旋塗剝離式奈米銀導線製程開發與應用

Development of A Combined Spin Coating and Lift-off Process (CSLP) for Silver Interconnect Applications

檔案

日期

2020

類型

語言

中文

摘要

本論文開發旋塗剝離製程技術,並透過奈米導電銀墨水實現銀導線微結構。透過將含有12 nm銀顆粒的導電銀墨水經旋塗剝離而成10-100 μm的銀線寬、四點探針結構、電容結構以及電感結構。使用旋塗剝離製程技術製作具有60 μm銀線寬的四點探針結構,進行銀鏡反應30分鐘,再送入填充混合氣體(95% N2+5% H2)的爐管進行300C 30min熱燒結後,可得到約2.36 μΩ∙cm的電阻率,約為塊狀銀電阻率的1.48倍。此方法在低溫實現低電阻率的導線,將有利於軟性電子的金屬連接互聯層應用。另該旋塗剝離製程技術亦應用於製作厚膜金屬結構於軟性基板之上,使用黏度為1000 cP的奈米導電銀墨水,其奈米銀顆粒為50 nm,在聚醯亞胺基板上可製作出線寬與線距均為150 μm、線平均厚度為70 μm 的指叉電容結構與螺旋方型電感,在燒結溫度150 C下可得到電阻率為50.9 μΩ∙cm,且導線結構具有0.47之高深寬比。相較於現今其他製程,使用旋塗剝離製程來製作金屬結構,不需要昂貴的噴塗機器,製作成本非常便宜,此方法還適合大面積量產,外加上製程溫度屬於低溫,因此可應用在薄膜電晶體、感測器、太陽能電池、電子電路系統、生醫電子元件等軟性電子之製造。此外,該旋塗剝離製程技術不僅適合應用在軟性電子的金屬結構開發上,也可取代傳統半導體製程中製作金屬連接線的方式。
利用此技術可以簡化製程步驟,降低製程溫度,由於導電銀墨水也被視為相對環保的一種材料,因此可以減少環境污染,成為綠色半導體製造之另種選擇。
This thesis presents a new manufacturing method combining spin coating and lift-off process (CSLP) for silver interconnect and microstructure fabrications. Two kinds of silver nanoparticle inks are used for the demonstration of the technology feasibility. In thin film process, the CSLP can realize various microstructures, such as microlines with a line width ranging from 10 to 100 μm, four-point microstructures, interdigitated capacitors and spiral square inductors using the silver ink with an average particle diameter of 12 nm. The four-point I-V measurement shows a 60 μm wide silver line realized by the CSLP can exhibit an electrical resistivity of ~2.36 μΩ∙cm while the film is treated with a silver mirror reaction for 30 min followed by thermal sintering at 300C with forming gas (95% N2+5% H2) for 30 min. The resistivity of ~2.36 μΩ∙cm is 1.48 times greater than that of bulk silver (1.59 μΩ∙cm).
In thick film process, the CSLP can realize a 150 μm in line width, 70 μm in average thickness and a width vs. height aspect ratio of 0.47, microstructure on a polyimide substrate using the silver ink with a viscosity of 1000 cP and average particle diameters of 50 nm. After being sintered in an oven at 150 C for 30 min, the microstructure can exhibit an electrical resistivity of ~50.93 μΩ∙cm. In thick film process, the CSLP can realize various microstructures, such as interdigitated capacitors and spiral square inductors. Low cost facility and process temperature characteristics of the CSPL have shown its potential for the manufacture of electrical interconnects for flexible electronics. Furthermore, the conductive silver ink has been regarded as a relatively environmentally friendly material, so the newly developed process can be an alternative green manufacture technology for future microsystem fabrication.
Keywords: Spin coating and lift-off, silver inks, microstructure

所屬典藏

電子研究所
顯示完整詮釋資料 統計資料

引用此條目

黃啓富 (2020). 旋塗剝離式奈米銀導線製程開發與應用. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/76545