於聚對苯二甲酸乙二酯軟性基板上以低溫電漿輔助化學氣相沉積多層碳氮化矽/聚苯乙烯高性能水氣阻障膜
顯示簡易詮釋資料 統計資料| 欄位 | 內容 | 語言 |
|---|---|---|
dc.contributor.advisor |
呂志鵬、呂志鵬 | |
dc.contributor.advisor |
Jihperng Leu、Jihperng Leu | |
dc.contributor.author |
許書豪 | |
dc.contributor.author |
Shu-Hao Syu | |
dc.contributor.college |
工學院 | |
dc.contributor.committee |
||
dc.contributor.committee |
||
dc.contributor.department |
材料科學與工程學系所 | |
dc.contributor.studentid |
9818549 | |
dc.date.NCLavailable |
2017/02/17 | |
dc.date.USTavailable |
2017/02/17 | |
dc.date.issued |
2012 | |
dc.date.issuedROC |
101 | |
dc.date.paperavailable |
立即公開 | |
dc.date.schoolyear |
100 | |
dc.description.abstract |
有機元件像是,有機發光二極體、太陽能電池,在元件內部的電極、反應的主體都極易遭受到水氣和氧氣的攻擊,導致元件損壞。為了要延長有機元件的壽命,有機元件的封裝面臨了許多不可避免挑戰。最近有一個較為普遍的方法叫做“薄膜封裝“,他是直接在元件的基板上,鍍一層阻氣的薄膜。但是這之中還是有許多的問題存在,例如:在鍍膜的過程中,由於溫度太高,導致熱應力殘留,而使阻水阻氣的效果大為降低。 因此,一個有效的水氣阻障層,碳氮化矽和複合的碳氮化矽、聚苯乙烯薄膜被成功的開發出來與製備。吾人利用VSZ (1,3,5-trimethyl-1,3,5-trivinylcyclo- trisilazane)與Styrene在低溫電漿輔助化學沉積的系統在軟性聚對苯二甲酸乙二酯基板上沉積SiCxNy和PS (Polystyrene)阻障層。且利用自行組裝的鈣氧化電阻變化式的高靈敏度水氣穿透量測儀去量測阻障層的效果。我們可以得到單層SiCxNy 100nm可以將WVTR (water vapor transmit rate)從3降到5×10-2 g/m2/day.多層結構SiCxNy 可以更有效的降低WVTR到6×10-3g/m2/day.而單層複合阻障層SiCxNy/PS可以有效的降低WVTR到8×10-3g/m2/day.最後我們利用四層複合阻障層SiCxNy/PS可以得到一個極低的WVTR,8×10-3g/m5/day. 再者,為了要證實多層阻障層的效果,我們利用一個快速檢測阻障層缺陷的方法去佐證。我們利用電鍍鎳的方式去找出阻障層缺陷的數量,然後發現缺陷的數量與WVTR有正相關,於是得到多層結構可以有效的降低WVTR。其主要原因為多層結構會導致缺陷的不連續,而延長了水氣穿透的路徑,和在沉積上方的阻障層時,下方薄膜的缺陷會被癒合,進而減少了水氣穿透的路徑。 | |
dc.description.abstract |
Moisture and oxygen permeation barrier technology become critical in achieving the required lifetime reliability of flexible devices such as flexible organic light-emitting diode (FOLED) and flexible solar cells. To date, thin-film encapsulation using multilayered organic/inorganic barriers on flexible polymer substrate is the most promising. However, there are still several challenging issues such as defects and cost. This study first established a water-vapor-transmission-rate (WVTR) measurement system with a high sensitivity (~10-5 g/m2/day). Next we developed a high-performance moisture barrier (8x10-5 g/m2/day) on flexible PET substrate. This is achieved by an alternating organic barrier (plasma polymerized polystyrene, PPS)/inorganic barrier, silicon carbonitride (SiCxNy) multi-layered structure, using plasma-enhanced chemical vapor deposition (PECVD) at room temperature and without breaking the vacuum, based on 1,3,5-trimethyl-1,3,5-trivinylcyclo-trisilazane (VSZ) and styrene precursor, respectively. The effects of barrier materials, their thicknesses, and the numbers of layer on WVTR, and the controlling mechanism were also investigated. A single SiCxNy barrier layer (100 nm) effectively reduces the WVTR of a PET film from 3 g/m2/day to 5×10-2 g/m2/day. Multi-layered moisture barrier structures based on triple SiCxNy barrier layers or SiCxNy/PPS/SiCxNy (100 nm each) can further reduce WVTR to 6×10-3 and 8×10-3 g/m2/day, respectively. In summary, multi-layered barrier can effectively reduce WVTR as compared to single layer at the same total thickness. Also, moisture barrier materials consisting of alternating SiCxNy and PPS multi-layered stack (4-pair with a total thickness of 0.8 □m) can effectively reduce WVTR down to 8×10-5 g/m2/day. Through the pinhole decoration by Ni electro-deposition, the mechanism of high-performance WVTR in a multilayered barrier can be attributed to the much increase in diffusion paths due to a reduction of pinhole defects healed by the alternating deposited, upper layer. | |
