利用暫態液相法接合鋁/鈦平板
顯示簡易詮釋資料 統計資料| 欄位 | 內容 | 語言 |
|---|---|---|
dc.contributor.advisor |
林健正 | |
dc.contributor.advisor |
Lin, Chien-Cheng | |
dc.contributor.author |
楊宗霖 | |
dc.contributor.author |
Yang, Zong-Lin | |
dc.contributor.college |
工學院 | |
dc.contributor.committee |
林健正 | |
dc.contributor.committee |
吳耀銓 | |
dc.contributor.committee |
林昆霖 | |
dc.contributor.committee |
Lin, Chien-Cheng | |
dc.contributor.committee |
Wu, Yew-Chung | |
dc.contributor.committee |
Lin, Kun–Lin | |
dc.contributor.department |
材料科學與工程學系所 | |
dc.contributor.studentid |
0651531 | |
dc.date.NCLavailable |
2021/08/06 | |
dc.date.USTavailable |
2021/08/06 | |
dc.date.issued |
2019 | |
dc.date.issuedROC |
108 | |
dc.date.schoolyear |
107 | |
dc.description.abstract |
鈦具有優異的機械性能,使用於航太工業、生物醫學等方面已大有佳績,但是由於鈦本身昂貴不已、強度高且不容易加工成形,故可以結合鋁合金已利於達到成本降低、輕量化、易於加工之雙贏局面。然而,兩金屬之熱膨脹係數、熔點、導電性、導熱性等等各項物理性質差異甚大,故很難接合為一體。本研究利用雙電子槍蒸鍍鎳、銅、矽、鍺各300奈米為中間層以利於暫態液相接合法來接合兩金屬,並全程使用氬氣保護氣氛防止氧化,該方法取決於鋁金屬與中間蒸鍍層之間的共晶反應在接合界面處形成薄的連續液體來潤濕鋁金屬表面,即可在較低溫之情況使鋁與鈦接合並且形成Al3Ti中間反應相化合物,該反應還具有能夠除去表面氧化物的優點。 本研究利用使用X-射線繞射分析(XRD)來鑑定相、熱場發射掃描電子顯微鏡和能量散射光譜儀(FESEM / EDS),穿透式電子顯微鏡和能量散射光譜儀(TEM / EDS)觀察Al / Ti反應界面微觀組織,並且使用超音波掃描顯微鏡(SAT)來分析鈦/鋁接合界面之孔隙分布,也利用拉伸試驗來測試兩金屬之接合強度以及彎曲試驗來測量彎曲模數,結果為沉積鎳元素於鋁金屬表面的結果皆優於其餘三者,沉積鎳為共晶元素可使鋁與鈦在氬氣一大氣壓氣氛580°C下完成,且孔隙率低至1.56%、剪應力強度高至37 MPa、彎曲模數高至55 GPa。 | |
dc.description.abstract |
Titanium has excellent mechanical properties and has been used in aerospace, biomedical applications. However, titanium is expensive and difficult to be machined due to its high strength. Thus, it is possible to join the aluminum, which is low cost, light weight, and easy processing, to form a bilayer structure of metals. The physical properties of the aluminum and titanium, such as thermal expansion coefficient, melting point, electrical conductivity, thermal conductivity, etc., are great different, so it is difficult to bond together. In this study, dual E-Gun evaporation system were used to evaporate nickel, copper, silicon and germanium each 300 nm as an intermediate layer to facilitate the transient liquid phase (TLP) bonding method to bond the aluminum and titanium. In order to prevent the oxidation after bonding, the samples will be annealed at the atmosphere of argon gas. The samples will be used X-ray diffraction analysis (XRD) to identify the reactional phases. The thermal field emission scanning electron microscopy and energy scatter spectrometer (FESEM / EDS) and transmission electron microscopy and energy scatter spectrometer (TEM / EDS) will be performed to observe the microstructure of the titanium/aluminum reaction and the scanning acoustic tomography (SAT) will be used to analyze the pore distribution of the titanium/aluminum joint. The shear and bending strength are used to evaluate the joint strength and bending modulus of the