以限制效應合成奈米氧化鎂於ZIF-8應用於二氧化碳捕捉與轉酯化觸媒反應
MgO nanoparticles confined in ZIF-8 for CO2 capture and catalytic transesterification
摘要
本研究製備具高分散性之氧化鎂奈米顆粒於類沸石咪唑骨架材料ZIF-8的孔洞之中,並以奈米限制概念控制其顆粒大小。在本研究中,MgO@ZIF-8材料是由濕式沉澱法合成氫氧化鎂、並以鍛燒法兩步驟合成;X光繞射儀分析圖譜顯示出氧化鎂奈米晶粒之特徵峰成功在沒有其他雜質的出現下,合成於ZIF-8多孔基材之中,並透過Scherrer equation計算得知氧化鎂晶粒極小。在材料分析後,MgO@ZIF-8樣本被應用於二氧化碳吸附,其中50wt% MgO@ZIF-8樣本具有5.43wt% (1.23mmol/g)之吸附量,效果高於沒有ZIF-8分散的氧化鎂樣本。另一方面,在二氧化碳程序脫附實驗中,40 wt%之MgO@ZIF-8樣本之二氧化碳脫附溫度,相較於同系統下之標準品的脫附溫度降低約55℃。最後,將製備之MgO@ZIF-8進行轉酯化觸媒反應,發現對碳酸鹽有相當高的反應率,並推論一可能的反應機制,來解釋ZIF-8與氧化鎂之間可能存在的協同效應。
In this study, we prepared magnesium oxide (MgO) in the MOF (metal-organic framework) material ZIF-8 for carbon dioxide adsorption and transesterification purpose. Due to the microporosity of ZIF-8, nanoconfinement effect has been adopted to control well-dispersed MgO at ZIF-8 (denoted as MgO@ZIF-8) with different metal oxide loadings. MgO was prepared via wet precipitation of Mg(OH)2, which was further calcinated into MgO. From powder X-ray diffraction (PXRD), MgO crystals in ZIF-8 have small and regulated size, regardless of magnesium loadings. After material properties analysis, we apply our MgO@ZIF-8 for CO¬2 adsorption. 50% MgO@ZIF-8 showed an improved CO2 adsorption capacity (1.23mmol) than those of neat MgO and ZIF-8. On the other hand, CO¬2 desorption was tested with CO2-TPD. It was discovered that the lowest CO2 desorption temperature of 40% MgO@ZIF-8, 345°C, which is lowered by 55 degrees compared to the commercial magnesium carbonate. Finally, we tested the activity of MgO@ZIF-8 for transesterification catalytic reactions. It showed higher catalytic activities than their physically-mixed counterparts, indicative of a synergistic effect between MgO and ZIF-8, explained by a proposed mechanism based on acid-base bifunctional sites on the surface.