dc.description.abstractopendate |
||
dc.description.degree |
碩士 | |
dc.description.tableofcontents |
摘要 IIAbstract IVAcknowledgements VIContents VIIList of tables IXList of figures XChapter 1 Introduction 11.1Background 11.2 Overview 3Chapter 2 Literature Review 42.1 Moisture degradation in flexible devices 42.1.1 Moisture degradation in solar cells 42.1.2 Moisture induced degradation in organic light-emitting-diode 82.1.3 Organic light-emitting-diode degradation by substrate 102.2 The current methods on prevention the moisture ingress 122.3 Techniques and Instruments for Measuring WVTR 142.3 Mechanisms of vapor permeation through multilayer barrier films 172.4 Passivation Technology by SiCxNy 202.5 Defect decoration 23Chapter 3 Experimental 263.1 Sample preparation 263.1.1 Chemicals 263.1.2 Experimental procedures 273.2 Plasma Enhance Chemical Vapor Deposition SiCxNy and Polystyrene 283.3 Analytic instrument 303.3.1 n&k analyzer 303.3.2 X-ray reflectivity (XRR) 303.3.3 Fourier transform infrared spectroscopy (FTIR) 313.3.4 Atomic force microscope (AFM) 313.3.5 FE-SEM 313.3.6 Nano-Indantation 313.4 Water vapor transmission rate (WVTR) 323.5 Pinhole density quantification 343.5.1 Decoration by electro-deposition 343.5.2 Pinhole numbers analysis by Image J 36Chapter 4 Results and Discussion 394.1 FTIR of SiCxNy and PS Chemical structure 394.1.1 Chemical structure of SiCxNy 394.1.2 Chemical structure of PS 424.2 Basic properties of SiCxNy barrier 444.2.1 Roughness of barrier layer 444.2.2 Density of SiCxNy thin film, elastic modulus, and thickness 464.3 WVTR of multi-barrier layer on PET substrate 464.3.1 Sensitivity of home built WVTR system 464.3.2 Effect of SiCxNy multi-barrier layer 484.3.3 Influence of hybrid (SiCxNy /PS) multilayer 524.4 Pinhole density quantification by SEM 564.5 Correlation between pinhole density and WVTR 63Chapter 5 Conclusions 65References 67 | |
dc.identifier.citation |
[1] M.B. Schubert, J.H. Werner, Material Today, 9, 42 (2006).[2] L. Han, K. Song, P. Mandlik, S. Wagner, Appl. Phys. Lett., 96, 042111 (2010)[3] H. Cho, C. Yun, J.W. Park, S. Yoo, Org. Electron., 10, 1163 (2009).[4] A.B. Chwang, M.A. Rothman, S.Y. Mao, R.H. Hewitt, M.S. Weaver, J.A. Silvernail, K. Rajan, M. Hack, J.J. Brown, X. Chu, L. Moro, T. Krajewski, N. Rutherford, Appl. Phys. Lett., 83, 413 (2003).[5] E. Vassallo, A. Cremona, F. Ghezzi, F. Dellera, L. Laguardia, G. Ambrosone, and U. Coscia, Appl. Surf. Sci., 252, 7993 (2006).[6] J. Fahlteich, M. Fahland, W. Schonberger, and N. Schiller, Thin Solid Films 517, 3075 (2009).[7] M. Schaer, F. Nuesch, D. Berner, W. Leo, L. Zuppiroli, Adv. Funct. Mater., 11, 116 (2001).[8]M. J. Chen, Y. T. Shih, M. K. Wu, and F. Y. Tsai, JAP., 101, 033130 (2007)[9] J. Fathlteich, M. Fahland, W. Schonberger, N. Schiller, Thin solid film, 517, 3075 (2009.)