two metals. The results indicated the aluminum is bonded to the titanium at a lower temperature and formed an Al3Ti intermediate reaction phase compound. The deposition of nickel on the aluminum metal to join titanium possessed the best bonding properties than that of copper, silicon, and germanium. The void distribution, shear strength, and bending modulus of the aluminum/titanium plate with nickel film were measured as low as 1.56%, 37 MPa, and 55 GPa, respectively. | |
dc.description.abstractopendate |
2021/08/06 | |
dc.description.degree |
碩士 | |
dc.description.tableofcontents |
摘要...iAbstract...iii誌謝...vi表目錄...xi圖目錄...xii第一章 前言...1第二章 原理與文獻回顧...32.1 鈦金屬之發展背景...32.1.1 Grade.2鈦合金...32.1.2 鈦合金之應用...42.2 鋁合金之發展背景...52.2.1 AA6061鋁合金...62.2.2 鋁合金之應用...62.3 鈦合金與鋁合金之接合...72.3.1 暫態液相接合法(Transient Liquid Phase)...72.3.2 雷射焊接接合法(Laser welding)...82.3.3 焊料擴散接合法(Diffusion welding)...92.3.4 攪拌螺旋接合法(Friction stir welding)...92.4 鈦合金與鋁合金接合後之性質...102.4.1 附著力的強度(Adhesion Strength)測試...102.4.2 潤濕能力(Wettability)測試...102.4.3 彎曲測試(Bending test)...112.4.4 拉伸測試(Tensile test)...13第三章 實驗步驟與儀器原理...233.1 實驗材料...233.1.1 Gr.2 鈦合金 (Grade.2 Titanium alloy)...233.1.2 6061鋁合金 (6061 Aluminum alloy)...233.2 Grade.2 鈦合金接合6061鋁合金...243.2.1 接合前之試片製備...243.2.2 鈦/鋁接合...243.3 接合之後的樣品製備與分析...253.3.1 鈦/鋁界面微觀分析試片製備...253.3.2 界面與接合中間層之微觀分析...263.3.3 界面缺陷分析...273.3.4 拉伸試驗...283.3.5 三點彎曲試驗...293.4 儀器原理...303.4.1 超音波震盪機 (Ultrasonic Cleaner)...303.4.2 雙電子束蒸鍍機 (Dual E-Gun Evaporation)...303.4.3 真空濺鍍機 (Sputtering System)...313.4.4 真空管型高溫爐 (tube furnace)...323.4.5 掃描式電子顯微鏡 (Scanning Electron Microscope, SEM)/X光能量分散光譜儀 (Electron Dispersive Spectrum, EDS)...323.4.6 聚焦離子束電子束掃描式顯微鏡 (Dual-beam Focused Ion Beam, FIB)...343.4.7 穿透式電子顯微鏡 (Transmission Electron Microscope, TEM)/ X光能量分散光譜儀 (Electron Dispersive Spectrum, EDS)...353.4.8 超音波掃描顯微鏡(Scanning Acoustic Tomography, SAT)...36第四章 結果與討論...484.1 接合前鈦合金/鋁合金之相鑑定...484.2 接合後之微觀結構分析...484.2.1 SEM之微觀結構分析...484.2.2 TEM之微觀結構分析...504.3 鈦合金與鋁合金接合後內部缺陷分析...534.4 鈦合金與鋁合金接合界面強度分析...544.4.1 接合後拉伸試驗分析...544.4.2 接合後彎曲試驗分析...554.5 鈦合金與鋁合金接合機制探討...564.6 Al3Ti 、Al15Fe3Si2之生成機制...56第五章 結論...75文獻回顧...77 | |
dc.identifier.citation |
1.ASM Handbook, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM International Handbook Committee., tenth ed., vol. 2, 1990.2.W.S. Miller, L. Zhuang, J. Bottema, A.J. Wittebrood, P. De Smet, A. Haszler, A. Vieregge, Mater. Sci. Eng. A 280 (1) (2000) 37.3.K. Faller, F.H. (Sam) Froes, JOM 53 (4) (2001) 27.4.https://www.sciencedirect.com/science/article/pii/S2238785418302813.5.S.M. Sze, VLSI Technology, McGraw-Hill, New York, 1983.6.K.H. Rendigs, Materials Science Forum 242 (1997) 11.7.A. Heinz, A. Haszler, C. Keidel, S. Moldenhauer, R. Benedictus, W.S. Miller, Mater. Sci. Eng. A 280 (1) (2000) 102.8.J.R. Williamson, in: N.E. Paton, C.H. Hamilton (eds.), Superplastic forming of structural alloys TMS AIME, Warrendale, 1982, p. 291.9.S. Chen, M. Zhang, J. Huang, C. Cui, H. Zhang, X. Zhao, Microstructures and mechanical property of laser butt welding of titanium alloy to stainless steel, Mater. Des. 53 (2014) 504-511. https://doi.org/10.1016/j.matdes.2013.07.044. [3] P. Li, H. Dong, Y. Xia, X. Hao, S. Wang, L. Pan, J. Zhou, Inhomogeneous interface structure and mechanical properties of rotary friction welded TC4 titanium alloy/316L stainless steel joints, J. Manuf. Process. 33 (2018) 54-63. https://doi.org/10.1016/j.jmapro.2018.05.001.10.M. Tisza, Lightweight Manufacturing of Automotive Parts, AutoTech project, No.: TAMOP-4-2-2.A-11/1/KONV-2012-0029, Co- financed by the European Union and the Hungarian Government, Miskolc-Hungary, 2012-2014.11.Woong H. Sohn, Ha H. Bong, Soon H. Hong, Microstructure and bonding mechanism of Al/Ti bonded joint using Al_/10Si_/1Mg filler metal, Materials Science and Engineering A355 (2003) 231_/240.12.Wu, A., Song, Z., Nakata, K., Liao, J., Zhou, L., Interface and properties of the friction stir welded joints of titanium alloy Ti6Al4V with aluminum alloy 6061, Materials and Design (2014), doi: http://dx.doi.org/10.1016/j.matdes.2014.12.01513.M. Ma, P. Huo, W.C. Liu, G.J. Wang, D.M. Wang, Microstructure and mechanical properties of Al/Ti/Al laminated composites prepared by roll bonding, Materials Science & Engineering A, http://dx.doi.org/ 10.1016/j.msea.2015.03.086]14.S.Y. Changa,∗, L.C. Tsaob, Y.H. Lei a, S.M. Maoa, C.H. Huang, Brazing of 6061 aluminum alloy/Ti–6Al–4V using Al–Si–Cu–Ge filler metals, Journal of Materials Processing Technology 212 (2012) 8– 1415.M.S. Kenevisi, S.M. Mousavi Khoie, An investigation on microstructure and mechanical properties of Al7075 to Ti–6Al–4V Transient Liquid Phase (TLP) bonded joint, Materials and Design 38 (2012) 19–2516.S.Y. Changa, L.C. Tsaob, T.Y. Li a, T.H. Chuangc,∗, Joining 6061 aluminum alloy with Al–Si–Cu filler metals, Journal of Alloys and Compounds 488 (2009) 174–18017.Shaohong Wanga ,*, Heping Zhoua, Yuping Kangb, The influence of rare earth elements on microstructures and properties of 6061 aluminum alloy vacuum-brazed joints, Journal of Alloys and Compounds 352 (2003) 79–8318.Shant Prakash Gupta*, Intermetallic compounds in diffusion couples of Ti with an Al–Si eutectic alloy, Materials Characterization 49 (2003) 321– 33019.Shaohong Wanga ,*, Heping Zhoua, Yuping Kangb, The influence of rare earth elements on microstructures and properties of 6061 aluminum alloy vacuum-brazed joints, Journal of Alloys and Compounds 352 (2003) 79–8320.A. Arankalle, Advances in lightweight materials for body in white, in: Bajpai, Chandrasekhar (Eds.), Innovative Design and Development Practices in Aerospace and Automotive Engineering, Lecture