T6熱處理後之選擇性雷射熔化AlSi10Mg的微結構與機械性質研究
Investigation of the Microstructure & Mechanical Properties of SLM AlSi10Mg after T6 Treatment
摘要
AlSi10Mg屬於近共晶的鋁矽合金,具有低比重、高比強度和良好的電、熱傳導性,而由於元素組成中含有高比例的矽成分,有利於在高溫下保持流動性、避免快速冷卻時發生破裂,因此在眾多鋁合金組成中,為其中一種適合使用選擇性雷射熔化(Selective Laser Melting, SLM)來製備的鋁合金。利用選擇性雷射熔化製備的AlSi10Mg在微結構上會有特殊的共晶矽網絡狀結構,可分成(FMP、CMP、HAZ)三個微結構部位。在經過T6熱處理後,可觀察到共晶矽的網絡狀結構消失,而有了矽顆粒的析出;而在機械性質的表現上,在固溶處理後維氏硬度大幅下降,經過時效處理後提升維氏硬度,到一定峰值後開始下降,即發生過時效。本研究著重在選擇性雷射熔化製備的AlSi10Mg在T6熱處理過後,微結構的演進與對機械性質的影響。
AlSi10Mg is a near-eutectic aluminum-silicon alloy with low specific gravity, high specific strength, and good electrical and thermal conductivity. High proportion of silicon in the chemical composition contributes to maintaining fluidity at high temperatures and avoiding crack caused by rapid cooling. Therefore, AlSi10Mg is one of the most widely used aluminum alloys for Selective Laser Melting (SLM). The SLM built-AlSi10Mg has a special microstructure of eutectic silicon network, which can be divided into three distinct microstructure regions (FMP, CMP, HAZ). After T6 heat treatment, it can be observed that the network structure of eutectic silicon disappears, and there is precipitation of silicon particles. The Vickers hardness decreases significantly after solution treatment and increases after aging treatment. Vickers hardness begins to decrease after reaching a certain peak value at which over-aging occurs. The present study focuses on the evolution of microstructure and its effect on the mechanical properties of SLM built-AlSi10Mg after T6 heat treatment.