直流反應濺鍍TiZrN於Si (100)之異質磊晶成長與退火

Heteroepitaxial Growth and Annealing of DC Reactive Sputtered Titanium Zirconium Nitride on Si (100)

檔案

全文未公開。

日期

2019

類型

語言

中文

摘要

氮化鈦鋯(Titanium Zirconium Nitride,TiZrN)屬於NaCl型的面心立方體(Face-centered cubic, FCC)結構,具有高熔點、高硬度、生物相容性佳、高耐磨耗性等特性。本篇論文利用2吋且純度為99.9%之Ti0.68Zr0.32合金靶材以直流反應式磁控濺鍍法通入氬氣與氮氣沉積TiZrN薄膜,於Si (100)基板以及TiN薄膜上形成TiZrN磊晶薄膜與(TiZrN/TiN)多層膜,再以微波電漿高溫退火方式,改善磊晶品質,最後以X光繞射儀 (X-Ray Diffraction, XRD)、掃描式電子顯微鏡、原子力顯微鏡、掃描穿透式電子顯微鏡 (Scanning Transmission Electron Microscope, STEM)、四點探針、X光電子能譜等分析探討TiZrN薄膜於Si (100)基板跟TiN薄膜上的結晶情況與退火後TiZrN薄膜品質與性質變化。
論文第一部份主要探討不同的製程參數對TiZrN薄膜品質影響,藉由改變功率、製程壓力、薄膜厚度與靶材到基板間的距離以得到較佳品質的TiZrN薄膜,除此之外,使用TiN當作緩衝層並於其上濺鍍(TiZrN/TiN)多層膜藉此來得到更佳品質的TiZrN薄膜
第二部份利用微波電漿高溫退火TiZrN薄膜以及(TiZrN/TiN)多層膜藉此來提升試片磊晶品質,並比較退火前與退火後TiZrN薄膜的性質及結構變化。XRD分析顯示,直接濺鍍於Si (100)基板的TiZrN單層薄膜之最低之(200) X光搖擺曲線(X-Ray Rocking Curve, XRC)其半高寬(Full Width at Half Maximum, FWHM)為1.18度。另外,使用TiN當作緩衝層於其上濺鍍(TiZrN/TiN)多層膜,其TiZrN薄膜(200) XRC FWHM 為0.99度,由X-ray phi-scan掃描結果得知TiZrN薄膜與Si (100)基板之間的磊晶關係為TiN (100) // Si (100)且TiN [011] // Si [011]。XPS分析顯示,N與(Ti + Zr)之比例接近1 : 1,而Ti與Zr之間的原子組成約為17 : 8,STEM觀察TiZrN與Si界面的原子影像亦證實有磊晶之關係。退火部份,若使用微波電漿退火TiZrN/Si單層膜可使其 (200) XRC FWHM 由1.99度降至0.85度,其表面粗糙度(Root Mean Square Roughness, rms)為2.0 nm,(TiZrN/TiN)多層膜方面,退火可使TiZrN (200) XRC FWHM 由0.99度降至0.79度,表面粗糙度為12.2 nm。
Titanium Zirconium Nitride (TiZrN) with cubic NaCl structure has been widely applied because it has high melting temperature、high hardness、good biocompatibility and great wear resistance. This thesis studies the epitaxial growth of titanium zirconium nitride (TiZrN) films on Si (100) by DC reactive magnetron sputtering and the effects of microwave plasma on TiZrN. TiZrN films were deposited at near 860C using Ti0.68Zr0.32 alloy target with purity of 99.9 % at various powers, work pressures, film thicknesses and target-substrate distances by DC reactive magnetron sputtering. The first part of this thesis focuses on the influence of different process parameters on the microstate and properties of single-layer TiZrN. In addition, (TiZrN/TiN) multilayer was deposited on Si (100) substrate in order to improve film quality. In the second part, single-layer TiZrN and multilayer were annealed by microwave plasma with gas mixture of N2 and H2 to improve the epitaxial layer quality.
The crystallinity, lattice parameter, elemental composition, morphology of both single-layer TiZrN and multilayer (TiZrN/TiN) were characterized by x-ray diffraction (XRD)、scanning electron microscope、atomic force microscope、X-ray photoelectron spectrometry (XPS) and transmission electron microscopy. The electrical resistivitys were measured by four-point probe and Hall effect measurement systems.
For single-layer TiZrN, the XRD analysis showed that the lowest full width at half maximum (FWHM) of (200) x-ray rocking cuve (XRC) is 1.18 degree. In addition, (200) XRC FWHM of (TiZrN/TiN) multilayer was 0.99 degree. The epitaxial relationship of TiZrN on the Si (100) substrate is TiN (100) // Si (100) and TiN [011] // Si [011]. XPS analysis showed that the composition ratio of N to (Ti + Zr) was close to 1:1, and composition ratio between Ti and Zr was about 17 : 8.
After annealing, the single-layer TiZrN (200) XRC FWHM decreaseed from 1.99 degree to 0.85 degree, with surface roughness (Root Mean Square roughness, rms) about 2.0 nm. For the (TiZrN/TiN) multilayer, microwave plasma annealing can reduce its (200) XRC FWHM from 0.99 degree to 0.79 degree, with the surface roughness about 12.2 nm.
顯示完整詮釋資料 統計資料

引用此條目

傅家威 (2019). 直流反應濺鍍TiZrN於Si (100)之異質磊晶成長與退火. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/73152

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享

永久網址:https://thesis.lib.nycu.edu.tw/handle/20.500.14371/73152