Notes in Mechanical Engineering, Springer, Singapore, 2016, pp. 517e525, 18 September 2016.21.Vaidya WV, Horstmann M, Ventzke V, Petrovski B, Koçak M, Kocik R, Tempus G. Improving interfacial properties of a laser beam welded dissimilar joint of aluminium AA6056 and titanium Ti6Al4V for aeronautical applications. J Mater Sci 2010;45:6242-54.22.Möller F, Grden M, Thomy C, Vollertsen F. Combined Laser Beam Welding and Brazing Process for Aluminium Titanium Hybrid Structures. Physics Procedia 2011;12, Part A:215-23.23.Song Z, Nakata K, Wu A, Liao J. Interfacial microstructure and mechanical property of Ti6Al4V/A6061 dissimilar joint by direct laser brazing without filler metal and groove. Mater Sci Eng A 2013;560:111-20.24.Chen S, Li L, Chen Y, Dai J, Huang J. Improving interfacial reaction nonhomogeneity during laser welding–brazing aluminum to titanium. Mater Des 2011;32:4408-16.25.Yao W, Wu AP, Zou GS, Ren JL. Formation process of the bonding joint in Ti/Al diffusion bonding. Materials Science and Engineering: A 2008;480:456-63.26.Yao W, Wu AP, Zou GS, Ren JL. 5A06/TA2 diffusion bonding with Nb diffusion-retarding layers. Mater Lett 2008;62:2836-9.27.Alhazaa AN, Khan TI. Diffusion bonding of Al7075 to Ti-6Al-4V using Cu coatings and Sn-3.6Ag-1Cu interlayers. J Alloy Compd 2010;494:351-8. 1228.Kimura M, Nakamura S, Kusaka M, Seo K, Fuji A. Mechanical properties of friction welded joint between Ti-6Al-4V alloy and Al-Mg alloy (AA5052). Science and Technology of Welding & Joining 2005;10:666-72.29.Katoh K, Tokisue H. Effect of insert metal on mechanical properties of friction welded 5052 aluminum alloy to pure titanium joint. Journal of Japan Institute of Light Metals 2004;54:430-5.30.Fuji A, Ameyama K, North TH. Influence of silicon in aluminium on the mechanical properties of titanium/aluminium friction joints. J Mater Sci 1995;30:5185-91.31.L.M. Peng ∗, H. Li, J.H. Wang, Processing and mechanical behavior of laminated titanium–titanium tri-aluminide (Ti–Al3Ti) composites, Materials Science and Engineering A 406 (2005) 309–31832.https://kknews.cc/zh-tw/science/4vpzjz2.html33.Greenwood, N. N.; Earnshaw, A. Chemistry of the Elements 2nd. Oxford: Butterworth-Heinemann. 1997. ISBN 0-7506-3365-4.34.https://www.moea.gov.tw/MNS/doit/industrytech/IndustryTech.aspx?menu_id=13545&it_id=11235.Moiseyev, Valentin N. Titanium Alloys: Russian Aircraft and Aerospace Applications. Taylor and Francis, LLC. 2006: 196. ISBN 9780849332739.36.https://zh.wikipedia.org/wiki/%E9%92%9B#cite_note-LANL-537.http://www.taiwell.com.tw/aluminium1.htm38.http://www.yuan-tai.com.tw/images/table02.pdf39.https://kknews.cc/zh-tw/home/4vxelk2.html40.Kuromitsu, Y., et al. Direct bonded aluminum on aluminum nitride substrates via a transient liquid phase and its application. in 2010 6th International Conference on Integrated Power Electronics Systems. 