利用同步加速器光源技術研究基板溫度及通氧脈衝時間於二氧化鉿高介電材料的晶體及電子特性之效應
Effects of Deposition Temperature of Substrate and Oxygen Pulse Time on Crystalline and Electronic Properties of HfO2 High-k Dielectrics Studied by Synchrotron Radiation Techniques
摘要
本論文的研究工作著重於利用原子沉積法所製備的不同條件之TiN/HfO2/Si高介電材料閘極堆疊結構,藉由控制於沉積HfO2薄膜時的基板溫度與通氧脈衝時間,觀察薄膜內部及其界面的晶相、電子結構及化學鍵結特性。該研究主要利用同步加速器光源設施之X光繞射、X光吸收光譜及X光光電子能譜技術,並輔以第一原理模擬計算,獲得薄膜物理特性變化之重要資訊。
研究結果指出,於沉積HfO2的薄膜時,基板溫度與通氧脈衝時間會影響其晶體結構之成相比例與穩定性,尤以前者影響較巨。然而,對於晶相缺乏結構穩定性之條件下,沉積後的高溫退火可造成較高比例之Hf-O斷鍵效應,並因由HfO2與SiO2的密度差異而造成氧離子擴散至SiO2薄膜,產生一個由HfO2指向SiO2方向之內建電場,導致HfO2薄膜之費米能及能帶結構向下彎曲。
研究結果指出,於沉積HfO2的薄膜時,基板溫度與通氧脈衝時間會影響其晶體結構之成相比例與穩定性,尤以前者影響較巨。然而,對於晶相缺乏結構穩定性之條件下,沉積後的高溫退火可造成較高比例之Hf-O斷鍵效應,並因由HfO2與SiO2的密度差異而造成氧離子擴散至SiO2薄膜,產生一個由HfO2指向SiO2方向之內建電場,導致HfO2薄膜之費米能及能帶結構向下彎曲。
This study focused on the effects of deposition temperature of substrate and oxygen pulse time on the crystalline phase, electronic structure, and chemical bonding properties of TiN/ HfO2/Si high-k material metal-gate stacks and their interfaces with different preparation conditions. The thin films were deposited on the p-type Si substrate by atomic-layer deposition (ALD) method. We used various synchrotron radiation techniques of X-ray diffraction (XRD), extended X-ray absorption fine structure (EXAFS), and X-ray photoelectron spectroscopy (XPS), compared to the simulated results with first priciple calculation method, to obtain an important physical information of the TiN/HfO2/Si thin film system.
The research results indicate that the substrate temperature and the oxygen pulse time influence the phase composition and the structural stability during the deposition process of the HfO2 layer, especially for the former effect. For the absence of the structural stability, however, the post-annealing process can lead to a higher probability of the bond-broken Hf-O, contributing to the diffusion behavior of ionized oxygen atoms into the interface SiO2 of HfO2/Si due to the density diffenence of HfO2 and SiO2. This effect makes an electric field built in the interface of HfO2/Si, leading to the corresponding band bending and the Fermi energy lowering.
The research results indicate that the substrate temperature and the oxygen pulse time influence the phase composition and the structural stability during the deposition process of the HfO2 layer, especially for the former effect. For the absence of the structural stability, however, the post-annealing process can lead to a higher probability of the bond-broken Hf-O, contributing to the diffusion behavior of ionized oxygen atoms into the interface SiO2 of HfO2/Si due to the density diffenence of HfO2 and SiO2. This effect makes an electric field built in the interface of HfO2/Si, leading to the corresponding band bending and the Fermi energy lowering.