3DIC 中電鍍銅膜厚度對介面孔洞演變的影響

Effect of copper thicknesses on the evolution of voids in Cu-Cu wafer bonding for 3DIC

檔案

日期

2023

類型

語言

中文

摘要

隨著近年來 5G、人工智慧等領域迅速發展與電子產品走向輕薄短小的趨勢下,
已逐漸逼近摩爾定律(Moore’s law)的極限,為了使晶片性能提升,業界在各式製程
技術上尋求突破,其中一項為先進封裝技術。先進封裝技術以三維積體電路(3D-IC)
作為突破方向,利用堆疊整合的方式提升晶片運算效能,並發展出利用矽穿孔
(Through-Silicon Via;TSV)技術將晶片垂直堆疊與接合。由於銅與其他金屬相比,
具有優異物理性質與節省成本等優點,時常作為 TSV 與接合的材料,進而發展出
了銅-銅直接接合技術。銅-銅接合前,需利用化學機械研磨(CMP)將接合表面平坦
化,但現今技術無法達成原子級平坦,使得接合後的介面會產生孔洞,這些孔洞會
降低電性表現與接合強度等不良影響。因此本實驗為了探討銅膜厚度介面孔洞的
關係,利用不同厚度的電鍍銅薄膜進行接合,並對接合後孔洞形貌的演變進行比較。
本實驗使用三種厚度之隨機取向電鍍銅試片,每組皆使用相同厚度的試片進
行對接。利用濕蝕刻方式將試片表面粗化,並與未粗化試片接合使介面出現人工孔
洞,初步熱壓接合溫度為 200℃、250℃、300℃,隨後再進行加壓退火,接合後透
過聚焦離子束(FIB)對接合介面的孔洞進行觀察,並利用孔洞高度(Void height)、孔
洞比例(Void fraction)以及接合比例(Bonding fraction)三種參數對接合結果進行分析
比較。接合結果顯示較厚之電鍍銅試片,能在較短的接合時間下達到良好的接合效
果與觀察到明顯的表面擴散。
With the rapid development of 5G, artificial intelligence, and other fields, as well as the trend towards smaller and thinner electronic products in recent years, the limit of
Moore's law has gradually been approached. In order to improve chip performance, the industry is seeking breakthroughs in Semiconductor process technologies, one of which is advanced packaging technology. Copper has excellent physical properties and costsaving advantages, and is often used as the material for TSV and bonding, leading to the
development of Cu-Cu direct bonding technology. Before bonding, chemical mechanical polishing (CMP) is required to flatten the bonding surface, but current technology cannot achieve atomic-level flatness, the interface after bonding will produce holes, which will negatively impact electrical performance and bonding strength. In order to investigate the influence of copper film thickness on interface holes
in this experiment, different thicknesses of electroplated copper thin films were used for bonding, and the evolution of hole morphology after bonding was compared.
In this experiment, three randomly oriented electroplated copper samples with different thicknesses were used, and each group was bonded with samples of the same thickness. The sample surface was roughened using a wet etching method, and then bond with an unroughened sample to create artificial holes . Pre-bonding temperatures at 200℃,
250℃, and 300℃ , followed by pressure annealing. After bonding, the holes at the bonding interface were observed using focused ion beam microscope (FIB), and the
bonding results were analyzed and compared using three parameters: void height, void fraction, and bonding fraction. The bonding results showed that thicker electroplated copper samples achieved good bonding results and significant surface diffusion in a shorter bonding time.
顯示完整詮釋資料 統計資料

引用此條目

許凱甯 (2023). 3DIC 中電鍍銅膜厚度對介面孔洞演變的影響. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/83405

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享

永久網址:https://thesis.lib.nycu.edu.tw/handle/20.500.14371/83405