This study conducted pool boiling experiments on high-flux samples with porous coating and smooth sample. The sample material was 90-10 copper-nickel alloy(C70600). For the high-flux samples, sintering with powder particle sizes of 45, 75, and 150 μm and coating thicknesses of 400 and 600 μm. The smooth samples were polished using 150 Cw sandpaper. The heat fluxes were ranging from 10 to 120 kW/m2, at working pressures of 1.5 and 2 bars, using R-1233zd(E) as the working fluid. Images of the high-flux samples were captured using an Optical microscope (OM) and scanning electron microscope (SEM). Additionally, a high-speed camera (Phantom EVO E-310L) was employed to record bubble behavior, allowing for the observation oh bubble size and quantity. The aim was to determine the heat transfer enhancement of high-flux samples compared to smooth sample.
For the smooth samples, at 1.5 bars, the heat transfer coefficient ranged from 1338.98 to 4693.01 W/m2-K. At 2 bars, this value ranged from 1667.93 to 4969.64 W/m2-K. However, the high-flux samples (such as 45_400, 75_400, 150_400, and 150_600 samples) exhibited even more impressive enhancements in heat transfer enhancement. For example, the 75_400 sample at a 1.5 bars achieved a heat transfer coefficient as high as 5418.08 to 18289.79 W/m2-K, with a enhancement of 266%. At 2 bars, it reached an even higher range of 7598.19 to 23026.12 W/m2-K, with a enhancement of 312%. Other high-flux samples, such as the 45_400 and 150_400 samples, also showed significant improvements in heat transfer coefficients. The 45_400 sample, at 1.5 bars, achieved a heat transfer coefficient ranging from 5719.02 to 18918.60 W/m2-K, representing a 266% increase compared to the smooth sample. These data not only demonstrate the remarkable advantages of high-flux samples in terms of heat transfer coefficients but also emphasize their excellent performance in controlling superheat, For example, the 150_600 sample achieved a maximum reduction of 13.45 K at 1.5 bars compared to the smooth sample.
本研究對擁有多孔塗層的高通量(high-flux)試片與平滑試片進行池沸騰實驗。試片材質為90-10銅鎳合金(C70600),高通量試片在其沸騰表面進行燒結,選用粒徑45、75、150 μm之粉末,塗層厚度400、600 μm,平滑試片使用150號砂紙進行表面拋光處理。本實驗在熱通量10~120 kW/m2間、環境壓力為1.5、2 bar下進行,工作液體為R-1233zd(E)。並由光學金相顯微鏡(Optical Microscope,OM)、電子式掃描顯微鏡(Scanning Electron Microscope,SEM)拍攝高通量試片,以高速攝影機(Phantom EVO E-310L)拍攝氣泡,觀察氣泡尺寸及數量,以求得高通量試片對平滑試片之熱傳增強。
對於平滑試片,在1.5 bar的壓力下,熱傳係數為1338.98~4693.01 W/m2-K。而在2 bar的壓力下,熱傳係數則為1667.93~4969.64 W/m2-K。然而,高通量試片(如45_400試片、74_400試片、150_400試片、150_600試片)在熱傳係數方面表現出更為優秀的熱傳增強,例如,75_400試片在1.5 bar的壓力下熱傳係數高達5418.08~18289.79 W/m2-K,最高提升266%。在2 bar的壓力下,熱傳係數更是達到了7598.19~23026.12 W/m2-K,最高提升312%。
其他高通量試片,如45_400試片和150_400試片,也在熱傳係數方面表現出顯著的提升,45_400試片在1.5 bar的工作壓力下,熱傳係數達5719.02~18918.60 W/m2-K,相較平滑試片提升了266%。這些數據不僅顯示高通量試片在熱傳係數方面有出色的優勢,而且也指出了它們在壁過熱度控制方面的優異表現,如150_600試片在1.5 bar的壓力下,相較平滑試片最大減少達到13.45 K。

所屬典藏

機械工程學系
顯示完整詮釋資料 統計資料

引用此條目

楊卓昕 (2023). 燒結多孔塗層於平板之沸騰熱傳研究. https://thesis.lib.nycu.edu.tw/handle/20.500.14371/869

BibTeX RIS

引用文字依 APA 第 7 版格式自動產生,使用前請再核對。

分享

永久網址:https://thesis.lib.nycu.edu.tw/handle/20.500.14371/869