不同厚度的鎳中間層對鋁與氧化鋁接合後之性質影響
Thickness Effect of Nickel Interlayer on the Properties after Aluminum and Alumina Interfacial Reactions
摘要
直接接合銅基板已被廣泛應用於電子元件的封裝與高功率元件之散熱上,但由於在熱循環下穩定性不佳,借鑒其技術,發展出了直接接合鋁基板。鋁與氧化鋁接合若要有良好之接合強度,通常要有中間反應相產生或利用熔融態之鋁來潤濕氧化鋁基板表面。本研究利用鎳作為中間層,當加熱至鋁-鎳共晶溫度以上時,即伴隨液相產生,利用此共晶液相來潤濕氧化鋁表面,可在較低溫接合鋁/氧化鋁,接合過程中通以氬氣氣氛,以防止鋁之氧化,並調整鎳中間層厚度,觀察對於鋁/氧化鋁接合後之性質影響。
本研究針對接合後之鋁/氧化鋁作界面與鋁層內部之微觀分析,並利用超音波掃描顯微鏡檢測鋁/氧化鋁接合處之孔洞分布,評估接合效果。隨著鎳膜厚增加,接合後鋁層內部有更多Al3Ni相生成,利用剪力試驗與雷射閃光法探討此相之生成對接合後熱性質與接合強度的影響,結果顯示:較厚的鎳中間層在接合後之直接接合鋁基板均有較高的界面強度與熱傳導係數,其熱傳導係數可達37Wm-1K-1,可應用於散熱基板。在電性量測部分,發現接合後含有Al3Ni之鋁層,其電阻相較接合前之純鋁沒有提升,並不會降低鋁的良好導電效果。
Al3Ni相可提升基板導熱效果,且由於較厚之鎳中間層,擴散後鋁層中有較高之鎳原子濃度,相對可在較低溫處生成液相,於氧化鋁基板表面有良好潤濕效果,來接合鋁/氧化鋁,但此Al3Ni介金屬相若生成於界面處,可能使直接接合鋁基板在冷卻過程中,產生較大熱應力,本研究即探討不同厚度之鎳中間層對接合後之鋁/氧化鋁界面性質之影響,來得到接合良好之鋁/氧化鋁基板。
本研究針對接合後之鋁/氧化鋁作界面與鋁層內部之微觀分析,並利用超音波掃描顯微鏡檢測鋁/氧化鋁接合處之孔洞分布,評估接合效果。隨著鎳膜厚增加,接合後鋁層內部有更多Al3Ni相生成,利用剪力試驗與雷射閃光法探討此相之生成對接合後熱性質與接合強度的影響,結果顯示:較厚的鎳中間層在接合後之直接接合鋁基板均有較高的界面強度與熱傳導係數,其熱傳導係數可達37Wm-1K-1,可應用於散熱基板。在電性量測部分,發現接合後含有Al3Ni之鋁層,其電阻相較接合前之純鋁沒有提升,並不會降低鋁的良好導電效果。
Al3Ni相可提升基板導熱效果,且由於較厚之鎳中間層,擴散後鋁層中有較高之鎳原子濃度,相對可在較低溫處生成液相,於氧化鋁基板表面有良好潤濕效果,來接合鋁/氧化鋁,但此Al3Ni介金屬相若生成於界面處,可能使直接接合鋁基板在冷卻過程中,產生較大熱應力,本研究即探討不同厚度之鎳中間層對接合後之鋁/氧化鋁界面性質之影響,來得到接合良好之鋁/氧化鋁基板。
Direct bonded copper (DBC) substrates have been widely used in power electronics and insulated gate bipolar transistors (IGBT) modules. However, poor thermal cycling reliability of DBC substrates restrict its applications. Direct bonded aluminum (DBA) substrates have been developed to replace DBC substrates due to its superior reliability. Previous studies used the silicon, germanium, silver, and copper as the interlayer to prepare DBA substrates. In this study, the Ni was selected and various thickness of nickel (100 nm、300 nm、500 nm) has been deposited on the Al2O3 substrate as the interlayer to join Al substrate by electron-beam evaporation. The specimens were then annealed at Al-Ni eutectic temperature (640℃) in argon atmosphere, the eutectic liquid phase formed at Al/Al2O3 interface to obtain better wettability. The purpose of present study is to analyze the microstructure of Al/Al2O3 contact by scanning electron microscopy (SEM) and transmission electron microscopy (TEM). Furthermore, scanning acoustic tomography (SAT) is used to reveal the voids distribution of Al/Al2O3 bonding layer for the purpose of evaluating the quality of DBA substrate. After joining of Al to Al2O3 with various thickness of nickel interlayers, Al3Ni phase were observed in the aluminum layer. The interfacial strength of Al/Al2O3 interfaces was measured by the shear strength test. The thermal conductivity of the sandwich (Al2O3/Al/Al2O3) specimens were measured by laser flash method. The resistivity of the aluminum layer with Al3Ni which was measured by four point probe. The results indicated that the interfacial strength of Al/Al2O3 interfaces and thermal conductivity of DBA substrates increased with the thickness of nickel interlayer increasing. The best thermal conductivity and shear strength of DBA specimens with 500 nm nickel interlayer was about 37 Wm-1K-1 and 31.5 MPa, respectively. In addition, comparing with the initial aluminum foil, the resistivity of aluminum layer with Al3Ni which was formed after Al/Al2O3 joint decreased insufficiently.