TiAlCr與TiAlCrNb之相圖建構、結構鑑定及其富Ti合金之機械性質探討

Phase diagram construction, structural characterization for TiAlCr and TiAlCrNb systems, and investigation of the mechanical properties of Ti-rich TiAlCr and TiAlCrNb alloys

檔案

日期

2023

類型

語言

中文

摘要

富鈦中熵合金有低密度、高比強度和高延展性的特性,是具有潛力的輕量化合金。雖然鑄態之富鈦中熵合金大多具有單相固溶體之微結構,但在高溫工作環境下可能產生的二次相將劇烈影響合金的機械性質。當大量脆性二次相生成時,將導致合金延展性急劇下降,更易發生脆性斷裂。
因此我們以實際實驗之方法,建構Ti-Al-Cr和Ti65-Al-Cr-Nb之液相線投影圖和1273 K等溫橫截面,藉此尋找具有高溫相穩定性的組成以輔助合金設計,再搭配密度與機械性質的量測,開發同時具有輕量化、高溫相穩定性和卓越機械性能的合金組成。我們亦運用國家同步輻射研究中心提供的高解析度同步輻射光源更深入的分析合金結構,確認了B2相在這兩個系統中的存在。在機械性質的量測上,在Ti-Al-Cr三元合金中A1(Ti75Al7Cr18)合金具有最佳的壓縮性質,不僅在1273 K下退火14天後仍舊保有超過30 %的壓縮應變量之外,更具有高達1254.96 MPa的壓縮降伏強度。在Ti65-Al-Cr-Nb四元合金系統中,N3 (Ti65Al11.67Cr11.67Nb11.66)合金具有最佳的拉伸性質,具有840.75 MPa的拉伸降伏強度,並且還有15.35 %的拉伸應變量。
Ti-riched medium-entropy alloys(MEAs) possess the potential as lightweight materials due to their combination of low density, high specific strength, and ductility. Although as-cast Ti-riched MEAs often possess a single-phase solid solution microstructure, the secondary phases that may form in high-temperature operating environments can profoundly impact the mechanical properties of these alloys. The formation of a significant amount of brittle secondary phases can lead to a sharp decrease in alloy ductility and an increased susceptibility to brittle fracture.
Addressing this challenge, we employed practical experiment to construct liquidus projections and 1273K isothermal sections for both the Ti-Al-Cr and Ti65-Al-Cr-Nb systems. This approach aims to identify compositions with high-temperature phase stability to assist in alloy design. Coupled with measurements of density and mechanical properties, we aim to develop alloy compositions that simultaneously possess lightweight characteristics, high-temperature phase stability, and exceptional mechanical performance. We further utilized the high-resolution synchrotron radiation source provided by the NSRRC for in-depth analysis of alloy structures, confirming the presence of the B2 phase in both of these systems. In terms of mechanical characteristics, in the Ti-Al-Cr ternary alloy, the A1 (Ti75Al7Cr18) alloy demonstrated optimal compressive properties, maintaining over 30% compressive strain even after a 14-day annealing period, alongside a remarkable compressive yield strength of 1254.96 MPa. In the Ti65-Al-Cr-Nb quaternary alloy system, the N3 (Ti65Al11.67Cr11.67Nb11.66) alloy displayed the best tensile properties, including a tensile yield strength of 840.75 MPa and a substantial tensile strain of 15.35%.
顯示完整詮釋資料 統計資料

引用此條目

王子瑜 (2023). TiAlCr與TiAlCrNb之相圖建構、結構鑑定及其富Ti合金之機械性質探討. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/516

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享

永久網址:https://thesis.lib.nycu.edu.tw/handle/20.500.14371/516