鐵軌缺陷之非接觸超聲導波檢測

Noncontact Ultrasonic Guided Wave Detection of Rail Dedects

檔案

日期

2021

類型

語言

中文

摘要

長重軌連續銲接一般採用閃電對銲及鋁熱銲,銲接處熔融不完全之裂縫、空孔及非金屬銲渣等瑕疵經長期運轉會造成斷軌意外。交通大學非破壞評估實驗室團隊已發展導波檢測鐵軌缺陷的方法,以空氣耦合超音波換能器在軌頭上方偵測導波響應,從方向濾波器析出微弱的缺陷背向散射波,可快速判別軌腹或軌底缺陷。本文應用及比較垂直軌頭正向激發壓力波及切線激發線性偏振剪力波生成的導波頻譜特徵,前者採用音洩感測器,後者為電磁超音波換能器。實驗發射中心頻率100 kHz之寬頻音調突發脈波以多重反射方式形成鐵軌導波。實驗結果顯示兩種方式不僅生成相同模態的導波,還能各自激發不同的模態。除非軌頭磨耗,正傳波的頻譜均維持不變。鐵軌缺陷的位置明顯影響反傳波的頻譜特徵。電磁超音波換能器具有檢測軌腹及軌底缺陷的潛力。
鋁熱銲經常會造成鐵軌斷面膨脹,也會改變反傳波的頻譜。有限元素法數值模擬及實驗結果證實41點以上的B掃描適合量測詳細的導波頻譜。較少點數(如21點)的B掃描雖然可以快速篩選鐵軌缺陷,卻無法分辨鋁熱銲接頭。本文最後採用暫態分析進一步探討銲接處斷面變化對於導波檢測的影響。
Continuous welded rails generally use flash butt welding or thermite welding. Defects due to lack of fusion, voids, and non-metallic inclusions in the welding joints are the major causes of rail breakages after long-term operation. The NDE Laboratory at NCTU developed a guided wave inspection method for rail defect detection based on directional filter using air-coupled ultrasonic transducers. The rail web and base defects can be quickly determined through the frequency spectra of relatively small backscatter signals extracted from the total waveforms captured over the rail heads. This thesis presents a comparison between the frequency spectra characteristics generated by normal incidences of pressure waves and linearly polarized shear waves. The former was carried out by an acoustic emission sensor; the latter was an electro-magnetic acoustic transducer (EMAT). Broad-band tone-bursts of center frequency at 100 kHz were transmitted to excite guided modes through multi-reflections in rails. The experimental results indicate both transmitters not only generate the same guided modes, but each can excite distinct modes. The frequency spectrum of forward propagation remains the same along the rails, but varies if the rail head was worn-out. However, the localization of rail defects has significant influence on the frequency spectra of backward propagation. Experimental evidence indicates EMAT has good potential to detect web and base defects.
The cross-section inflation often found at thermite welding joints has influence on frequency spectra of backward propagation. Simulations by finite element method and experimental results show that more than 41 point B-scan data are appropriate to measure detailed frequency spectra of guided modes. Fewer B-scan data points, e.g., 21 points, are good for rail defect screening, but cannot distinguish the thermite welds. Eventually, the transient analysis has been used to further explore the influence of weld cross-section profiles on defect detection.

所屬典藏

機械工程學系
顯示完整詮釋資料 統計資料

引用此條目

陳學威 (2021). 鐵軌缺陷之非接觸超聲導波檢測. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/77967

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享

永久網址:https://thesis.lib.nycu.edu.tw/handle/20.500.14371/77967