保護層對氧化亞錫薄膜電晶體特性之影響與長期穩定性之研究
Influences of passivation layers on the characteristics and stability of SnO thin film transistors
摘要
本論文藉由薄膜形貌工藝法製作p型氧化亞錫金屬氧化物電晶體,並研究使用電漿輔助化學氣相沉積系統,沉積三種不同保護層於氧化亞錫薄膜電晶體上,分別是TEOS-based SiO2、SiH4-based SiO2與SiNx。未覆蓋保護層的元件展現較一般文獻發表資料為佳的特性,如開關電流比~104、更陡的次臨界斜率(220mV/decade)與良好的場效遷移率(0.67cm2V-1s-1)。觀察保護層對元件電性的改變,發現TEOS-based SiO2會使元件失去特性呈短路的狀態。而SiH4- based SiO2則對元件特性影響小,與無保護層時的電性相當。SiNx則介於兩者之間,關閉電流過高。經過能量色散X射線譜、X-射線繞射分析、X射線光電子能譜分析與霍爾量測等材料分析,來了解保護層的沉積對氧化亞錫薄膜的改變,發現可能是因為TEOS-based SiO2與SiNx產生較高的熱預算而生成SnO2摻雜於氧化亞錫薄膜中,導致薄膜變質,產生更多的載子,使元件難以關閉,關閉區電流大幅上升。最後進行元件長期的量測,觀察保護層對元件長期穩定性幫助。保護層對元件有顯著的保護效果,無保護層在經過56天後,開關電流比剩下102,次臨界斜率增加434mV/decade。而使用SiH4-based SiO2則在56天後仍維持一樣的特性。
In this thesis, we study the influences of passivation layers on the operation of p-type SnO metal oxide thin-film transistors (MO TFTs) fabricated by the novel film-profile engineering scheme. Three kinds of passivation layers, namely, TEOS-based SiO2, SiH4-based SiO2 and SiNx were deposited on SnO TFTs by PECVD. The fabricated devices without passivation exhibit excellent characteristics in terms of high Ion/off ratio of ~104, steeper SS of 220mV/decade, and good field-effect mobility (0.67cm2V-1s-1). TEOS-based SiO2 capping causes the devices to lose switching function with high leakage, while SiH4-based SiO2 maintains the characteristics of devices close to that of un-passivated ones. SiNx capping leads to a rise in the off-state current. The transforms before and after the passivation processes are analyzed by EDS, XRD, XPS and hall measurements. The results show that the capping with TEOS-based SiO2 and SiNx result in generation of SnO2 textures in the SnO thin films. We speculate that the rather high thermal budgets of the TEOS-based SiO2 and SiNx depositions are responsible for the observations. Long-term stability is also inspected. The characteristics of un-passivation deviced degrade rapidly (Ion/off <102, SS~434mV/decade after 56 days), while the characteristics of SiH4-based SiO2 maintain well after 56 days.