摘要
現今廣泛被利用的3D列印成像技術以固化方式區分主要分為三大類,熱熔融層積(FDM)、雷射粉末燒結(SLS)、光固化(SLA.DLP),三者各有利弊,其中又以光固化的列印方式最為人利用,前兩種技術雖然列印方式不同,但皆為以單點固化至面,進而往z軸做堆疊,而光固化此種列印方式大多是利用DLP(Digital Light Processing)的投影機進行整面的固化,速度以及精密度都會比前述兩者要高,所以本研究是基於DLP的固化方式去改為利用繞射元件達到更好的效果。
基於光固化這種3D列印方式,我們將原有以高精密度數位微反射晶片(DMD)投影機固化的光源,改以實驗室自製之高解析度純相位矽基液晶(Liquid Crystal On Silicon, LCoS)空間光調制器做為光源,並結合z軸方向的移動平台去達到高精密度的光固化成果。
實驗中先以建模軟體(Autodesk Inventor)製作3D圖像的樣板檔,再將之以我們需要的精細度做細部的切層,每層厚度最小可達1μm,最後以近場繞射的迭代傅立葉演算法來製作我們每一層固化平面的電腦全像片,實驗中利用負焦距電腦全像片以及透鏡系統來遮擋零階光,並藉由控制移動平台的拉升時間與停留時間以及全像片的撥放時間來達到每層理想固化厚度。
基於光固化這種3D列印方式,我們將原有以高精密度數位微反射晶片(DMD)投影機固化的光源,改以實驗室自製之高解析度純相位矽基液晶(Liquid Crystal On Silicon, LCoS)空間光調制器做為光源,並結合z軸方向的移動平台去達到高精密度的光固化成果。
實驗中先以建模軟體(Autodesk Inventor)製作3D圖像的樣板檔,再將之以我們需要的精細度做細部的切層,每層厚度最小可達1μm,最後以近場繞射的迭代傅立葉演算法來製作我們每一層固化平面的電腦全像片,實驗中利用負焦距電腦全像片以及透鏡系統來遮擋零階光,並藉由控制移動平台的拉升時間與停留時間以及全像片的撥放時間來達到每層理想固化厚度。
3D printing technology are widely applied in three major categories: fused
deposition modeling (FDM), selective laser sintering (SLS), and stereolithography
(SLA). Each of them has its own strength and weakness. The FDM and SLS methods
are different approaches, however, these two methods apply single curing point on the
surface followed by stacked on z-axis. SLA method, on the other hand, cured a pattern
directly on the entire surface. As a result, SLA processes the advantages in terms of
accuracy and speed. DLP (Digital Light Processing) projector was mostly applied in
the SLA method. In this thesis, a full phase modulation LCoS was applied with a
moving platform in the z-axis direction to realize high precision curing result. In
addition, Autodesk Inventor software was applied to create a 3D image layer with the
thickness up to 1£gm. The image pattern of each layers was converted to corresponding
computer generated hologram (CGH) based on near-field diffraction of Iterative
Fourier Transform Algorithm (IFTA).
The Bottom-up set-up equipped 405 nm laser as light source. 1080p full phase
modulation LCoS was calibrated for pattern generation. In addition, the target lens
shape was sliced into layers by Autodesk Inventor software. Each layer was converted
to corresponding CGH image by Matlab. The layer thickness was set at 15~30 um for
practical use. The area of curing object is synchronized with high precision translation
stage to achieve high accuracy result. The error was estimated at 2.7% but was further
improved to 1.4%.
deposition modeling (FDM), selective laser sintering (SLS), and stereolithography
(SLA). Each of them has its own strength and weakness. The FDM and SLS methods
are different approaches, however, these two methods apply single curing point on the
surface followed by stacked on z-axis. SLA method, on the other hand, cured a pattern
directly on the entire surface. As a result, SLA processes the advantages in terms of
accuracy and speed. DLP (Digital Light Processing) projector was mostly applied in
the SLA method. In this thesis, a full phase modulation LCoS was applied with a
moving platform in the z-axis direction to realize high precision curing result. In
addition, Autodesk Inventor software was applied to create a 3D image layer with the
thickness up to 1£gm. The image pattern of each layers was converted to corresponding
computer generated hologram (CGH) based on near-field diffraction of Iterative
Fourier Transform Algorithm (IFTA).
The Bottom-up set-up equipped 405 nm laser as light source. 1080p full phase
modulation LCoS was calibrated for pattern generation. In addition, the target lens
shape was sliced into layers by Autodesk Inventor software. Each layer was converted
to corresponding CGH image by Matlab. The layer thickness was set at 15~30 um for
practical use. The area of curing object is synchronized with high precision translation
stage to achieve high accuracy result. The error was estimated at 2.7% but was further
improved to 1.4%.