[10] P.E. Burrows, G.L. Graff, M.E. Gross, P.M. Martin, M. Hall, E. Mast, C. Bonham, W.Bennet, L. Michalski, M. Weaver, J.J. Brown, D. Fogarty, L.S. Sapochack, Proc. SPIE, 4105, 75 (2001).[11]D. Li, E. J. Borkent, R. Nortrup, H. Moon, H. Katz, and Z. Bao, Appl. Phys. Lett. 86, 042105 (2005).[12] H. Nishiwaki, K. Uchihashi, K. Takaoka, M. Nakagawa, H. Inoue, A. Takeoka, S. Tsuda, and M. Ohnishi, Sol. Energy Mater. Sol. Cells 37, 295 (1995).[13] M. K. Quintana, D. L. King, T. J. McMahon and C. R. Osterwald, Conference record of the twenty-ninth IEEE photovoltaic specialists conference, 1436 (2002).[14] E. E. van Dyk, A. Audouard, E. L. Meyer, and C. D. Woolardb, Sol. Energy Mater. Sol. Cells 91, 167 (2007).[15] J. Mikkel, N. Kion, and C. K. Frederik, Sol. Energy Mater. Sol. Cells 92, 686 (2008).[16] G. Dennler, C. Lungenschmied, H. Neugebauer, N. S. Sariciftci, M. Latreche, G. Czeremuszkin, and M. R. Wetheimer, Thin Solid Films 511, 349 (2006).[17] C. H. Chen, OLED/Organic Electroluminescent Materials and Devices, Wunan, (2005).[18] H. C. Langowski, 46th Annual Technical Conference Proceedings of the Society of Vacuum Coaters , 559 (2003).[19] M. Schaer, F. Nuesch, D. Berner, W. Leo, and L. Zuppiroli, Adv. Funct. Mater. 11, 2 (2001).[20] L. Ke, R. S. Kumar, K. Zhang, S. J. Chua, A.T.S. Wee, Synth. Met., 140, 295 (2004).[21] J. A. McCormick, K. P. Rice, D. F. Paul, A. W. Weimer, and S. M. George, Chem. Vap. Deposition, 13, 491 (2007)[22] K. Mizuno, B. K. Gan, A. Kondyurin, M. M. Bilek, and D. R. McKenzie, Process. Polym. 5, 834 (2008).[23] D. G. Howells, B. M. Henry, Y. Leterrier, J. A. E. Manson, J. Madocks, and H. E. Assender, Surf. Coat. Technol. 202, 3529 (2008).[24] A. G. Erlat, B. M. Henry, J .J. Ingram, D .B. Mountain, A. McGuigan, R .P. Howson, C. R. M. Grovenor, G. A. D. Briggs, and Y. Tsukahara, Thin Solid Films 388, 78 (2001).[25] M. C. Lin, L. S. Chang, and H. C. Lin, Appl. Surf. Sci 254, 3509 (2008).[26] P. F. Carcia, R. S. McLean, M. H. Reilly, and S. M. George, Appl. Phys. Lett., 89, 031915(2006).[27] J. H. Choi, Y. M. Kim, Y. W. Park, J. W. Huh, B. K. Jua, I. S. Kim and H. N. Hwang, Rev. Sci. Instrum., 78, 064701 (2007).[28]R. Paetzold, D. Henseler, K. Heuser, V. Cesari, W. Sarfert, G. Wittmann, A. Winnacker, Proceedings of SPIE, 5214, 73 ( 2004)[29] Y. Chen, and Y. Li, Int. J. Pharm. 358, 137 (2008).[30] R. Dunkel, R. Bujas, A. Klein, and V. Horndt, Journal of Society for Information Display 13, 7 (2005).[31] J. Lewis, Materials Today, 9, 4 (2006)[32] G. L. Graff, R. E. Williford, and P. E. Burrows, Journal of Applied Physics 96, 4, (2004)[33] J. Greener, K. C. Ng, K. M. Vaeth, T. M. Smith, Journal of Applied Polymer Science, 106, 3534 (2007)[34] H. Nakayama and M. Ito, Thin Solid Films, 519, 4483 (2011)[35] A. Badzian, T. Badzian, W.D. Drawl, R. Roy, Diamond Relat, Mater. 7, 1519 (1998).[36] L.C. Chen, K.H. Chen, S.L. Wei, P.D. Kichambare, J.J. Wu, T.R. Lu, C.T. Kuo, Thin Solid Films, 112, 355 (1999).[37] H.L. Chang, C.T. Kuo, Diamond Relat. ,Mater., 10, 1910 (2001).[38] X.C. Wu, R.Q. Cai, P.X. Yan, W.M. Liu, J. Tian, Appl. Surf. Sci., 185, 262 (2002).[39] P. Jedrzejowski, J. Cizek, A. Massian, J.E. Klemberg-Sapieha, J. Vlcek, L. Martinu, Thin Solid Films, 201, 447 (2004).