有機無機混成鈣鈦礦量子點之配體工程與發光元件之應用
Ligand Engineering of Organic-Inorganic Hybrid Perovskite Quantum Dots and their Light-Emitting Applications
摘要
Organic-inorganic hybrid perovskite quantum dots with two different surface ligands are synthesized by using ligand-assisted reprecipitation method. The peak position of the photoluminescence (PL) from FAPbBr3 (FA+: formamidinium) PeQDs is unchanged after replacing the short chain n-octylamine (Octa) ligand to long chain oleylamine (OAm). The highest photoluminescence quantum yield (PLQY) of the OAm-capped PeQDs is as high as 96±3% and the full width at half-maximum (FWHM) of the PL emission is also as narrow as 25.6±0.8 nm. After mixing the PeQDs with poly(vinylcinnamate) (PVCN), the resulting nanocomposites can be patterned using UV light to provide a feature size less than 5 m for use micro-light-emitting diodes (μLEDs). Further, the nanocomposites containing OAm-capped PeQDs exhibit better film properties after patterning, suggesting that PVCN could protect the PeQDs better in the nanocomposition films. From the atomic force microscopy (AFM) images, we observe less phase separation between the PeQDs and PVCN polymers, presumably due to the ligand effects. Finally, the stability test indicates that the thin films containing OAm-capped FAPbBr3 QDs are more stable. In summary, the quality of the photopatternable films can be improved through with ligand engineering.
本論文以配體輔助再沈澱法(LARP)合成不同配體的有機無機混成鈣鈦礦量子點,當配體從較短鏈的辛胺改成長鏈的油胺之後,鈣鈦礦量子點甲苯膠體溶液之發光光譜位置並沒有太大變化,最大的螢光量子效率達96±3%,而最小半高寬也達25.6±0.8 nm。將鈣鈦礦量子點混合高分子材料聚乙烯醇肉桂酸酯後,此奈米複合薄膜可以UV光進行黃光圖案化製程,線寬可以小於5 𝜇m,可應用於微發光二極體的色轉換層。我們也發現以長鏈的油胺包覆的鈣鈦礦量子點製作的薄膜有更加的黃光製程特性,從原子力顯微鏡分析薄膜表面發現,以長鏈的油胺包覆的鈣鈦礦量子點與高分子之間有較少的相分離現象,可推論高分子可更有效地包覆鈣鈦礦量子點。最後我們也進行了穩定性測試,發現以長鏈的油胺包覆的鈣鈦礦量子點製作的奈米複合薄膜有較佳的穩定性。這些結果顯示配體工程可有效地改善可光圖形化鈣鈦礦量子點高分子薄膜的特性。