高功率元件陶瓷散熱基板之熱循環評估

Thermal Cycling effects on Thermal Dissipation Ceramic Substrates for High Power Electronics

檔案

日期

2023

類型

語言

中文

摘要

本研究將評估三種不同的陶瓷散熱基板在經過熱循環後的性能評估,第一種是DBA (Direct Bonded Aluminium)散熱基板,利用暫態液相法於645⁰C接合Al-AlN。第二種為DBAC(Direct bonded Aluminum and Copper)散熱基板,利用已完成的DBA再加上銅於555⁰C採取共晶接合法Cu-Al,第三種為DBAC(Ag),在DBAC的基礎上加入20µm的銀箔當作銅鋁的中間層,於560⁰C接合Al-Ag-Cu。本研究將三種陶瓷散熱基板進行0、100、200、500次的-50℃~150℃冷熱循環測試,並進行剪切強度試驗、微觀結構分析、熱傳導評估及斷裂面分析判斷裂痕生成機制。
DBA的初始接合強度為36.2MPa,在500次循環後下降至11.2MPa,氮化鋁內部有YAlO3(第二相)的存在,在熱循環過程中,會因熱膨脹係數(CTE)不一致導致殘留應力無法釋放,進而造成裂紋產生。而DBAC的初始接合強度為28.2MPa,在500次循環後下降至12.3MPa,由於Al-Cu介金屬層的硬脆性遠高於純銅純鋁,且每一個相的CTE皆不同,循環過程中產生的不斷累積進而造成嚴重的斷裂在介金屬層上。DBAC(Ag)的初始接合強度為32.7MPa,經過500次循環後則下降至18.5MPa,銀箔加入成功抑制硬脆且導熱性差的Al-Cu介金屬層產生,由於銀和鋁的CTE相差較大,在500循環後,除了接合面的邊緣處有發生分離現象外,整體接合面大部分皆維持良好接合,DBAC(Ag) 陶瓷散熱基板的耐用度確實高於DBA和DBAC。
This study will evaluate the performance of three different ceramic heat sink substrates after thermal cycling. The first is a DBA (Direct Bonded Aluminum) heat sink substrate, which is bonded to Al-AlN at 645⁰C using a transient liquid phase method. The second type is DBAC (Direct bonded Aluminum and Copper) heat dissipation substrate, which uses the completed DBA plus copper at 555⁰C to adopt the eutectic bonding method Cu-Al, and the third type is DBAC (Ag), which is added on the basis of DBAC The 20µm silver foil is used as the intermediate layer of copper and aluminum, and Al-Ag-Cu is bonded at 560⁰C. In this study, three kinds of ceramic heat dissipation substrates were subjected to 0, 100, 200, 500 times of -50℃ ~ 150℃ cold and hot cycle tests, and shear strength tests, microstructure analysis, heat conduction evaluation and fracture surface analysis were carried out to determine the crack formation mechanism.
The initial bonding strength of DBA is 36.2MPa, which drops to 11.2MPa after 500 cycles. There is YAlO3 (second phase) inside the aluminum nitride. During the thermal cycle, the residual stress will be caused by the inconsistent coefficient of thermal expansion (CTE). Unable to release, thus causing cracks. The initial bonding strength of DBAC is 28.2MPa, which drops to 12.3MPa after 500 cycles. Since the hardness and brittleness of the Al-Cu interlayer metal layer is much higher than that of pure copper and pure aluminum, and the CTE of each phase is different, the cycle process produces the continuous accumulation and then cause serious fracture on the intermetallic layer. The initial bonding strength of DBAC(Ag) was 32.7MPa, and it dropped to 18.5MPa after 500 cycles. The addition of silver foil successfully suppressed the generation of hard, brittle and poor thermal conductivity Al-Cu intermetallic layer. Due to the large difference in CTE between silver and aluminum , after 500 cycles, except for the separation at the edge of the joint surface, most of the overall joint surface maintains a good joint. The durability of the DBAC(Ag) ceramic heat dissipation substrate is indeed higher than that of DBA and DBAC.
顯示完整詮釋資料 統計資料

引用此條目

江鴻懋 (2023). 高功率元件陶瓷散熱基板之熱循環評估. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/83402