溫度變化對錫銀銲錫可靠度與微結構之影響
顯示簡易詮釋資料 統計資料| 欄位 | 內容 | 語言 |
|---|---|---|
dc.contributor.advisor |
吳耀銓 | |
dc.contributor.advisor |
Wu, Yew-Chung Sermon | |
dc.contributor.author |
李岳陽 | |
dc.contributor.author |
Lee, Yueh-Yang | |
dc.contributor.college |
工學院 | |
dc.contributor.committee |
李宜璋 | |
dc.contributor.committee |
林蔚叡 | |
dc.contributor.committee |
吳耀銓 | |
dc.contributor.committee |
Lee, Yi-chang | |
dc.contributor.committee |
Lin, Wei-Jui | |
dc.contributor.committee |
Wu, Yew-Chung Sermon | |
dc.contributor.department |
工學院半導體材料與製程設備學程 | |
dc.contributor.studentid |
0761312 | |
dc.date.NCLavailable |
不公開 | |
dc.date.USTavailable |
不公開 | |
dc.date.etdavailablereason |
已經提供紙本論文 | |
dc.date.issued |
2022 | |
dc.date.issuedROC |
111 | |
dc.date.paperavailable |
2025/07/13 | |
dc.date.schoolyear |
110 | |
dc.description.abstract |
In this study, the difference between tin-silver solder concentration in Cu/Sn-Ag pillar is discussed, the height of copper part is 70 um, and tin-silver part is 30um, we observethe multiple samples (1wt%/2wt%/3wt% Sn-Ag) microstructure after various reliability test condition, include 1 to 3 times 260oC reflow, -65+1500oC thermal cycling, 1250oC and 1500oC high temperature storage test, -65+150oC and -55oC+125oC, and see if the 3 different concentration undergoes differnet intermetallic growing mechanism. The samples were then conducted shear test, observed the failure mode of rupture surface by cross-section and discuss the shear force effect. After high temperature test, the IMCs (intermetallic compounds) become thicker over time. However the pin-holes, cracks, ruptures are'nt growing in intermetallic compound by SEM (scanning electronic microscope) cross-section observation. The reliability test results also show the IMCs growing behaviour are similar in various concentration above, the interface between both side of IMCs after shear test are simlar either. The rupture mechanism of shear test is the extension of interior crack in Sn-Ag solder instead of abnormal brittle fracture mechanism. In the copper part, we analyze the plating copper shear test, besides the shear force is normal, all fracture part occured in the copper. Furthermore, we found the hardness obviously increase over reflow times when Ag concentration raise in hardness test. It suggest that Ag concentration is positive to the SA hardness. | |
dc.description.abstract |
在本實驗,探討銅柱(Cu/SnAg)中不同錫銀焊錫濃度主要銅高度70um錫銀銲料30um,濃度1wt%/2wt&/3wt%-SnAg使用260C 1-3次迴焊、-65+1500C溫度循環、1250C 及1500C高溫儲存及溫度循環(-65C+150C/-55C+125C)等可靠度測試後,觀察不同銀濃度金屬化合物之微結構變化,經由三種不同錫銀銲錫濃度的介金屬成長機制,並進行錫銀銅界面的推力測試,觀察剖面比較與推力及破裂失效面探討,並探討錫銀焊錫濃度對抗剪應力強度(Shear strength)之影響。 經由高溫測試,隨可靠度時間讀點增加,不同錫銀銲錫濃度的介金屬化合物厚度皆有增長。以SEM進行剖面觀察觀察微結構,金屬化合物介面間未觀察孔洞、裂縫、破裂,等增長。 不同的錫銀焊錫濃度試片,經可靠度的實驗後,雖然錫銀銲錫濃度不同,但IMC成長行為趨勢相近,推力測試的介金屬化合物界面結果,趨勢也是相近的,之後採用光學顯微鏡觀察錫銀焊錫剪應力測試破裂面觀察,觀察出所有的破裂機制發生在錫銀銲錫內部破裂併延伸,並無分析到異常的脆性破裂機制。並測試分析其電鍍銅剪應力強度,銅的推力測試結果為正常,光學顯微鏡觀察銅剪力測試破裂面,可發現所有的破裂機構全發生在銅破裂。 硬度測試中,試驗結果顯示Ag濃度越高,硬度隨迴銲次數加就越明顯,表示銀濃度對SA硬度變化有影響。 | |
