降低熱預算之製程與模擬技術平台開發應用於堆疊/積層型三維積體電路

Development and Simulation of Lowering Thermal Budget Technology Platform on Stacking/Monolithic 3D Integrated Circuits

檔案

日期

2020

類型

語言

英文

摘要

近十年來,隨著現代科技追求的輕薄短小與元件的操作速度,勢必得將電晶體的尺寸與線寬不斷的微縮,但是當尺寸不斷的微縮,二維積體電路受到物理的限制終將達到極限,因此為了解決此一問題,勢必得朝三維晶片堆疊發展。在近幾年提出的超越摩爾定律(More than Moore)中的一項利器:三維積體電路(3DIC),其可以達到高密度封裝、高異質整合以及更快速的訊號連接速度,而在三維積體電路中可簡單分為傳統式的堆疊型三維積體電路(Stacking 3DIC)與積層型三維積體電路(Monolithic 3DIC)。
在堆疊型的三維積體電路中,是指將兩個或兩個以上之晶片,在接合前進行研磨(Thinning)、晶片承載(Handling)、對準(Alignment)等工藝技術,而晶片之間的機械強度與電性連接可藉由矽穿孔(Through-silicon via, TSV)或是透過金屬接合(Metal Bonding)、氧化物接合(Oxide Bonding)、聚合物黏著接合(Polymer-Adhesive Bonding)完成,在這些接合中又以銅金屬接合較為受重視,因為銅具有良好之電性、抗電遷移佳、延展性、製程成本也較低。然而傳統銅對銅直接接合需在300~400°C才有較佳之表現結果,使得熱預算有過高之問題,且銅在空氣中容易氧化其表面不利於接合進行,因此本篇論文將銀作為鈍化層(Passivation Layer),將銀鈍化層沉積約30奈米在接合處以防止銅氧化的發生。另外,本研究是在RDL層上再成長直徑約為10um的微凸塊並將其做為接合的結構以更符合科技實際之用途。透過不同的方法測試出適當之實驗參數、顯影、曝光時間、沉積之方式,使得銅微凸塊可以有較好的沉積品質成長在 RDL層上。研究結果顯示接合之溫度可以降低至大約200°C,並且可以承受溫溼度之測驗(uHast)、溫度循環測試(TCT)以及400小時之定電流電遷移測試,經過可靠度測驗以及電遷移測試,其電阻值呈現一穩定之結果,說明具有銀鈍化層之微凸塊接合結構可以有效降低接合之溫度。
堆疊型三維積體電路中層與層之距離大約為微米等級,然而積層型三維積體電路,可以將其間距縮小至奈米等級,縮小了一百倍可以使得訊號連接更為快速,以符合現在科技追求的高頻寬之特性,但積層式三維積體電路在製作時,因為高溫的退火造成在後製成(BEOL)電路上有隨機晶格邊界(radom grain boundary)的出現,會造成元件漏電流上升,這會使得電路的特性受到變異,而影響整個電路的波形和特性。此研究主要目的為透過特殊的微小孔洞設計(cooling hole)來有效控制晶格邊界,稱為晶格控制技術(Location-controlled-grain Technique)。
本篇論文第二部分透過有限元素模擬軟體Ansys,模擬當利用奈秒雷射加熱,使得非晶矽薄膜退火再結晶成多晶矽結構時,計算出其整體結構的時變溫度。由於矽薄膜之溫度與熔融態時間會影響薄膜的晶粒大小、品質與晶格邊界的成長,我們量測了其溫度與熔融態時間以分析出最佳之製程參數。另外在雷射退火法加熱時,利用Ansys軟體可得知底層元件之整體溫度,以確保底層元件不超過熱預算400°C。雷射加熱時,整體的溫度在製程時是無法確切知道的,因此透過此研究可以得知整體溫度並預防底層元件溫度過高,最後找出最佳之製成參數。
In recent years, the critical dimension (CD) has been continuously reduced. However, the miniaturization of two-dimensional integrated circuit will eventually approach the physical limit. To achieve high-density packaging, three-dimensional integrated circuit (3D IC) is proposed to stack components vertically, which has lower power consumption, shorter interconnect, and higher heterogeneous integration. 3D ICs can be divided into stacked three-dimensional integrated circuit (Stacking 3DIC) and monolithic three-dimensional integrated circuit (Monolithic 3DIC).
In Stacking 3DIC, two or more wafers are subjected to the following process: thinning, wafer handling, alignment and bonding. The interconnection with high mechanical strength and good electrical property can be realized by the following process: through-silicon via (TSV) and bonding techniques, including metal bonding, oxide bonding, and polymer-adhesive bonding. Among these bonding techniques, copper to copper metal bonding is more important due to the good electrical properties, good resistance to electromigration, and low process cost of copper. However, traditional copper-to-copper direct bonding with better performance has to be achieved at 300~400°C, leading to the issue of thermal budget. The other concern is that copper is easily oxidized in the air, which will result in poor bonding quality. In this paper, we deposit 30nm silver as a passivation layer to prevent the oxidation of copper. In addition, we deposit micro bumps with a diameter of 10um on the RDL layer to meet the demands of practical application in the industry. The appropriate experimental parameters, development, exposure time, and deposition methods are proposed in this study. Thus, the copper micro bumps can be grown on the RDL with good deposition quality. The results of this work show that the bonding temperature can be reduced to about 200 °C, and electrical performance of the bonding structure can maintain with a slight variation after reliability test, including test of temperature and humidity (uHast), temperature cycle test (TCT), and 500hrs electromigration test.
Compared with the micro-level distance between layers in stacking 3D IC, the distance between layers can be reduced to nano-level in monolithic 3DIC, which can provide shorter interconnection for faster signal transmission to achieve the characteristics of high frequency bandwidth. However, high temperature annealing is involved in the fabrication of monolithic 3DIC, leading to random grain boundaries on the BEOL circuits. The leakage current of the structure is increased due to the grain boundaries and cause the characteristics of the circuit with large variation. Thus, the main purpose of this research is to effectively control the lattice boundary through a special tiny hole design (cooling hole), called the“Location-Controlled-Grain Technique”.
In the second part of this paper, the analyses are performed by the finite element simulation software Ansys. We simulate the time-dependent temperature of the whole structure when nanosecond laser crystallization method is applied to recrystallize amorphous silicon into polysilicon silicon. Since the temperature and melting duration dominates grain size, crystallinity, and grain boundary of the silicon film, we measured the temperature and melting duration to adjust the process parameters. In addition, the temperature of the bottom device can be obtained to ensure that the temperature of bottom device is less than the thermal budget of 400°C. The overall temperature cannot be known exactly during the laser heating process. Therefore, the simulation was conducted to analyze the temperature of this structure during laser heating to optimize the best manufacturing parameters.

所屬典藏

電子研究所
顯示完整詮釋資料 統計資料

引用此條目

Huang, C.-C. (2020). Development and Simulation of Lowering Thermal Budget Technology Platform on Stacking/Monolithic 3D Integrated Circuits. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/75883

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享