於矽鍺基板上高溫退火對以氧電漿及雙氧水成長介面層之閘極堆疊之研究

A Study of the Impact of High Temperature Annealing on Gate Stack with Interfacial Layer Grown by O2 Plasma and High-purity H2O2 on SiGe Substrates

檔案

日期

2020

類型

語言

英文

摘要

本篇論文中,我們使用氧電漿與高純度雙氧水前驅物於矽鍺(Si0.5Ge0.5)基板上進行氧化,並使用二氧化鉿與氮化鈦作為閘極堆疊。在用氧電漿長完氧化層後,使用高溫的退火可以形成選擇性氧化矽原子,減少氧化層中氧化鍺的含量,可以有效降低介面能態密度(Dit)到2×1012 cm-2eV-1,並同時擁有極低的等效氧化層缺陷密度(Ntrap)9.6×1010 #cm-2,然而在退火過程中,會因為腔體中殘存的氧氣會稍微再次氧化矽鍺,進而造成等效閘極氧化層(EOT)變厚。而高純度雙氧水前驅物在高鍺組成的矽鍺(Si0.5Ge0.5)上,因為形成較緻密的氧化層,可以避免等效閘極氧化層(EOT)在高溫退火過程中變厚,同時在還沒使用高溫退火前就可以達到較佳的介面能態密度(Dit)4×1012 cm-2eV-1。此外,1000度為太高的氧化層退火溫度,會造成矽鍺磊晶層與下方矽基板產生交互擴散的行為,造成矽鍺磊晶層的組成改變,甚至因為鍺原子的往下擴散,導致在穿透式顯微鏡下,可以觀察到矽鍺層的厚度有明顯的增加,而此會導致矽鍺晶層產生鬆弛(relaxation)與差排(dislocation),所以1000度的氧化層退火並不適合於矽鍺(Si0.5Ge0.5)上製作元件,而800度的氧化層退火為形成選擇性氧化矽原子較適合的溫度。
然而,在7奈米的矽鍺(Si0.5Ge0.5)層上,會遇到PN接面二極體製程的困難,造成汲極端的漏電過大,不利於金氧半場效應電晶體的製作。於是,我們改去製作在170奈米厚的矽鍺(Si0.8Ge0.2)層上,同時先研究氧電漿與高純度雙氧水前驅物氧化於矽鍺(Si0.8Ge0.2)基板上的電性分析,我們將其與前面在矽鍺(Si0.5Ge0.5)基板上的電性分析比較,可以發現在矽鍺(Si0.8Ge0.2)基板上,經過氧電漿處理後的低介面能態密度(Dit)比在矽鍺(Si0.5Ge0.5)基板上小許多,這是源自於在矽鍺(Si0.8Ge0.2)上形成的氧化層中氧化鍺含量較少。然而,雙氧水前驅物氧化於矽鍺(Si0.8Ge0.2)的介面特性居然比在矽鍺(Si0.5Ge0.5)上的特性還差,這與過去用氣體氧化在矽鍺上的結果相悖,代表高純度雙氧水對矽鍺氧化方式與傳統氣體氧化方式不同,且高純度雙氧水較適用於高鍺組成的矽鍺(Si0.5Ge0.5)上。
我們成功於矽鍺(Si0.8Ge0.2)基板上製作出P型的金氧半場效應電晶體,並發現在製作完氧化層後,經過高溫800度退火,可以有效的降低次臨界擺福(S.S.),最低可以達到74.89 mV/decade;並發現臨界電壓(Vth)在經過800度退火後,會往正的方向偏移,這可能是在使用高溫退火過程中,有效填補氧化層當中原先帶正電的氧空缺;此外,矽鍺金氧半場效應電晶體擁有高的電流開關比,最高可以達到1.15×108;使用完高溫800度氧化退火後,還可以提升電洞的遷移率,這是源自於有效改善介面缺陷電荷,使得電洞在矽鍺通道的傳輸過程中受到較小的庫倫散射所致。
In this thesis, we used O2 plasma and high-purity H2O2 precursor to oxidize Si0.5Ge0.5 substrates. The HfON/HfO2/TiN was used as the high-k metal gate in the gate stacks. After interfacial layer formation by O2 plasma, high-temperature annealing was conducted to form preferential SiO2 growth. Reducing the content of germanium oxide in the interfacial layer (IL) can effectively improve the Dit to 2×1012 cm-2eV-1. At the same time, very low equivalent oxide layer traps density (Ntrap) could be attained to 9.6×1010 #cm-2. However, during the annealing process, the remaining oxygen in the RTA chamber would oxidize the silicon germanium slightly. This resulted in the increase of equivalent oxide thickness (EOT). Comparing to the IL formed by O2 plasma, H2O2-IL can effectively avoid the increase of EOT during high temperature annealing process due to formation of a denser interfacial layer. In addition, the annealing temperature for the interfacial layer as high as 1000C would cause the inter-diffusion between epitaxial SiGe layer and the underlying Si substrates. The composition of SiGe layer would change due to germanium atoms diffusion downward. The thickness of SiGe layer significantly increased observed by the Transmission Electron Microscope (TEM). Moreover, Ge diffusion behavior would cause the relaxation and dislocation in the SiGe layer, so we knew that 1000C IL annealing was not suitable for Si0.5Ge0.5 device fabrication. Comparing to 1000C IL annealing, 800C IL annealing was more suitable for the preferential SiO2 growth.
However, we encountered difficulties in the process of PN junctions on the 7-nm Si0.5Ge0.5 layer. The difficulty was the excessive drain leakage current which was not conducive to the fabrication of MOSFETs. Therefore, we turned into fabricating on 170-nm Si0.8Ge0.2 layer. We firstly studied the quality of IL formed by O2 plasma and high purity H2O2 precursor on Si0.8Ge0.2 substrates. Comparing the previous electrical analysis by O2 plasma oxidizing Si0.5Ge0.5 substrates, the lower Dit value on Si0.8Ge0.2 substrates was obtained due to less amount of GeOx in IL. However, the interface quality of H2O2-IL on Si0.8Ge0.2 substrates was worse than that on Si0.5Ge0.5 substrates. This was contrary to the previous results of gas oxidation on SiGe. Thus, the oxidation of SiGe by high-purity H2O2 precursor was different from the traditional gas oxidation method on SiGe. As a result, high-purity H2O2 precursor oxidation may be suitable for high-Ge-content silicon.
We successfully fabricated p-MOSFETs on Si0.8Ge0.2 substrates. After using 800C IL annealing, S.S. could be improved and the lowest value was 74.89 mV/decade. Moreover, Vth would shift in the positive direction. The original positively charged oxygen vacancies may be repaired after 800C IL annealing. Furthermore, Si0.8Ge0.2 p-MOSFETs showed a high Ion/Ioff ratio of 1.15×108. The hole mobility could also be improved after 800C IL annealing. This resulted from the improvement of the interface quality, so holes were less scattered from coulomb scattering during the transport through silicon germanium channel.

所屬典藏

電子研究所
顯示完整詮釋資料 統計資料

引用此條目

Lin, H.-J. (2020). A Study of the Impact of High Temperature Annealing on Gate Stack with Interfacial Layer Grown by O2 Plasma and High-purity H2O2 on SiGe Substrates. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/76017

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享

永久網址:https://thesis.lib.nycu.edu.tw/handle/20.500.14371/76017