化學氣相沉積之無機鈣鈦礦薄膜品質及膜厚控制之研究
The Quality and Thickness Control of Inorganic Perovskites Film by Chemical Vapor Deposition Method
摘要
本研究是以低壓化學氣相沉積法(LPCVD)生長無機鈣鈦礦CsPbBr3材料,並藉由控制水平爐管式腔體內載流氣流流量以及前驅物揮發速率達到CsPbBr3薄膜的優化;經過一系列參數的改變與探討後,當腔體爐心溫度510度、壓力700 mtorr、氣流30 sccm、前驅物揮發速率為每分鐘0.2毫克、持溫10分鐘的條件下生長可獲得最佳的薄膜品質;而在薄膜厚度的控制部份是藉由生長時間的長短來控制薄膜的生成厚度,從生長時間5分鐘到40分鐘可成功控制薄膜厚度從150 nm到2.3 µm,並探討在不同厚度下對於材料的光學特性造成的影響,這對以CsPbBr3應用在不同的元件製作上是很有助益。
In this study, we used the Low Pressure Chemical Vapor Deposition method to grow the inorganic perovskite CsPbBr3 material. To optimize CsPbBr3 film, we controlled the flow rate of the carrier gas flow inside the horizontal furnace tube and the evaporate rate of the precursor. After a series testing in different parameters and discussion, it was found that we can have the best quality of CsPbBr3 film with furnace center temperature of 510 degrees Celsius, 700 mtorr pressure, 30 sccm carrier gas flow, and 0.2 mg per minute evaporate rate of precursor for 10 minutes. Furthermore, the control of the film thickness is growth time. The film thickness can successfully grow from 150 nm to 2.3 µm from 5 minutes to 40 minutes. This study also we discussed the influence of the optical characteristics under different thin thickness. This is very helpful to apply the CsPbBr3 film characters to different component production.