dc.description.abstractopendate |
2025/07/13 | |
dc.description.degree |
碩士 | |
dc.description.tableofcontents |
中文摘要 ii英文摘要 iii誌謝 v目錄 vi圖目錄 vii表目錄 ix一、緒論 --------------------------------------------------1二、文獻回顧與探討------------------------------------------22-1 Sn-Ag無鉛銲料------------------------------------------32-2銅柱凸塊(copper pillar bump,CPB)------------------------62-3金屬間化合物(Intermetallic Compound, IMC)----------------7三、研究方法及步驟-------------------------------------------93.1樣本製程與結構--------------------------------------------93.2樣本截面觀察與分析設備------------------------------------123.2.1轉盤式研磨機-------------------------------------------123.2.2離子拋光機---------------------------------------------133.2.3場發射掃瞄式電子顯微鏡(SEM)與能量光譜散射儀(EDS)----------143.2.4硬度試驗機----------------------------------------------153.2.5推球測試機----------------------------------------------163.3.1觀察IMC生長情況------------------------------------------173.3.2 SA硬度與Ag3Sn分布---------------------------------------183.3.3推球測試與斷面觀察---------------------------------------18四、結果與討論------------------------------------------------194.1 IMC厚度量測-----------------------------------------------194.2 硬度測試與晶相觀察-----------------------------------------294.3推球剪力測試與斷面分析--------------------------------------37五、結論------------------------------------------------------44參考文獻------------------------------------------------------45 | |
dc.identifier.citation |
[1]K. Seeling and D. Suraski, "The Current Status of Lead-Free Solder Alloys," IEEE Transactions on Electronics Packaging Manufacturing, Vol.24, Issue 4, 2001, p.244-248[2]L.J. Turbini, G.C. Munie, D. Bernier, J. Gamalski, and D.W. Bergman, "Examining the Environmental Impact of Lead-Free Soldering Alternatives," IEEE Transactions on Electronics Packaging Manufacturing, Vol.24, No.1, 2001, p. 6-9[3]K. Seeling and D. Suraski, "The Current Status of Lead-Free Solder Alloys," IEEE Transactions on Electronics Packaging Manufacturing, Vol.24, Issue 4, 2001, p.244-248[4]D. Rys and P. Cox, "Directive 2002/95/EC of the European Parliament and of the Council of 27 January 2003 on the Restriction of the Use of Certain Hazardous Substances in Electrical and Electronic Equipment," Official Journal of the European Union, 2003[5]N.C. Lee, "Getting Ready for Lead-free Solder," Soldering and Surface Mount Technology, Vol.26, No.2, 1997, p.65-68[6]M. Abtew and G. Selvaduray, "Lead-free Solders in Microelectronics," Materials Science and Engineering R-reports, Vol.27, Issue 5-6, 2000, p.95-141[7]S. Choi, J.G. Guo, T.R. Bieler, K.N. Subramanian, and J.P. Lucas, "Creep Properties of Sn-Ag solder Joints Containing Intermetallic Particles," Journal of the Minerals Metals and Materials Society, Vol.53, Issue 6, 2001, p.22-26.[8]Kim S.H.,Yu J., “Effects of Ag on the Kirkendall void formation of Sn–xAg/Cu solder joints,” J. Appl Phys, 108, 083532, 2010.