including potassium hydroxide (KOH) and a mixture of KOH and isopropyl alcohol (IPA), on the boron ion etch stop layer. The etch depth was measured using a surface profilometer to calculate the etch selectivity, with the highest etch selectivity reaching 512 under KOH + IPA solution at 60 degrees Celsius. We also used Atomic Force Microscopy (AFM) to analyze the impact of different wet etching parameters on surface roughness. In the final stage, two wafers were bonded together, and a series of wafer thinning processes, including coarse grinding, silicon grinding, chemical mechanical polishing, and wet etching, were performed on the wafer containing the stop layer to verify this method. The extremely thin chip structure after the thinning process, verified using Focused Ion Beam (FIB) prepared Scanning Electron Microscope (SEM) cross-sectional images, was ultimately 400 nanometers thick.