後段製程相容之高微縮性鐵電 HfxZr1-xO2電容
Back-End-of-Line Compatible HfxZr1-xO2 Ferroelectric Capacitors with High Scalability
摘要
在人工智慧與物聯網時代,高性價比的即時醫療監控或日常生活可攜式輕便裝置的需求,持續推動元件微縮。為滿足融入人工智慧的高品質生活,類神經突觸元件的實現勢在必行,大量平行運算需求驅使低成本、低功耗且快速的非揮發性記憶體新元件被開發,以打破高能耗的馮‧諾伊曼(Von Neumann)硬體架構而發展新穎記憶體內運算架構(In-memory computing)。HfxZr1-xO2 作為介電層的鐵電電容是熱門非揮發性記憶體元件,其各個特性如蝴蝶效應般環環相扣,不同特性間的權衡與最佳值的探討成了元件設計上的困難挑戰。鐵電電容常見的應用為 FeRAM、FTJ 以及 MFMFET,這些元件皆是將鐵電電容整合於 CMOS 後段製程當中,以獨立最佳化 CMOS 前段製程與後段製程的參數設計。多數研究採用原子層沉積技術沉積 HfxZr1-xO2 薄膜,剛沉積出的薄膜呈現非晶態,經過快速退火製程後有機會發生相變化形成具備鐵電特性的斜方晶。大多文獻指出快速退火製程所需溫度落於攝氏 500 度至 700 度,此溫度區間容易造成鐵電電容整合入 CMOS 後段製程時產生金屬品質劣化與可靠度問題。因此探討如何採用 CMOS 後段製程相容之低溫製程製造具備良好鐵電特性元件成了目前的重要議題。許多文獻已提出有效的低溫
製程方法,如電漿輔助原子層沉積技術、深紫外光照射技術、應力優化以及高壓退火。然而多數文獻尚未兼顧低溫製程下的元件微縮性,元件具備高微縮性是人工智慧與物聯網時代下不被淘汰的重要因素。本研究乃首創針對低溫製程下的元件面積微縮性以及厚度微縮性進行分析與探討,討論非揮發性鐵電電容面臨元件微縮的挑戰,並提出有效改善方法。透過待測元件的設計、與電性量測分析,如 P-E 遲滯量測、CVS 漏電分析及可靠度分析,輔以物性檢測來診斷低溫製程下的元件微縮性劣化之原因,並建立元件失效模型。本研究透過改變薄膜表面與體積比例實驗及待測元件的設計與分析手法,發現元件的邊緣漏電主宰元件面積的微縮,且邊緣區域鐵電特性是否良好極為關鍵。並以背向散射電子繞射技術佐證低溫製程下鐵電電容的邊緣區域難以生成具備鐵電特性的斜方晶,而會被單斜晶或是非晶態主導。以此線索,本研究提出解決方案,以 Nitride 護層優化邊緣特性,在只採用 CMOS
後段製程相容之低溫退火溫度條件下,實現了 10 奈米 Hf0.5Zr0.5O2 鐵電電容。該鐵電特性指標 2Pr 值高達 48 𝜇C/cm2,且具備極高面積微縮性,同時降低漏電 10 倍。據此,更進一步,透過鐵電電容結構介面最佳化,本研究成功將 Hf0.5Zr0.5O2 厚度由 10 奈米微縮至 6 奈米,以利未來的低功耗應用。
製程方法,如電漿輔助原子層沉積技術、深紫外光照射技術、應力優化以及高壓退火。然而多數文獻尚未兼顧低溫製程下的元件微縮性,元件具備高微縮性是人工智慧與物聯網時代下不被淘汰的重要因素。本研究乃首創針對低溫製程下的元件面積微縮性以及厚度微縮性進行分析與探討,討論非揮發性鐵電電容面臨元件微縮的挑戰,並提出有效改善方法。透過待測元件的設計、與電性量測分析,如 P-E 遲滯量測、CVS 漏電分析及可靠度分析,輔以物性檢測來診斷低溫製程下的元件微縮性劣化之原因,並建立元件失效模型。本研究透過改變薄膜表面與體積比例實驗及待測元件的設計與分析手法,發現元件的邊緣漏電主宰元件面積的微縮,且邊緣區域鐵電特性是否良好極為關鍵。並以背向散射電子繞射技術佐證低溫製程下鐵電電容的邊緣區域難以生成具備鐵電特性的斜方晶,而會被單斜晶或是非晶態主導。以此線索,本研究提出解決方案,以 Nitride 護層優化邊緣特性,在只採用 CMOS
後段製程相容之低溫退火溫度條件下,實現了 10 奈米 Hf0.5Zr0.5O2 鐵電電容。該鐵電特性指標 2Pr 值高達 48 𝜇C/cm2,且具備極高面積微縮性,同時降低漏電 10 倍。據此,更進一步,透過鐵電電容結構介面最佳化,本研究成功將 Hf0.5Zr0.5O2 厚度由 10 奈米微縮至 6 奈米,以利未來的低功耗應用。
In the era of artificial intelligence and Internet-of-things (IoT), the demand for cost-effective real-time medical monitoring or lightweight portable devices in daily life continues to drive device scaling. To satisfy the high-quality life integrated with artificial intelligence, the realization of the artificial synaptic device is imperative. The demand for highly parallel computing drives the development of the new low-cost, low-power, and high-speed non-volatile memory devices. It is of great interest to develop the novel in-memory computing to overcome the high energy consumption of the conventional Von Neumann architectures. The HfxZr1-xO2-based ferroelectric capacitors are popular choices of non-volatile memory devices. However, it is challenging to optimize various device trade-offs that are tightly coupled.
