循環負載下牙科黏著層破裂檢測與臨床應用
Monitoring Dental Adhesive Layer Failure and Clinical Application under Cycling Load
摘要
針對大範圍缺損之牙冠,近年來結合電腦輔助設計系統製造陶瓷復形體,並以牙科黏著劑連結剩餘齒質,恢復牙體結構。在復形初期雖能提供良好的黏著強度,但在長期咬合下,黏著層內部容易產生裂紋導致復形體脫落,目前對於黏著層破裂情形仍不清楚,因此將利用音洩系統進行黏著層裂紋檢測,探討受力過程中黏著層之破裂情形,並利有限元素分析,探討復形體的幾何設計對於黏著層內部應力之影響,最後將音洩系統應用於復形牙的體外測試上,監測其裂紋成長情形。首先,本研究將牙科陶瓷藉由黏著劑黏貼於剩餘齒質(牙釉質/牙本質)上,以循環負載模擬口腔咬合,對黏著層進行體外剪力測試,並在實驗過程中以音洩系統監測黏著層破裂情形,最後利用光學同調斷層造影術(OCT)觀察黏著層有無裂紋產生,驗證音洩系統能監測黏著層破裂情形。在電腦模擬分析中,利用Micro-CT擷取小臼齒影像,藉由影像重組方式獲得其輪廓線,匯入有限元素軟體建構出小臼齒模型,並設計四種MODP復形體(Without slot (WOS)、Slot (S)、Coverage (CWOS)、Coverage with slot (CWS))觀察牙體內部應力分布情形並進行疲勞分析,模擬復形牙在反覆咬合下之使用壽命。最後以音洩系統監測復形牙在體外力學測試(靜態/動態)中的裂紋產生情形。研究結果顯示,當偵測到音洩訊號時以OCT觀察黏著層發現有裂紋產生,驗證音洩系統確實能監測黏著層破裂情形。從剪力測試中發現當黏著層承受高負載時,黏著層內部容易產生災難性破壞(Catastrophic failure),但在低負載時,內部會不斷產生小裂紋,導致陶瓷塊剝落。在有限元素分析中,發現Coverage設計(WOS V.S. CWOS)在承受軸向力時,能降低黏著層上的應力,並明顯的增加使用壽命,而Slot設計(WOS V.S. S)不論在承受軸向力或側向力,對於黏著層上的應力與壽命均無明顯影響。以MODP復形牙進行體外實驗,從靜態力學測試中發現復形體的外型設計對於斷裂強度沒有明顯的提升,但Coverage設計不論在靜態或著動態的軸向負載下均能減少復形牙裂紋產生。
Restorations, like veneer, crown, resin-bonded fixed prostheses and post and core, are routinely bonded to tooth substrates via the used of adhesive cement in the indirect adhesive procedures. Nevertheless, it is difficult to observe the fracture of the interface between the restoration and tooth until the interfacial failure. Therefore, the aim of this study is to investigate the behavior of micro-crack on the ceramic/cement/tooth interface using the fatigue test and acoustic emission (AE) technique. Using optical coherence tomography (OCT) have been used to observe the distribution the micro-crack to validate the results from AE technique. In addition, Four cavity(Without slot (WOS)、Slot (S)、Coverage (CWOS)、Coverage with slot (CWS)) was designed in a typical MODP restoration failure shape calculated fatigue life using finite element (FE) analysis. Finally, acoustic emission (AE) technique used in dental restorations in vitro tests, monitoring the crack growth. In the study, the AE technique and OCT images could potentially be used as a pre-clinical assessment tool to determine the integrity of cemented. When exposed to high load, adhesive layer prone to brittle fracture. But at low load, the adhesive will continue to produce microcracks, lead to failure of restoration. In finite element (FE) analysis, we found that the coverage under the axial force, can reduce the stress on the adhesive layer, and increase the fatigue life. From in vitro tests found restorations design for improved without significantly improved of restorations fracture strength. However, coverage design of restorations could reduce the generation of cracks.