整合重分佈製程之微型加熱封裝平台的設計與量測
Design and Experiment of Micro-hotplate Integrated Redistribution Layer for Package
摘要
本研究利用微型加熱器與重分佈製程整合成為一個封裝平台,由微型加熱器與重分佈製程中的焊墊、導線組成球柵陣列形式的佈局,採用覆晶方式進行對位,以一秒鐘時間供電加熱器對焊墊瞬間加熱將溫度傳遞到焊料,使焊料融化與焊墊接合形成接合點,晶片與封裝平台就能相互導通傳遞訊號。將焊接之樣品進行量測迴路阻抗變化量、X-Ray檢測及拉力測試,分析加熱方法的焊接品質。
以單顆加熱器工作對多個焊墊加熱時,利用矽基板良好的傳熱特性,能以較低的功耗使周圍焊墊達到融化焊料的溫度,其加熱方式的拉力測試結果為13.86MPa;當每個焊墊下的加熱器皆為工作狀態時,則可以較快速使焊墊達到焊料熔點,因為工作的加熱器數量較多功耗也較高,其加熱方法的拉力測試結果為17.39MPa,兩種加熱方式各有優缺點。針對焊點位置瞬間加熱可以大幅減少整體元件在高溫環境中加熱的時間,降低對元件、IC晶片的影響。
以單顆加熱器工作對多個焊墊加熱時,利用矽基板良好的傳熱特性,能以較低的功耗使周圍焊墊達到融化焊料的溫度,其加熱方式的拉力測試結果為13.86MPa;當每個焊墊下的加熱器皆為工作狀態時,則可以較快速使焊墊達到焊料熔點,因為工作的加熱器數量較多功耗也較高,其加熱方法的拉力測試結果為17.39MPa,兩種加熱方式各有優缺點。針對焊點位置瞬間加熱可以大幅減少整體元件在高溫環境中加熱的時間,降低對元件、IC晶片的影響。
This research purpose micro heater integrated redistribution layer process into package platform, The micro heater and redistribution layer of trace and pad in the redistribution process form ball grid array of solder joints. Package method of flip chip is used for alignment, and micro heater is powered by electricity in a second, Solder pad is heated instantly to transfer the temperature to solder, so that the solder melts and the solder pad form a solder joint, the chip and the package platform can communicate with each other and transmit signals. The Bonding sample are subjected to measurement impedance of loop, X-Ray defect inspection, tensile test to analyze the welding quality of heating method.
By the good thermal conductivity characteristic of silicon substrate, the method that using single heater to heat the surrounding solders pads brings the rising of temperature of solder pads to melt solder balls with lower power consumption. And this heating method of tensile test result is 13.86MPa. With method that a pad is heated by a heater leads to faster melting time. Because the number of heaters working is larger, the power consumption is higher than another method. And the tensile test result of the heating method is 17.39MPa. Both heating method have their pros and cons. The instant heating of the solder joint position can greatly reduce the heating time of the whole component in high-temperature environment and reduce the impact of IC and semiconductor device.
By the good thermal conductivity characteristic of silicon substrate, the method that using single heater to heat the surrounding solders pads brings the rising of temperature of solder pads to melt solder balls with lower power consumption. And this heating method of tensile test result is 13.86MPa. With method that a pad is heated by a heater leads to faster melting time. Because the number of heaters working is larger, the power consumption is higher than another method. And the tensile test result of the heating method is 17.39MPa. Both heating method have their pros and cons. The instant heating of the solder joint position can greatly reduce the heating time of the whole component in high-temperature environment and reduce the impact of IC and semiconductor device.