The metal-ferroelectric-metal capacitors are widely used in the various ferroelectric non-volatile memory such as FeRAM, FTJ, and MFMFET. The ferroelectric capacitors are integrated into the CMOS back-end-of-line (BEOL) process so that the design and process windows of the CMOS front-end-of-line (FEOL) process and the CMOS BEOL process could be independently optimized. Most studies use atomic-layer deposition technology to deposit HfxZr1-xO2 thin films. The as-deposited HfxZr1-xO2 films are usually in an amorphous state. After the rapid thermal annealing, they could be transformed into the ferroelectric orthorhombic phase. Most literature pointed out that the temperature required for the rapid thermal annealing process is between 500 °C and 700 °C. This annealing temperature range is higher than the desirable standard CMOS BEOL process temperature. The relatively high annealing temperature leads to negative impacts on the metal integrity and the reliability issues on the CMOS. Therefore, using the CMOS BEOL compatible process temperature to achieve excellent ferroelectricity is an important research topic. Recently, several studies have proposed effective low-temperature process approaches, such as plasma-enhanced atomic-layer deposition (PE-ALD), deep ultraviolet light irradiation, stress optimization, and high-pressure annealing. However, most of them largely ignore the area scalability under the low-temperature process. High area scalability is an important factor for cost-effective mass production in the era of artificial intelligence and IoT.
This work first researches the scalability issue with the CMOS BEOL compatible annealing through the device test structure design, the electrical test and analysis methodology such as the P-E hysteresis measurement, the constant voltage stress (CVS) leakage, and reliability tests. Meanwhile, the physical analysis was also performed to diagnose the cause of poor area scalability under a low-temperature process. In addition, the failure model was established. This work finds the importance of characterizing the phase transition at the edge of the devices. Using backscattered electron diffraction technology distinguishes that it is more difficult to nucleate the ferroelectric orthorhombic phase at the edge region of the ferroelectric capacitors under a low-temperature process. The edge regions are dominated by the monoclinic phase or amorphous phase. Finally, the improved approaches were proposed and demonstrated. The 10 nm-thick Hf0.5Zr0.5O2 ferroelectric capacitors with the optimized edge characteristics were realized by using the nitride passivation layer. The devices adopted the CMOS BEOL compatible annealing at 400 °C for 600 s and achieved excellent ferroelectric characteristics with a 2Pr value as high as 48 μC/cm2. Furthermore, the outstanding area scalability was demonstrated, and the leakage current was improved by one order of magnitude. Not only demonstrates the CMOS BEOL compatible annealing and the area scalability, but this work also enables the further thickness scalability of Hf0.5Zr0.5O2. We optimized the interfacial layer of the ferroelectric capacitor structure to reduce the thickness from 10 nm to 6 nm for low-power applications.
The metal-ferroelectric-metal capacitors are widely used in the various ferroelectric non-volatile memory such as FeRAM, FTJ, and MFMFET. The ferroelectric capacitors are integrated into the CMOS back-end-of-line (BEOL) process so that the design and process windows of the CMOS front-end-of-line (FEOL) process and the CMOS BEOL process could be independently optimized. Most studies use atomic-layer deposition technology to deposit HfxZr1-xO2 thin films. The as-deposited HfxZr1-xO2 films are usually in an amorphous state. After the rapid thermal annealing, they could be transformed into the ferroelectric orthorhombic phase. Most literature pointed out that the temperature required for the rapid thermal annealing process is between 500 °C and 700 °C. This annealing temperature range is higher than the desirable standard CMOS BEOL process temperature. The relatively high annealing temperature leads to negative impacts on the metal integrity and the reliability issues on the CMOS. Therefore, using the CMOS BEOL compatible process temperature to achieve excellent ferroelectricity is an important research topic. Recently, several studies have proposed effective low-temperature process approaches, such as plasma-enhanced atomic-layer deposition (PE-ALD), deep ultraviolet light irradiation, stress optimization, and high-pressure annealing. However, most of them largely ignore the area scalability under the low-temperature process. High area scalability is an important factor for cost-effective mass production in the era of artificial intelligence and IoT.
This work first researches the scalability issue with the CMOS BEOL compatible annealing through the device test structure design, the electrical test and analysis methodology such as the P-E hysteresis measurement, the constant voltage stress (CVS) leakage, and reliability tests. Meanwhile, the physical analysis was also performed to diagnose the cause of poor area scalability under a low-temperature process. In addition, the failure model was established. This work finds the importance of characterizing the phase transition at the edge of the devices. Using backscattered electron diffraction technology distinguishes that it is more difficult to nucleate the ferroelectric orthorhombic phase at the edge region of the ferroelectric capacitors under a low-temperature process. The edge regions are dominated by the monoclinic phase or amorphous phase. Finally, the improved approaches were proposed and demonstrated. The 10 nm-thick Hf0.5Zr0.5O2 ferroelectric capacitors with the optimized edge characteristics were realized by using the nitride passivation layer. The devices adopted the CMOS BEOL compatible annealing at 400 °C for 600 s and achieved excellent ferroelectric characteristics with a 2Pr value as high as 48 μC/cm2. Furthermore, the outstanding area scalability was demonstrated, and the leakage current was improved by one order of magnitude. Not only demonstrates the CMOS BEOL compatible annealing and the area scalability, but this work also enables the further thickness scalability of Hf0.5Zr0.5O2. We optimized the interfacial layer of the ferroelectric capacitor structure to reduce the thickness from 10 nm to 6 nm for low-power applications.