2010.41.https://kknews.cc/zh-tw/news/e4xkgzr.html42.https://www.geniray.com/09.html43.https://kknews.cc/zh-tw/science/znl3qkp.html44.Volinsky, A.A., N.R. Moody, and W.W. Gerberich, Interfacial toughness measurements for thin films on substrates. Acta Materialia, 2002. 50(3): p. 441-466.45.Dauskardt, R.H., et al., Adhesion and debonding of multi-layer thin film structures. Engineering Fracture Mechanics, 1998. 61(1): p. 141-162.46.Wei, Y. and J.W. Hutchinson, Interface strength, work of adhesion and plasticity in the peel test. International Journal of Fracture, 1998. 93(1): p. 315.47.International Standard-ISO 13124, F.C.a.c., advanced technical ceramics), Test method for interfacial bond strength ceramic materials.48.Ksiazek, M., et al., Wetting and bonding strength in Al/Al2O3 system. Materials Science and Engineering: A, 2002. 324(1): p. 162-167.49.Sobczak, N. and A. Belosi. in NATO ASI Series, Proceeding Partner, Sub-series 3. High Technology. 1998. Dordrecht: Kluwer Academic.50.Della-Bona, A., The Relationship of Surface Treatment, Bond Strength, Interfacial Toughness and Fractography. J. Appl. Oral Sci., 2005. 13(2).51.https://mmplab.um.ac.ir/images/248/standard/bending/metals/ASTM%20E290%20%2014-Test%20Methods%20for%20Bend%20Testing%20of%20Material%20for%20Ductility.pdf52.https://kknews.cc/zh-tw/tech/gyna6e8.html53.https://www.astm.org/Standards/E854.https://www.astm.org/Standards/D1002.htm55.https://www.astm.org/Standards/D76.htm6.https://zh.wikipedia.org/wiki/%E6%8B%89%E4%BC%B8%E8%A9%A6%E9%A9%9757.http://www.ma-tek.com/zh-tw/services/index/Pro_category_04/Pro_1758.http://cmnst.ncku.edu.tw/p/405-1006-159877,c17606.php?Lang=zh-tw59.http://www.uvat.com/OutWeb/L_CT/Technology/Technology.asp60.https://zh.wikipedia.org/wiki/%E6%89%AB%E6%8F%8F%E7%94%B5%E5%AD%90%E6%98%BE%E5%BE%AE%E9%95%9C61.http://www.ma-tek.com/zh-tw/services/index/material/FIB62.https://zh.wikipedia.org/wiki/%E9%80%8F%E5%B0%84%E7%94%B5%E5%AD%90%E6%98%BE%E5%BE%AE%E9%95%9C | |
dc.identifier.uri |
https://hdl.handle.net/20.500.14371/72012 | |
dc.language.iso |
中文 | |
dc.relation.alma |
991001230479706772 | |
dc.relation.page |
85 | |
dc.subject.keyword |
鋁 | |
dc.subject.keyword |
鈦 | |
dc.subject.keyword |
暫態液相接合 | |
dc.subject.keyword |
微觀分析 | |
dc.subject.keyword |
剪應力 | |
dc.subject.keyword |
彎曲模數 | |
dc.subject.keyword |
6061 Aluminum | |
dc.subject.keyword |
Grade.2 Titanium | |
dc.subject.keyword |
microstructure | |
dc.subject.keyword |
transient liquid phase bonding | |
dc.subject.keyword |
shear strength | |
dc.subject.keyword |
bending modulus | |
dc.title |
利用暫態液相法接合鋁/鈦平板 | zh-TW |
dc.title |
Transient liquid phase bonding of aluminum / titanium plate | en |
dc.type |
Thesis | zh-TW |
檔案
- 01.pdf (3.81 MB, Adobe PDF)
所屬典藏: 材料科學與工程學系