利用濕式蝕刻大間距圖形化藍寶石基板的側壁成長氮化鎵
GaN grown on the side plane of large size wet etching Patterned Sapphire Substrate
摘要
近幾年發光二極體(LED)廣泛的被應用於智慧照明與顯示方面,逐漸取代傳統燈源,許多方法被研發來改善GaN LED的內部量子效率(IQE)及光取出效率(LEE),其中圖形化藍寶石基板(PSS)因為可大量生產且同時可提升IQE和LEE,被大量用來製作LED的基板。由於藍寶石基板的結構為hexagonal,導致磊晶出來的GaN通常也是hexagonal結構的wurtzite相,其在[0001]方向上會因為內部電荷不均勻的緣故有內部極化的現象產生,此現象造成了量子侷限效應(Quantum Confine Stark Effect, QCSE),QCSE會造成IQE下降,根據實驗室早先的研究指出,透過濕蝕刻的方式製作的PSS可以透過(1 2 ¯3 5)面長出zinc-blende結構的GaN,zinc-blende結構為cubic,不會有內部極化的情形出現,所以能夠避免QCSE,本實驗希望能透過長時間的濕式蝕刻來製作出較大顆的PSS然後期望能在更大的E面上磊出大面積的zinc-blende GaN。
在前半部實驗我們利用黃光和濕蝕刻得到了大小約60μm的NO-PSS,而在磊晶後觀察到GaN在側壁長成片狀,透過PL和拉曼的分析都沒有找到zinc-blende的結構,最後透過TEM確定了磊晶關係為(0 ¯2 1)sap//(0 0 1)GaN,和學長實驗中的E面有一定差距。之後推論可能是底部的c-plane在磊晶過程中消耗太多磊晶氣體導致成長不出zinc-blende結構的GaN,接著在後半部的實驗利用黃光微影設法把底部露出的c-plane覆蓋上一層SiO2並將試片命名為WO-PSS,SEM影像看出確實成長成20µm厚的GaN代表一開始的構想是正確的,可以透過更長時間的蝕刻來獲得更大面積的側壁磊晶出更大顆的GaN,但是透過PL、拉曼、TEM的分析仍舊沒有找到zinc-blende GaN的訊號,但我們確定了磊晶之關係為(1 ¯2 2)sap//(0 0 2)GaN這組關係代表GaN是從藍寶石的(1 ¯2 2)面磊晶的,但是這組平面仍舊跟E面有一定的差距。我們推測是由於磊晶條件中溫度和壓力的影響使得zinc-blende不易成長。
在前半部實驗我們利用黃光和濕蝕刻得到了大小約60μm的NO-PSS,而在磊晶後觀察到GaN在側壁長成片狀,透過PL和拉曼的分析都沒有找到zinc-blende的結構,最後透過TEM確定了磊晶關係為(0 ¯2 1)sap//(0 0 1)GaN,和學長實驗中的E面有一定差距。之後推論可能是底部的c-plane在磊晶過程中消耗太多磊晶氣體導致成長不出zinc-blende結構的GaN,接著在後半部的實驗利用黃光微影設法把底部露出的c-plane覆蓋上一層SiO2並將試片命名為WO-PSS,SEM影像看出確實成長成20µm厚的GaN代表一開始的構想是正確的,可以透過更長時間的蝕刻來獲得更大面積的側壁磊晶出更大顆的GaN,但是透過PL、拉曼、TEM的分析仍舊沒有找到zinc-blende GaN的訊號,但我們確定了磊晶之關係為(1 ¯2 2)sap//(0 0 2)GaN這組關係代表GaN是從藍寶石的(1 ¯2 2)面磊晶的,但是這組平面仍舊跟E面有一定的差距。我們推測是由於磊晶條件中溫度和壓力的影響使得zinc-blende不易成長。
Recently, Light-emitting diodes (LEDs) are widely used in smart lightening and display and gradually replace traditional light sources. There are many ways to improved gallium nitride based LEDs’ internal quantum efficiency (IQE) and light extraction efficiency(LEE). Patterned sapphire substrates (PSS) are preferred due to advantages such as improving IQE, LEE and high production rate. The structure of sapphire is hexagonal, which cause GaN as wurtzite structure during epitaxy. Due to the internal polarization which caused by uneven electron distribution through [0001] direction of wurtzite GaN, it induced the Quantum Confine Stark Effect (QCSE). QCSE may decrease the IQE. According to our previous research, zinc-blende GaN can grow on (1 2 ¯3 5) plane of sapphire by wet etching process. Zinc-blende structure is cubic phase which don’t have problem about internal polarization, so that can avoid QCSE. In this experiment, we expect to obtain larger zinc-blende GaN by using wet etching for long enough time. For long period of time, we tried to get larger area of E-plane (1 2 ¯3 5) so that we can epitaxy large zinc-blende GaN.
In experiment 1 we use photolithography and wet etching to obtain NO-PSS(No bottom Oxide Patterned Sapphire Substrate) with size about 60μm. After epitaxy GaN, we found that GaN grown as flat type on the side plane of PSS. Through PL and RAMAN analysis, we didn’t find the zinc-blende structure. Then we confirm the epitaxy relationship between side plane of PSS and GaN is (0 ¯2 1)sap//(0 0 1)GaN by using TEM. (0 ¯2 1)sap is different from E plane. We thought that bottom c-plane consume too many precursor during epitaxy to grow zinc-blende GaN. In experiment 2, we covered 200nm SiO2 on bottom c-plane by PECVD and photolithography which called WO-PSS(With bottom Oxide Patterned Sapphire Substrate). SEM image show that GaN is almost 20µm thick which proved that what we think in beginning is true. We can obtain larger GaN by wet etching for long time. Through PL、RAMAN and TEM analysis we still didn’t find zinc-blende GaN signal. We confirm the epitaxy relationship between PSS and GaN is (1 ¯2 2)sap//(0 0 2)GaN ,but (1 ¯2 2)sap is still different from E-plane. Then we thought that temperature and pressure during epitaxy process is the main problem for zinc-blende to growth.
In experiment 1 we use photolithography and wet etching to obtain NO-PSS(No bottom Oxide Patterned Sapphire Substrate) with size about 60μm. After epitaxy GaN, we found that GaN grown as flat type on the side plane of PSS. Through PL and RAMAN analysis, we didn’t find the zinc-blende structure. Then we confirm the epitaxy relationship between side plane of PSS and GaN is (0 ¯2 1)sap//(0 0 1)GaN by using TEM. (0 ¯2 1)sap is different from E plane. We thought that bottom c-plane consume too many precursor during epitaxy to grow zinc-blende GaN. In experiment 2, we covered 200nm SiO2 on bottom c-plane by PECVD and photolithography which called WO-PSS(With bottom Oxide Patterned Sapphire Substrate). SEM image show that GaN is almost 20µm thick which proved that what we think in beginning is true. We can obtain larger GaN by wet etching for long time. Through PL、RAMAN and TEM analysis we still didn’t find zinc-blende GaN signal. We confirm the epitaxy relationship between PSS and GaN is (1 ¯2 2)sap//(0 0 2)GaN ,but (1 ¯2 2)sap is still different from E-plane. Then we thought that temperature and pressure during epitaxy process is the main problem for zinc-blende to growth.