[40] L.C. Chen, C.K. Chen, S.L. Wei, D.M. Bhusari, K.H. Chen, Y.F. Chen, Y.C. Jong, Y.S. Huang, Appl. Phys. Lett., 72, 2463 (1998).[41] Z. Chen, H. Lin, J. Zhou, Z. Ma, E. Xie, Journal of Alloys and Compounds 48, 531 (2009)[42] T. Sakurai, IEEE Trans. Electron. Devices, 40, 118 (1993)[43] International Technology Roadmap for Semiconductors, executive summary (2007).[44] Zs. Tokei, Y.-L. Li and G.P. Beyer, Microelectron. Reliab., 45, 1436 (2005)[45] D. Shamiryan, T. Abell, Q.T. Le and K. Maex, Microelectr. Eng., 70, 341 (2003)[46] B. D. Schrag, X. Liu, W. Shen and G. Xiao, Appl. Phys. Lett., 84, 2937 (2004)[47] A. Schulz, D.Herrmann, F. Kessler, J. Schneider, M. Walker and U. Schumacher, Surf. and Coat. Techol., 200, 213 (2005)[48] R. Schad, D. Allen, G. Zangari, I. Zana, D. Yang, M. Tondra, D. Wang, Appl. Phys. Lett., 76, 607 (2000)[49] A. R. Forouhi and I. Bloomer, Phys. Rev. B., 34, 7018 (1986).[50] C. M. Wang, Materials Analysis, Materials Research Society (1998).[51] E. Vassallo, A. Cremona, F. Ghezzi, F. Dellera, L. Laguardia, G. Ambrosone, and U. Coscia, Appl. Surf. Sci., 252, 7993, (2006)[52] A. M. Coclite, G. Ozaydin-Ince, F. Palumbo, A. Milella, and K. K. Gleason, Plasma Process. Polym., 7, 561, (2010).[53] J. Lubguban, T. Rajagopalan, N. Mehta, B. Lahlouh, S. L. Simon, and S. Gangopadhyaya, J. Appl. Phys., 92, 1033, (2002).[54] T. A. Brooks and D.W. Hess, J. Appl. Phys., 64, 841, (1988).[55] H. Nakayama and M. Ito, Thin Solid Films, 519, 4483, (2011).[56]J. H. Lee, D. S. Kim, Y. H. Lee and B. Farouk, J. Electrochem. Soc., 143, 1451 (1996)[57]D. Merche, C. Poleunis, P. Bertrand, M. Sferrazza, and F. Reniers, IEEE Trans. on Plasma Science, 37, 951 (2009)[58] H. Windischmann, J. Appl. Phys, 62, 5 (1987)[59] M. Martyniuk, C.A. Musca, J.M. Dell, L. Faraone, Materials Science and Engineering B, 163, 26 (2009)[60] C. Igathinathane, L. O. Pordesimo, E. P. Columbus, W. D. Batchelor, S. R. Methuku, Comput. Electron. Agric., 63, 168 (2008)[61] R. Schad, D. Allen, G. Zangari, I. Zana, D. Yang, M. Tondra, D. Wang, Appl. Phys. Lett., 76, 607 (2000)[62] T.W. Scharf, J. Gong, G. Zangari, and J.A. Barnard, Appl. Phys. A, 74, 827 (2002) | |
dc.identifier.uri |
https://hdl.handle.net/20.500.14371/49549 | |
dc.language.iso |
英文 | |
dc.relation.alma |
990050730670206772 | |
dc.relation.page |
70 | |
dc.subject.keyword |
薄膜封裝 | |
dc.subject.keyword |
碳氮化矽 | |
dc.subject.keyword |
水氣量測 | |
dc.subject.keyword |
||
dc.subject.keyword |
||
dc.subject.keyword |
WVTR | |
dc.subject.keyword |
moisture | |
dc.subject.keyword |
SiCxNy | |
dc.subject.keyword |
barrer layer | |
dc.subject.keyword |
pinhole | |
dc.title |
於聚對苯二甲酸乙二酯軟性基板上以低溫電漿輔助化學氣相沉積多層碳氮化矽/聚苯乙烯高性能水氣阻障膜 | zh-TW |
dc.title |
Low-temperature PECVD deposited SiCxNy/polystyrene multi-layered, high-performance moisture barrier on flexible PET fil | en |
dc.type |
Thesis | zh-TW |
檔案
- 854901.pdf (2.43 MB, Adobe PDF)
所屬典藏: 材料科學與工程學系
引用此條目
Shu-Hao Syu (2012). Low-temperature PECVD deposited SiCxNy/polystyrene multi-layered, high-performance moisture barrier on flexible PET fil. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/49549
引用文字依 APA 第 7 版格式自動產生,使用前請再核對。
分享
永久網址:https://thesis.lib.nycu.edu.tw/handle/20.500.14371/49549