鈦及鉭應用於銦鎵鋅氧化物薄膜電晶體電極之研究

A Study of Ti and Ta Serving as the Electrodes of In-Ga-Zn-O Thin-film Transistors

檔案

日期

2021

類型

語言

中文

摘要

本研究探討鈦(Titanium,Ti)及鉭(Taltalum,Ta)作為銦鎵鋅氧化物(In-Ga-Zn-O,IGZO)薄膜電晶體(Thin-film Transistor,TFT)源極與汲極對元件之影響。研究第一部分利用傳輸線模型(Transmission Line Model,TLM)量測兩種金屬與IGZO薄膜界面在退火處理前後的特徵接觸電阻(Specific Contact Resistance,c),並以X光電子能譜儀(X-ray Photoelectron Spectroscopy,XPS)分析金屬與IGZO界面退火前後縱深組成變化。TLM分析結果顯示退火前Ti/IGZO之c值為3.63×103 Ω∙cm2,Ta/IGZO為2.71×103 Ω∙cm2,經300°C、一小時退火可得Ti/IGZO最低c值為6.27×104 Ω∙cm2,Ta/IGZO為8.56×104 Ω∙cm2。XPS分析顯示退火前Ti/IGZO界面氧化態以Ti2+及Ti3+為主,退火後則為Ti3+及Ti4+;退火前Ta/IGZO界面氧化態為Ta3+及Ta4+,退火後兩者含量增加。退火後形成的氧化物也使氧缺陷增加,此同時提升載子濃度,使金屬與IGZO薄膜間c值降低。第二部分進行Ti-TFT及Ta-TFT元件分析,使用第一部分最低c值之退火溫度300°C,退火時間為一分鐘及一小時。Ti-TFT的飽和遷移率(Saturation Mobility,sat)為1.57 cm2/Vsec,臨界電壓(Threshold Voltage,Vth)為7.72 V,電流開關比(On/Off Current Ratio,Ion/Ioff)為2.35×105,次臨界擺幅(Subthreshold Swing,SS)為0.86 V/decade;Ta-TFT之sat為18.3 cm2/Vsec,Vth值為2.3 V,Ion/Ioff為1.24×104,SS為2.1 V/decade。經300°C退火一分鐘及一小時後,Ti-TFT之SS為0.76及2.06 V/decade,Ion/Ioff為3.75×104及2.64×103,Vth為5.6 V及1.48 V,sat為18.5 cm2/Vsec及41.0 cm2/Vsec。Ta-TFT退火後則失去元件特性。
This study investigates the feasibility of titanium (Ti) and tantalum (Ta) serving as the source/drain electrodes of amorphous indium-gallium-zinc-oxide (a-IGZO) thin-film transistors (TFTs). First, the specific contact resistances (c’s) at the interfaces of Ti or Ta and a-IGZO were measured before and after annealing by the transmission line model (TLM) method. The evolutions of chemical status at Ti/IGZO and Ta/IGZO interfaces were also analyzed by the x-ray photoelectron spectroscopy (XPS) depth profiles. Before annealing, the c of Ti/IGZO interface was 3.63×103 Ω∙cm2 whereas that of Ta/IGZO interface was 2.71×103 Ω∙cm2. After the annealing for 1 hr at 300°C in vacuum atmosphere, the lowest c of Ti/IGZO interface was 6.27×104 Ω∙cm2 and that of Ta/IGZO interface was 2.71×103 Ω∙cm2. XPS analysis revealed the presence of Ti2+ and Ti3+ at the Ti/IGZO interface before annealing and that of Ti3+ and Ti4+ at the Ti/IGZO interface after annealing. As to the Ta/IGZO interface, Ta3+ and Ta4+ were observed before annealing and their contents increased after annealing. Annealing was found to increase the amounts of oxygen defects at the Ti/IGZO and the Ta/IGZO interfaces which, in turn, increases the carrier concentration and results in the decrement of c values at Ti/IGZO and Ta/IGZO interfaces. This study also prepared the a-IGZO TFTs within Ti or Ta as the source/drain electrodes and the transfer characteristics of devices were measured. Before annealing, Ti-TFTs exhibited the saturation mobility (sat) of 1.57 cm2/Vsec, threshold voltage (Vth) of 7.72 V, on/off current ratio (Ion/Ioff ) of 2.35×105 and subthreshold swing (SS) of 0.86 V/decade. For Ta-TFTs, μsat of 18.3 cm2/Vsec, Vth of 2.3 V, Ion/Ioff of 1.24×104 and SS of 2.1 V/decade were observed. After the annealing for 1 min and 1 hr at 300°C in vacuum atmosphere, the Ti-TFTs exhibited μsat of 18.5 cm2/Vsec and 41.0 cm2/Vsec, Vth of 5.6 V and 1.48 V, Ion/Ioff of 3.75×104 ,and 2.64×103, SS of 0.76 V/decade and 2.06 V/decade, respectively. As to the Ta-TFTs, their electrical characteristics diminished after annealing.
顯示完整詮釋資料 統計資料

引用此條目

陳蔚璉 (2021). 鈦及鉭應用於銦鎵鋅氧化物薄膜電晶體電極之研究. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/79353

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享

永久網址:https://thesis.lib.nycu.edu.tw/handle/20.500.14371/79353