高效能高穩定性矽基複合材料開發:具綠色環保與實用之合成方法應用於鋰離子電池
Sustainable Silicon-Based Composite Development: A Green and Practical Synthesis Approach for Superior Li-ion Batteries
摘要
本研究比較了 α-Si3N4 和 β-Si3N4 的鋰化/脫鋰性能,並檢驗了碳塗層的影響。將 β-Si3N4 作為第二相納入 Si 中,在 β-Si3N4/Si 界面引入了新的 N−Si−O 物種,從而提高了比電容量。於臨場分析實驗中表明,β-Si3N4 在鋰化過程中被部分消耗,形成良好的導電 Li3N。由此產生的碳包覆 β-Si3N4/Si 複合陽極在 0.2 和 5 A g−1 電流下表現出 1068 和 480 mAh g−1 的比電容量,並且在 300 次循環後具有出色的穩定性。接下來,利用超臨界二氧化碳 (SCCO2) 在矽顆粒上生成 SiOx/碳。它產生了連續的 SiOx 層,減輕了鋰化/脫鋰過程中的體積變化。 Si@SiOx 周圍塗有一層薄且較少氧官能基的高電導率之碳將其包覆。使用葡萄糖前驅物可實現最高的振實密度和最佳的 Li+ 傳輸動力學,在 5 A g-1 下實現 918 mAh g-1 比電容量,同時在 300 次循環後保持電極完整性。最後,利用SCCO2作為介質和前驅體,製備碳氧化矽(SiOC)塗層,退火後形成核殼Si@SiOC顆粒。柔性SiOC層透過連接Si@SiOC顆粒來輔助電子和Li+傳輸。 SiOC 層也減少了 Li15Si4 晶體尺寸的生長,增強了其循環可逆性。 Si@SiOC電極在0.2和5 A g−1下的比電容量分別為2250和1013 mAh g−1。 500 次循環後,它還表現出強大的穩定性。所提出的合成方案為鋰離子電池獨特的矽基陽極提供了環保、經濟且可擴展的生產方法。
This study compares the lithiation/delithiation properties of α-Si3N4 and β-Si3N4 for the first time. Also, it examined the effects of carbon-coating on them. Incorporating β-Si3N4 as a secondary phase in a Si introduced new N−Si−O species at the β-Si3N4/Si interface, enhancing specific capacities. Operando analyses revealed that β-Si3N4 was partially consumed during lithiation, forming a favourable conductive Li3N. The resulting C-coated β-Si3N4/Si composite anode demonstrated promising specific capacities of 1068 and 480 mAh g−1 at 0.2 and 5 A g−1, along with excellent stability after 300 cycles. Next, supercritical CO2 (SCCO2) was harnessed to create a SiOx/carbon on Si particles. It yielded a continuous SiOx layer, mitigating volume changes during lithiation/delithiation. A thin, high-conductivity carbon with fewer oxygen-functional groups was coated around the Si@SiOx. Using glucose precursor resulted in the highest tap density and the best Li+ transport kinetics, achieving a notable specific capacity of 918 mAh g–1 at 5 A g–1 while retaining electrode integrity after 300 cycles. For the last part, utilizing SCCO2 as medium and precursor, a silicon oxycarbide (SiOC) coating was produced, forming core-shell Si@SiOC particles after annealing. The flexible SiOC layer aided electron and Li+ transport by connecting Si@SiOC particles. The SiOC layer also reduced the Li15Si4 crystal size growth, enhancing its cycling reversibility. The Si@SiOC electrode exhibited specific capacities of 2250 and 1013 mAh g−1 at 0.2 and 5 A g−1, respectively. It also demonstrated robust stability after 500 cycles. The proposed synthesis protocols present eco-friendly, cost-effective, and scalable production methods for a distinctive Si-based anode for Li-ion batteries.
所屬典藏
材料科學與工程學系引用此條目
Hernandha, R. F. H. (2023). Sustainable Silicon-Based Composite Development: A Green and Practical Synthesis Approach for Superior Li-ion Batteries. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/834
引用文字依 APA 第 7 版格式自動產生,使用前請再核對。
分享
永久網址:https://thesis.lib.nycu.edu.tw/handle/20.500.14371/834