[9] W. Yang, R.W. Messler, and L.E. Felton, "Microstructure Evolution of Eutectic Sn-Ag Solder Joints," Journal of Electronic Materials, Vol.23, Issue 8, 1994, 90 p.765-772[10]K.S. Kim, S.H. Huh, and K. Suganuma, "Effect of Cooling Speed on Microstructure and Tensile Properties of Sn-Ag-Cu Alloys," Materials Science and Engineering A, Vol.333, Issue 1-2, 2002, p.106-114[11]K. Suganuma, S.H. Huh, K. Kim, H. Nakase ,and Y. Nakamura, "Effect of Ag Content on Properties of Sn-Ag Binary Alloy Solder," Materials Transactions, Vol. 42, No.2, 2001, p.286-291[12]K. Suganuma, "Interface Phenomena in Lead-free Soldering," Proceedings. EcoDesign '99: First International Symposium On Environmentally Conscious Design and Inverse Manufacturing 1999, p.620-625, Tokyo, Japan, 1999.[13]C.-S. Oh, J.-H. Shim, B.-J. Lee and D.N. Lee, J. Alloys & Compds. 238 (1996) 155-166:Full thermodynamic assessment.[14]S. Choi, J.G. Lee, F. Guo, T.R. Bieler, K. N. Subramanian, and J. P. Lucas, "Creep Properties of Sn-Ag Solder Joints Containing Intermetallic Particles," Journal of the Minerals Metals and Materials Society, Vol.53, Issue 6, p.22-26, 2001.[15]J.O.G. Parent, D.D.L. Chung, and I.M. Bernstein., "Effects of Intermetallic Formation at the Interface between Copper and Lead-Tin Solder," Journal of Materials Science, Vol.23, Issue 7, p.2564-2572, 1988.[16]P.G. Harris and K.S. Chaggar, "The Role of Intermetallic Compounds in Lead-Free Soldering," Soldering and Surface Mount Technology, Vol.10, Issue 3, 1998, p.33-38[17]Tong An, Fei Qin, “Cracking of the Intermetallic Compound Layer in Solder Joints Under Drop Impact Loading,” Journal of Electronic Packaging, vol.133, n 3, 2011.[18]Chun Yu, Yang Yang, Jieshi Chen, Jijin Xu, Junmei Chen, Hao Lu, “Effect of deposit thickness during electroplating on Kirkendall voiding at Sn/Cu joints,” Materials Letters, vol. 128, p. 9–11, 2014.[19]D.Q. Yu, L. Wang, “The growth and roughness evolution of intermetallic compounds ofSn–Ag–Cu/Cu interface during soldering reaction,” Journal of Alloys and Compounds, 458, 542, 2008.[20]D.Q. Yua, C.M.L. Wu, C.M.T. Law, L. Wang, J.K.L. Lai, “Intermetallic compounds growth between Sn–3.5Ag lead-freesolder and Cu substrate by dipping method,” Journal of Alloys and Compounds, 392, 192, 2005.[21]J.K. Shang, Daping Yao, “Effect of interface Roughness on Fatigue Crack Growth in Sn-Pb Solder Joints,” journal of Electronic Packaging, 118, 173, 1996. | |
dc.identifier.uri |
https://hdl.handle.net/20.500.14371/80113 | |
dc.language.iso |
中文 | |
dc.relation.alma |
991003845247006772 | |
dc.relation.page |
47 | |
dc.subject.keyword |
可靠度 | |
dc.subject.keyword |
銅柱 | |
dc.subject.keyword |
錫銀銲錫 | |
dc.subject.keyword |
金屬化合物 | |
dc.subject.keyword |
溫度循環 | |
dc.subject.keyword |
Reliability | |
dc.subject.keyword |
Cu pillar | |
dc.subject.keyword |
SnAg solder | |
dc.subject.keyword |
intermetallic compounds | |
dc.subject.keyword |
Temperature cycle test | |
dc.title |
溫度變化對錫銀銲錫可靠度與微結構之影響 | zh-TW |
dc.title |
Effect of thermal treatment on the reliability and the microstructure of SnAg solder | en |
dc.type |
Thesis | zh-TW |
檔案
全文未公開。
所屬典藏: 工學院專班-半導體材料與製程設備學程