Abstract
過去的研究中利用溶膠凝膠法將金屬釕(Ru)摻雜在La2Ti2O7的鈦(Ti)位置作為觸媒使用,其中La2Ti1.7Ru0.3O7為最佳化觸媒,在乙醇氧化蒸氣重組(OSRE)反應中具有最佳的活性。而本論文利用相同的製備方法,將鎂(Mg)、鈣(Ca)、鍶(Sr)分別部分摻雜在La2Ti1.7Ru0.3O7的鑭(La)位置,形成La2-xMgxTi1.7Ru0.3O7(x=0~0.1)、La2-xCaxTi1.7Ru0.3O7(x=0~0.2)、La2-xSrxTi1.7Ru0.3O7(x=0~0.2)系列觸媒。由於La1.8Mg0.2Ti1.7Ru0.3O7中出現RuO2雜相,因此後續鑑定和效率討論僅討論Ca、Sr系列觸媒。根據X光粉末繞射結構精算的結果得知,La2-xMxTi1.7Ru0.3O7(M=Ca、Sr)觸媒的相寬介於0~0.2之間。以X光電子能譜(XPS)和程序升溫還原(TPR)結果顯示,隨著Ca、Sr摻雜量的增加,高價態Ru≥4+相對百分比下降,氧空缺增加。效率測試的部分,本研究在C/O=0.7的條件下,分成固定外部熱源溫度300°C的OSRE反應,以及300°C啟動反應後,隨即關閉熱源,進行100小時長時間自放熱重組反應(ATRE)。在OSRE反應的部分,發現摻雜Ca、Sr可以有效促進水煤氣反應(WGS),WGS活性大小順序為La1.8Sr0.2Ti1.7Ru0.3O7>La1.8Ca0.2Ti1.7Ru0.3O7> La2Ti1.7Ru0.3O7。在100小時ATRE反應的部分,三個觸媒在反應後均維持穩定,其中La1.8Sr0.2Ti1.7Ru0.3O7/LZO在100小時反應後能維持最高的乙醇轉換率。經由熱重分析和拉曼圖譜鑑定反應後的觸媒,三者均未有碳沉積的訊號。La1.8Sr0.2Ti1.7Ru0.3O7/LZO在C/O=0.7、300°C啟動與自放熱反應條件下,經100小時反應後能維持最高的乙醇轉換率,因此是一個具有發展性的觸媒。
本論文另一個主題為利用原位漫散反射式傅立葉轉換紅外光譜儀研究鎳(Ni)金屬觸媒在不同水醇比以及不同載體上的反應機制,結果顯示Ni含浸在La2Zr2O7(LZO)上,LZO載體能有效的發揮促進甲烷蒸氣重組反應以及水煤氣反應的功用,避免甲烷、一氧化碳堆積在觸媒上,造成觸媒積碳失活。Ni金屬含浸在Al2O3上,在高溫下觸媒表面仍會有甲烷、一氧化碳以及大量的乙酸堆積,表示商用載體Al2O3並無法有效地促進含碳中間產物的轉換,因而增加觸媒表面積碳失活的機率。因此LZO作為觸媒載體,是一個具有潛力且相當合適的材料。
本論文另一個主題為利用原位漫散反射式傅立葉轉換紅外光譜儀研究鎳(Ni)金屬觸媒在不同水醇比以及不同載體上的反應機制,結果顯示Ni含浸在La2Zr2O7(LZO)上,LZO載體能有效的發揮促進甲烷蒸氣重組反應以及水煤氣反應的功用,避免甲烷、一氧化碳堆積在觸媒上,造成觸媒積碳失活。Ni金屬含浸在Al2O3上,在高溫下觸媒表面仍會有甲烷、一氧化碳以及大量的乙酸堆積,表示商用載體Al2O3並無法有效地促進含碳中間產物的轉換,因而增加觸媒表面積碳失活的機率。因此LZO作為觸媒載體,是一個具有潛力且相當合適的材料。
In previous study, we successfully synthesized the optimized solid solution La2Ti1.7Ru0.3O7 by sol-gel method and use it as a catalyst for oxidative steam reforming of ethanol(OSRE) reaction. In this research, we use the same method and successfully synthesized a series of La2-xMxTi1.7Ru0.3O7(M=Mg, Ca, Sr) catalysts. Due to the impurity phase RuO2 formed in La1.8Mg0.2Ti1.7Ru0.3O7, the characterization and performance study were focusing on La2-xMxTi1.7Ru0.3O7(M=Ca, Sr). According to powder X-ray diffraction(PXRD) and Rietveld structure refinement, the phase width of La2-xMxTi1.7Ru0.3O7(M=Ca, Sr) catalyst is between 0~0.2. X-ray Photoelectron Spectroscopy(XPS) and Temperature-Programmed Reduction(TPR) study indicates the relative percentage of high ruthenium oxidation state (Ru≥4+) decreased and the oxygen vacancy increased as the content of Ca, Sr increased. In the performance test, we fixed the C/O ratio at 0.7 and 300°C, and utilized OSRE reaction and 100 hour time on stream test under autothermal steam reforming of ethanol (ATRE) to evaluate the catalyst activity. In OSRE reaction, the results indicated the substitution of Ca and Sr can promote water gas shift reaction (WGS) reaction effectively. The order of WGS activity on catalysts is: La1.8Sr0.2Ti1.7Ru0.3O7 > La1.8Ca0.2Ti1.7Ru0.3O7 > La2Ti1.7Ru0.3O7. The used catalysts La1.8M0.2Ti1.7Ru0.3O7(M=Ca, Sr)/LZO and La2Ti1.7Ru0.3O7/LZO were not decomposed. The catalyst La1.8Sr0.2Ti1.7Ru0.3O7/LZO exhibits the highest ethanol conversion during the time on stream test and there is no sign of carbon deposition on used catalyst.
The second part of this thesis contains the Diffused Reflectance Infrared Fourier Transform Spectroscopy (DRIFT) study on the effect of support on reaction routes of nickel catalyst under different steam/ethanol ratio. The result indicates that using La2Zr2O7 as supporting material could promote methane steam reforming and water gas shift reaction effectively, which prevent the deposition of methane and carbon monoxide on the catalyst. On the other hand, using Al2O3 as supporting material shows low activity on the conversion of C1, C2 intermediate.There are significant amount of methane, carbon monoxide, and acetate attached on the surface of catalyst at high temperature(T=450~500°C) and thus promote the probability on deactivation of the catalyst. Therefore, La2Zr2O7 is a appropriate supporting material for metal or metal oxide catalyst.
The second part of this thesis contains the Diffused Reflectance Infrared Fourier Transform Spectroscopy (DRIFT) study on the effect of support on reaction routes of nickel catalyst under different steam/ethanol ratio. The result indicates that using La2Zr2O7 as supporting material could promote methane steam reforming and water gas shift reaction effectively, which prevent the deposition of methane and carbon monoxide on the catalyst. On the other hand, using Al2O3 as supporting material shows low activity on the conversion of C1, C2 intermediate.There are significant amount of methane, carbon monoxide, and acetate attached on the surface of catalyst at high temperature(T=450~500°C) and thus promote the probability on deactivation of the catalyst. Therefore, La2Zr2O7 is a appropriate supporting material for metal or metal oxide catalyst.
Collections
Department of Applied ChemistryCite this item
黃聿愷 (2019). 鹼土金屬摻雜鑭系層狀鈣鈦礦氧化物觸媒 La2-xMxTi1.7Ru0.3O7 (M = Mg, Ca, Sr) 對乙醇氧化蒸氣重組產氫反應的影響. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/73291